Fracture toughness testing of nanocrystalline alumina and fused quartz using chevron-notched microbeams
Source abstract
Abstract
We show that chevron-notched samples offer an attractive approach to the measurement of fracture toughness in micron-scale samples of brittle materials and use the method to characterize quartz and nanocrystalline alumina. Focused ion beam milling is used to carve bend bars of rectangular cross-section a few micrometres wide and containing a notch with a triangular ligament. Load-controlled testing is conducted using a nanoindentation apparatus. If the notch is appropriately machined, cracks nucleate and propagate in a stable fashion before becoming unstable. Sample dimensions are measured using a scanning electron microscope, and are used as input in finite element simulations of the bars’ elastic deformation for various crack lengths. The calculated compliance calibration curve and the measured peak load then give the local fracture toughness of the material. Advantages of the method include a low sensitivity to environmental subcritical crack growth, and the fact that it measures toughness at the tip of a sharp crack situated in material unaffected by ion-milling. The approach is demonstrated on two materials, namely, monolithic fused quartz and nanocrystalline alumina Nextel™ 610 fibres; results for the latter give the intrinsic grain boundary toughness of alumina, free of grain bridging effects.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced Surface Polishing Techniques · Ultrasonics and Acoustic Wave Propagation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (68)
Show source-provided references
1. Hartzell · 2011
2. Zhang · Thin Solid Films · 2012 · 520 · 237510.1016/j.tsf.2011.09.036 ↗
3. Casellas · Acta Mater. · 2007 · 55 · 427710.1016/j.actamat.2007.03.028 ↗
4. Evans · J. Am. Ceram. Soc. · 1976 · 59 · 37110.1111/j.1151-2916.1976.tb10991.x ↗
5. Quinn · J. Am. Ceram. Soc. · 2007 · 90 · 67310.1111/j.1551-2916.2006.01482.x ↗
6. Zhang · Surf. Coat. Technol. · 2005 · 198 · 7410.1016/j.surfcoat.2004.10.021 ↗
7. Östlund · Adv. Funct. Mater. · 2009 · 19 · 243910.1002/adfm.200900418 ↗
8. Mook · Nanotechnology · 2010 · 21 · 05570110.1088/0957-4484/21/5/055701 ↗
9. Gerberich · J. Mater. Res. · 2012 · 27 · 55210.1557/jmr.2011.348 ↗
10. Zhang · Thin Solid Films · 2004 · 469–470 · 23310.1016/j.tsf.2004.08.094 ↗
11. Di Maio · J. Mater. Res. · 2005 · 20 · 29910.1557/JMR.2005.0048 ↗
12. Liu · Appl. Phys. Lett. · 2013 · 102 · 17190710.1063/1.4803928 ↗
13. Kahn · Sens. Actuators A-Phys. · 2000 · 82 · 27410.1016/S0924-4247(99)00366-0 ↗
14. O. Kraft, R. Schwaiger, W.D. Nix, Measurement of mechanical properties in small dimensions by microbeam deflection, in: MRS online proceedings library 1998, 518.10.1557/PROC-518-39 ↗
15. Koyama · Key Eng. Mat. · 2005 · 297–300 · 29210.4028/www.scientific.net/KEM.297-300.292 ↗
16. Matoy · Thin Solid Films · 2009 · 518 · 24710.1016/j.tsf.2009.07.143 ↗
17. Iqbal · Acta Mater. · 2012 · 60 · 119310.1016/j.actamat.2011.10.060 ↗
18. Fracture toughness and fatigue investigations of polycrystalline silicon
19. Bagdahn · J. Microelectromech. Syst. · 2003 · 12 · 30210.1109/JMEMS.2003.814130 ↗
20. Halford · Fatigue Fract. Eng. Mater. · 2005 · 28 · 69510.1111/j.1460-2695.2005.00893.x ↗
21. Li · Sens. Actuators A-Phys. · 2005 · 117 · 14310.1016/j.sna.2004.06.003 ↗
22. Li · Sens. Actuators. A-Phys. · 2005 · 119 · 22910.1016/j.sna.2003.10.063 ↗
23. Ando · Fatigue Fract. Eng. Mater. · 2005 · 28 · 68710.1111/j.1460-2695.2005.00920.x ↗
24. Espinosa · J. Microelectromech. Syst. · 2005 · 14 · 15310.1109/JMEMS.2004.839013 ↗
25. Xiang · Int. J. Fract. · 2007 · 144 · 17310.1007/s10704-007-9095-0 ↗
26. Massl · Acta Mater. · 2009 · 57 · 176810.1016/j.actamat.2008.12.018 ↗
27. Merle · Acta Mater. · 2011 · 59 · 177210.1016/j.actamat.2010.11.043 ↗
