journal article·2013-11Open access

In situ synchrotron tomography estimation of toughening effect by semi-ductile fibre reinforcement in a tungsten-fibre-reinforced tungsten composite system

J. Riesch, J.-Y. Buffiere, T. Höschen, M. di Michiel, M. Scheel, Ch. Linsmeier, J.-H. You

Acta Materialia· Volume 61· Issue 19

Abstract

Tungsten-fibre reinforced tungsten composites (W f=W) are supposed to enable enhanced toughness owing to extrinsic energy dissipation mechanisms such as interface debonding and plastic deformation of fibre. In particular, the latter is an e ective source of toughening, since ductile tungsten fibre can absorb considerable amount of plastic work. For a precise evaluation of the toughening capability, the energy dissipation mechanisms need to be analysed in detail. To this end, single-fibre tungsten composite specimens are fabricated and the stress-strain behaviour of the tungsten fibre bridging a matrix crack is measured by means of in-situ high energy synchrotron micro-tomography during an uniaxial tension test. Despite the high X-ray attenuation in tungsten a su ciently high resolution is achieved and clear images of crack extension and deformation are obtained. The amount of absorbed energy due to plastic deformation of the tungsten fibre is determined and compared with values obtained conventionally from single-fibre tension tests.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Baluc N. Final report on the EFDA task TW1-TTMA-002 deliverable 5. Tech. Rep. Centre de Recherches en Physique de Plasmas; 2002.
2. Lassner · 1999
3. Probabilistic failure analysis of a water-cooled tungsten divertor: impact of embrittlement10.1016/j.jnucmat.2008.01.009 ↗
4. Recent progress in research on tungsten materials for nuclear fusion applications in Europe10.1016/j.jnucmat.2012.08.018 ↗
5. Wurster S, Baluc N, Battabyal M, Crosby T, Du J, García Rosales C, et al. Recent progress in R&D on tungsten alloys for divertor structural and plasma facing materials. J Nucl Mater 2013, http://dx.doi.org/10.1016/j.jnucmat.2013.02.074.10.1016/j.jnucmat.2013.02.074 ↗
6. Feasibility study of a tungsten wire reinforced tungsten matrix composite with ZrOx interfacial coatings10.1016/j.compscitech.2010.04.028 ↗
7. Interfacial fracture behavior of tungsten wire/tungsten matrix composites with copper-coated interfaces10.1016/j.msea.2009.10.046 ↗
8. Riesch J, Höschen T, Galatanu A, You JH. Tungsten-fibre reinforced tungsten composites: a novel concept for improving the toughness of tungsten. In: Proceedings of the 18th international conference on composite materials. Jeju, South Korea; 2011. .
9. Riesch J. Entwicklung und Charakterisierung eines wolframfaserverstärkten Wolfram-Verbundwerkstoffs. Ph.D. thesis; Technische Universität München; 2012. .
10. Chawla · 1993
11. Wachtman · 1996
12. Aveston J, Cooper GA, Kelly A. Proceedings of the conference on the properties of fibre composites. Single and Multiple Fracture. IPC Science & Technology Press; 1971. p. 15–26 [chapter].
13. The mechanics of matrix cracking in brittle-matrix fiber composites10.1016/0001-6160(85)90124-5 ↗
14. Matrix fracture in fiber-reinforced ceramics10.1016/0022-5096(86)90035-9 ↗
15. Crack deflection at an interface between dissimilar elastic materials10.1016/0020-7683(89)90021-8 ↗
16. Rice RW. Mechanisms of toughening in ceramic matrix composites. In: Proceedings of the 5th annual conference on composites and advanced ceramic materials: ceramic engineering and science proceedings. The American Ceramic Society; 1981. p. 661–701.10.1002/9780470291092.ch20 ↗
17. Rice RW. Ceramic matrix composite toughening mechanisms: an update. In: Proceedings of the 9th annual conference on composites and advanced ceramic materials: ceramic engineering and science proceedings. The American Ceramic Society; 1985. p. 589–607.10.1002/9780470320280.ch11 ↗
18. Perspective on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
19. Toughening mechanisms for ceramic materials10.1016/0955-2219(92)90026-A ↗
20. McDanels DL. Tungsten fiber reinforced copper matrix composites. NASA Technical Paper 2924; NASA; 1989. [accessed 2013].
21. Flow characteristics of highly constrained metal wires10.1016/0001-6160(89)90069-2 ↗
22. Interfacial shear strength of Ti/SiC fibre composites measured by synchrotron strain measurement10.1016/S1359-835X(02)00152-5 ↗
