Solute cluster evolution during deformation and high strain hardening capability in naturally aged Al–Zn–Mg alloy

Peng Zhang, Kunkun Shi, Jianjun Bian, Jinyu Zhang, Yong Peng, Gang Liu, Alexis Deschamps, Jun Sun

Acta Materialia· Volume 207
Publisher page

Abstract

Abstract The natural aging (NA) response of a commercial Al–Zn–Mg alloy has been tracked to investigate the effects of solute clusters on its mechanical properties. It has been observed that the increase of yield strength during NA is not accompanied by the degradation of uniform elongation due to the simultaneously enhanced strain hardening ability. As a consequence, the Al–Zn–Mg alloy with dense solute clusters shows a comparable yield strength, better strain hardening ability and uniform tensile strain relative to its artificially aged counterparts containing precipitates. This positive effect of solute clusters on strain hardening has been systematically studied by tracing the microstructure evolution during deformation through synchrotron X-ray diffraction and atom probe tomography. We found that the dislocation multiplication dominates over the entire deformation process until failure in NA alloys; however, no effect of solute clusters on the dislocation density evolution can be identified. On the other hand, solute clusters themselves dramatically evolve, showing a dissolution-to-coarsening transition during deformation, which can be understood on the basis of a kinetic model. The experimental evidence strongly suggest that the dislocation storage and strain-induced evolution of solute clusters are insufficient to account for the observed high strain hardening rate, and the contribution from other possible mechanisms are estimated in a semi-quantitative manner.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Experiment and multiscale modeling of the coupled influence of constituents and precipitates on the ductile fracture of heat-treatable aluminum alloys10.1016/j.actamat.2005.04.002 ↗
2. Effect of interfacial solute segregation on ductile fracture of Al–Cu–Sc alloys10.1016/j.actamat.2012.11.043 ↗
3. Heat treatment of 7xxx series aluminium alloys–some recent developments10.1016/S1003-6326(14)63306-9 ↗
4. Hrem study and structure modeling of the η′ phase, the hardening precipitates in commercial al–zn–mgalloys10.1016/S1359-6454(99)00138-X ↗
5. Microstructural evolution and age hardening in aluminium alloys: atom probe field-ion microscopy and transmission electron microscopy studies10.1016/S1044-5803(99)00051-0 ↗
6. New techniques for the analysis of fine-scaled clustering phenomena within atom probe tomography (APT) data10.1017/S1431927607070900 ↗
7. Evolution of solute clustering in Al–Cu–Mg alloys during secondary ageing10.1016/j.actamat.2009.11.021 ↗
8. In-situ small-angle X-ray scattering study of dynamic precipitation in an Al–Zn–Mg–Cu alloy10.1080/0141861021000051091 ↗
9. In situ evaluation of dynamic precipitation during plastic straining of an Al–Zn–Mg–Cu alloy10.1016/j.actamat.2012.01.002 ↗
10. Hardening nanostructures in an alznmg alloy10.1080/14786430701271959 ↗
11. Early stages of solute clustering in an Al–Mg–Sialloy10.1016/j.actamat.2015.02.019 ↗
12. Effect of pre-strain on the solute clustering, mechanical properties, and work-hardening of a naturally aged Al–Cu–Mgalloy10.1007/s11661-017-4204-9 ↗
13. Solute clustering in Al–Cu–Mg alloys during the early stages of elevated temperature ageing10.1016/j.actamat.2010.05.020 ↗
14. Analysis of strengthening in aa6111 during the early stages of aging: atom probe tomography and yield stress modelling10.1016/j.actamat.2013.08.033 ↗
15. 3D atom probe study of solute atoms clustering during natural ageing and pre-ageing of an Al–Mg–Si alloy10.1080/09500830600643270 ↗