28. Armstrong · Philos. Mag. Lett. · 2011 · 91 · 39410.1080/09500839.2011.573813 ↗
29. Armstrong · Thin Solid Films · 2012 · 520 · 436910.1016/j.tsf.2012.02.059 ↗
30. Wurster · Philos. Mag. · 2012 · 92 · 180310.1080/14786435.2012.658449 ↗
31. Jaya · Microsc. Microanal. · 2013 · 19 · 183610.1017/S1431927613011173 ↗
32. Matoy · Thin Solid Films · 2010 · 518 · 579610.1016/j.tsf.2010.05.114 ↗
33. Nakao · J. Micromech. Microeng. · 2008 · 18 · 01502610.1088/0960-1317/18/1/015026 ↗
34. Kamiya · Thin Solid Films · 2005 · 473 · 12310.1016/j.tsf.2004.05.135 ↗
35. Matoy · Surf. Coat. Technol. · 2009 · 204 · 87810.1016/j.surfcoat.2009.09.013 ↗
36. Liu · Key Eng. Mater. · 2012 · 525–526 · 1310.4028/www.scientific.net/KEM.525-526.13 ↗
37. R. Ballarini, H. Kahn, N. Tayebi, A. Heuer, ASTM Special Technical Publication, 1413, 2001, 37.10.1520/STP10979S ↗
38. Kahn · MRS Bull. · 2001 · 26 · 30010.1557/mrs2001.64 ↗
39. Chasiotis · J. Appl. Mech. · 2005 · 73 · 71410.1115/1.2172268 ↗
40. Cho · Fatigue Fract. Eng. Mater. · 2007 · 30 · 2110.1111/j.1460-2695.2006.01086.x ↗
41. Y. Ichikawa, S. Maekawa, K. Takashima, M. Shimojo, Y. Higo, M.V. Swain, Fracture behavior of micro-sized Ni–P amorphous alloy specimens, in: MRS Online Proceedings Library 1999, 605.10.1557/PROC-605-273 ↗
42. Takashima · Fatigue Fract. Eng. Mater. · 2005 · 28 · 70310.1111/j.1460-2695.2005.00923.x ↗
43. Yang · Metall. Mater. Trans. A · 2007 · 38 · 122310.1007/s11661-007-9147-0 ↗
44. Fracture Behavior of Single- and Polycrystalline Silicon Films for MEMS Applications10.4028/www.scientific.net/KEM.297-300.551 ↗
45. Strength assessment of wafer-bonded micromechanical components using the Micro-Chevron-Test
46. Naumann · Microsyst. Technol. · 2013 · 19 · 68910.1007/s00542-012-1655-1 ↗
47. Fischer · Intermetallics · 2011 · 19 · 166110.1016/j.intermet.2011.07.015 ↗
48. Test Methods for Determination of Fracture Toughness of Advanced Ceramics at Ambient Temperature, ASTM Standard C1421-10, 2010.
49. Test Method for Plane-Strain (Chevron-Notch) Fracture Toughness of Metallic Materials, ASTM Standard E1304-97, 2008.
50. Development of ASTM C 1421-99 standard test methods for determination of fracture toughness of advanced ceramics
51. Barker · Eng. Fract. Mech. · 1977 · 9 · 36110.1016/0013-7944(77)90028-5 ↗
52. Cantonwine · J. Mater. Sci. · 2003 · 38 · 46110.1023/A:1021867530979 ↗
53. Minoshima · Fatigue Fract. Eng. Mater. · 2000 · 23 · 103310.1046/j.1460-2695.2000.00354.x ↗
54. Lawn · 1993
55. G. Žagar, A. Singh, V. Pejchal, M. Mueller, A. Mortensen (Submitted for publication).
56. Ingraffea · Int. J. Fract. · 1980 · 15 · 1427
57. Carpinteri · Eng. Fract. Mech. · 1992 · 42 · 103510.1016/0013-7944(92)90142-2 ↗
58. Kolhe · Int. J. Fract. · 1998 · 94 · 18910.1023/A:1007451005263 ↗
59. Wilson · Compos. Part A · 2001 · 32 · 114310.1016/S1359-835X(00)00176-7 ↗
60. Asmani · J. Eur. Ceram. Soc. · 2001 · 21 · 108110.1016/S0955-2219(00)00314-9 ↗
61. D.S. Harding, W.C. Oliver, G.M. Pharr, Cracking during nanoindentation and its use in the measurement of fracture toughness, in: MRS online proceedings library, 1994, 356.10.1557/PROC-356-663 ↗
62. L. Barker, Short bar specimens for KIC measurements, in: S.W. Freiman (ed.), Fracture mechanics applied to brittle materials. ASTM STP 678, ASTM International, Conshohocken, PA, 1979, 73–82.10.1520/STP36626S ↗
63. Scholz · Appl. Phys. Lett. · 2004 · 84 · 305510.1063/1.1711164 ↗
64. Wiederhorn · J. Am. Ceram. Soc. · 1974 · 57 · 33610.1111/j.1151-2916.1974.tb10917.x ↗
65. Mecholsky · J. Am. Ceram. Soc. · 1974 · 57 · 44010.1111/j.1151-2916.1974.tb11377.x ↗
66. Salem · J. Am. Ceram. Soc. · 2013 · 96 · 28110.1111/jace.12089 ↗
67. Lucas · Scripta Metal Mater. · 1995 · 32 · 74310.1016/0956-716X(95)91596-H ↗
68. Chantikul · J. Am. Ceram. Soc. · 1990 · 73 · 241910.1111/j.1151-2916.1990.tb07607.x ↗