23. SiC single fibre full-fragmentation during straining in a Ti–6Al–4V/SiC matrix studied by synchrotron X-rays10.1016/S1359-6454(02)00134-9 ↗
24. Fatigue crack growth and load redistribution in Ti/SiC composites observed in situ10.1016/j.actamat.2008.09.042 ↗
25. The effect of fibre fractures in the bridging zone of fatigue cracked Ti–6Al–4V/SiC fibre composites10.1016/j.actamat.2003.11.024 ↗
26. Fibre bridging during high temperature fatigue crack growth in Ti/SiC composites10.1016/j.actamat.2011.10.036 ↗
27. Interfacial shear strength behaviour of Ti/SiC metal matrix composites at room and elevated temperature10.1016/j.actamat.2010.07.027 ↗
28. The mechanical properties of tungsten grown by chemical vapour deposition10.1016/j.jnucmat.2008.12.182 ↗
29. Anderson · 2005
30. Kim · 1998
31. Stress transfer in a model composite containing a single embedded fiber10.1016/S1359-6454(96)00262-5 ↗
32. The estimation of statistical fiber strength by fragmentation tests of single-fiber composites10.1016/S0266-3538(00)00084-1 ↗
33. Morphological investigations of polypropylene single-fibre reinforced polypropylene model composites10.1016/S0032-3861(00)00660-1 ↗
34. Characterization of interphase properties: microfatigue of single fibre model composites10.1016/j.compositesa.2010.07.006 ↗
35. Interface debond crack growth in tensiontension cyclic loading of single fiber polymer composites10.1016/j.compositesa.2012.08.019 ↗
36. Du J. A feasibility study of tungsten-fiber-reinforced tungsten composites with engineered interfaces. Ph.D. thesis. Technische Universität München; 2011. .
37. Zinn AF. Chemical vapor deposition of tungsten. In: Kodas T, Hampden-Smith M, editors. The chemistry of metal CVD. VCH Verlagsgesellschaft mbH; 1994. p. 105–74.10.1002/9783527615858.ch3 ↗
38. In situ X-ray tomography studies of microstructural evolution combined with 3D modelling10.1557/mrs2008.126 ↗
39. Linsmeier C, Fu CC, Kaprolat A, Nielsen S, Mergia K, Schäublin R, et al. Advanced materials characterization and modeling using synchrotron, neutron, TEM, and novel micro-mechanical techniquesa european effort to accelerate fusion materials development. J Nucl Mater 2013, http://dx.doi.org/10.1016/j.jnucmat.2013.04.042.10.1016/j.jnucmat.2013.04.042 ↗
40. Zivelonghi A. Thermomechanical behaviour of two heterogeneous tungsten materials via 2d and 3d image-based FEM. Ph.D. thesis. Technische Universität München; 2011.
41. Recent developments in X-ray imaging with micrometer spatial resolution10.1107/S0909049506000550 ↗
42. ImageJ. rsbwebnihgov/ij/2011.
43. Characterization of internal damage in a MMCp using X-ray synchrotron phase contrast microtomography10.1016/S1359-6454(99)00024-5 ↗
44. Pippan R, Wurster S, Baluc N, Battabyal M, Crosby T, Du J, et al. Recent progress in R&D on tungsten alloys for divertor structural and plasma facing components. In: 15th International conference of fusion reactor materials (ICFRM), Charlston, USA; 2011.
45. Fracture modes in tungsten wire10.1016/0022-5088(76)90238-1 ↗
46. 1993
47. Hull D, Clyne T. An Introduction to composite materials. Cam; 1996.10.1017/CBO9781139170130 ↗
48. Pierson H. Handbook of chemical vapor deposition (CVD) – principles technology and applications, 2 ed. Noyes Publications/William Andrew Publishing, LLC; 1999.10.1016/B978-081551432-9.50005-X ↗
49. The evolution of growth stresses in chemical vapor deposited tungsten films studied by in situ wafer curvature measurements10.1063/1.354485 ↗
50. Relationships between hysteresis measurements and the constituent properties of ceramic matrix composites: II experimental studies on unidirectional materials10.1111/j.1151-2916.1995.tb08047.x ↗
51. Touloukian · 1977
52. Wilken T, Morcom W, Wert C, Woodhouse J. Reduction of tungsten oxide to tungsten metal. 1976;7(4)589–597.10.1007/BF02698592 ↗
53. Davis JR. Tensile Testing, vol. 2. ASM International; 2004.10.31399/asm.tb.tt2.9781627083553 ↗
54. The fracture energy of metal fibre reinforced ceramic composites (MFCs)10.1016/j.compscitech.2010.10.011 ↗
55. The one dimensional car parking problem and its application to the distribution of spacings between matrix cracks in unidirectional fiber-reinforced brittle materials10.1111/j.1151-2916.1992.tb05456.x ↗
56. Fiber fragmentation in a single-filament composite10.1063/1.104349 ↗