16. A model for the thermodynamics of and strengthening due to co-clusters in Al–Mg–Si-based alloys10.1016/j.actamat.2012.04.032 ↗
17. Design strategy for controlled natural aging in Al–Mg–Si alloys10.1016/j.actamat.2016.07.048 ↗
18. Clustering in age-hardenable aluminum alloys10.1002/adem.201800255 ↗
19. Gp-zones in Al–Zn–Mg alloys and their role in artificial aging10.1016/S1359-6454(01)00251-8 ↗
20. Low-temperature dynamic precipitation in a supersaturated Al–Zn–Mg alloy and related strain hardening10.1080/01418619908214295 ↗
21. Effects of natural aging on the formation and strengthening effect of gp zones in a retrogression and re-aged Al–Zn–Mg–cu alloy10.1016/j.jallcom.2020.154469 ↗
22. Natural Aging in Al–Mg–Si alloys—A process of unexpected complexity10.1002/adem.201000041 ↗
23. Cluster hardening in Al-3Mg triggered by small cu additions10.1016/j.actamat.2018.08.050 ↗
24. Cluster evolution mechanisms during aging in Al–Mg–Si alloys10.1016/j.actamat.2015.09.027 ↗
25. Strengthening of an Al–Cu–Mg alloy processed by high-pressure torsion due to clusters, defects and defect-cluster complexes10.1016/j.msea.2014.12.107 ↗
26. Solute clustering and solute nanostructures in an Al–3.5Cu–0.4Mg–0.2Ge alloy10.1016/j.actamat.2013.03.004 ↗
27. Solute nanostructures and their strengthening effects in Al-7Si-0.6Mg alloy f35710.1016/j.actamat.2011.10.029 ↗
28. Reversal of the negative natural aging effect in Al–Mg–Si alloys10.1016/j.actamat.2012.07.047 ↗
29. Effect of pre-ageing and natural ageing on the paint bake response of alloy aa6181a10.1016/j.msea.2013.01.065 ↗
30. Effect of natural ageing or pre-ageing on the evolution of precipitate structure and strength during age hardening of Al–Mg–Si alloy aa 601610.1016/j.msea.2019.05.073 ↗
31. Diffusion on demand to control precipitation aging: application to Al–Mg–Si alloys10.1103/PhysRevLett.112.225701 ↗
32. Cluster hardening in an aged Al–Cu–Mg alloy10.1016/S1359-6462(96)00415-0 ↗
33. Formation of solute nanostructures in an Al–Zn–Mgalloy during long-term natural aging10.1016/j.jallcom.2019.153572 ↗
34. Precipitation strengthening of aluminum alloys by room-temperature cyclic plasticity10.1126/science.aav7086 ↗
35. Training high-strength aluminum alloys to withstand fatigue
36. Enhanced strength-plasticity combination in an Al–Cu–Mg alloy—-Atomic scale microstructure regulation and strengthening mechanisms10.1016/j.msea.2020.139447 ↗
37. The thermodynamics of and strengthening due to co-clusters: general theory and application to the case of Al–Cu–Mgalloys10.1016/j.actamat.2009.01.021 ↗
38. Atomistic insights into cluster strengthening in aluminum alloys10.1016/j.mtla.2018.11.020 ↗
39. Ultrastrong steel via minimal lattice misfit and high-density nanoprecipitation10.1038/nature22032 ↗
40. Highly monodisperse core–shell particles created by solid-state reactions10.1038/nmat3077 ↗
41. Cluster strengthening in aluminium alloys10.1016/j.scriptamat.2014.04.018 ↗
42. The effect of shear-resistant, plate-shaped precipitates on the work hardening of Al alloys: towards a prediction of the strength–elongation correlation10.1016/j.actamat.2009.08.034 ↗
43. Static and dynamic precipitation behavior of the Al–20 wt.% Zn alloy10.1088/0256-307X/33/5/056101 ↗
44. Quantifying the strain-induced dissolution of precipitates in Al alloy microstructures using nuclear magnetic resonance10.1016/j.actamat.2009.07.060 ↗
45. Dynamic precipitation, segregation and strengthening of an Al–Zn–Mg–Cu alloy (aa7075) processed by high-pressure torsion10.1016/j.actamat.2018.09.060 ↗
46. On strain-induced dissolution of θ′ and θ particles in Al–Cu binary alloy during equal channel angular pressing10.1016/j.msea.2010.12.060 ↗
47. Analysis on the dissolution behavior of various size Cu-Mg co-clusters near a fatigue crack tip of underaged Al–Cu–Mg alloy during cyclic loading10.1016/j.jallcom.2016.12.323 ↗
48. Quantitative measurements of dynamic precipitation during fatigue of an Al–Zn–Mg–(Cu) alloy using small-angle X-rayscattering10.1016/j.actamat.2014.04.027 ↗
49. Dynamic strain ageing and dynamic precipitation in aa7030 during cyclic deformation10.1016/j.proeng.2010.03.029 ↗
50. Hirsch · 2008 · 1
51. Influence of copper addition on precipitation kinetics and hardening in Al–Zn–Mg alloy10.1179/026708399101506832 ↗
52. Early-stage precipitation in Al–Zn–Mg–Cu alloy (7050)10.1016/j.actamat.2004.06.025 ↗
53. Effect of copper addition on the cluster formation behavior of Al–Mg–Si, Al–Zn–Mg, and Al–Mg–Ge in the natural aging10.1007/s11661-018-4832-8 ↗
54. Kinetic monte carlo simulation of clustering in an Al–Zn–Mg–Cu alloy (7050)10.1016/j.actamat.2004.10.048 ↗
55. Anomalous strain hardening behaviour of a supersaturated Al–Zn–Mg alloy10.1016/S0921-5093(97)00324-9 ↗
56. Strength, grain refinement and solute nanostructures of an Al–Mg–Si alloy (aa6060) processed by high-pressure torsion10.1016/j.actamat.2013.10.022 ↗
57. Atom probe tomography data analysis procedure for precipitate and cluster identification in a ti-mo steel10.1016/j.dib.2018.03.094 ↗
58. MWP-FIT: a program for multiple whole-profile fitting of diffraction peak profiles by ab initio theoretical functions10.1107/S0021889801011451 ↗
59. Correlation between strength and microstructure of ball-milled Al–Mg alloys determined by X-ray diffraction10.1016/j.msea.2004.01.089 ↗
60. Quantifying dislocation density in Al–Cu coatings produced by cold spray deposition
61. Theoretical aspects of kinematical X-ray diffraction profiles from crystals containing dislocation distributions(fourier transform of X-ray diffraction line profiles from crystals with dislocations)
62. The contrast factors of dislocations in cubic crystals: the dislocation model of strain anisotropy in practice10.1107/S0021889899009334 ↗
63. Residual resistivity of clusters in solid solutions10.1088/0305-4608/10/5/016 ↗
64. In situ evaluation of dynamic precipitation during plastic straining of an Al–Zn–Mg–cu alloy10.1016/j.actamat.2012.01.002 ↗
65. Study of formation and reversion of Guinier-Preston zones in Al-4.5 at% Zn-x at% Mg alloys by positrons10.1007/BF01117364 ↗
66. The influence of precipitation on the work-hardening behavior of the aluminum alloys aa6111 and aa703010.1007/s11661-003-0007-2 ↗
67. Strengthening mechanisms of T1 precipitates and their influence on the plasticity of an Al–Cu–Li alloy10.1016/j.msea.2014.03.024 ↗
68. Physics and phenomenology of strain hardening: the FCC case10.1016/S0079-6425(02)00003-8 ↗
69. Kinetics of flow and strain-hardening10.1016/0001-6160(81)90112-7 ↗
70. A unified phenomenological description of work hardening and creep based on one-parameter models10.1016/0001-6160(84)90202-5 ↗
71. Microstructure-based modelling of isotropic and kinematic strain hardening in a precipitation-hardened aluminium alloy10.1016/j.actamat.2011.02.035 ↗
72. Metrology of small particles and solute clusters by atom probe tomography10.1016/j.actamat.2020.02.023 ↗
73. The effect of dislocation contrast on X-ray line broadening: a new approach to line profile analysis10.1063/1.117951 ↗
74. The evolution of dislocation density during heat treatment and creep of tempered martensite ferritic steels10.1016/S1359-6454(03)00324-0 ↗
75. Effect of strain-induced precipitation on the low angle grain boundary in aa7050 aluminum alloy10.1016/j.matdes.2011.04.025 ↗
76. Effect of dynamic plastic deformation on the microstructure and mechanical properties of an Al–Zn–Mg alloy10.1016/j.msea.2020.139287 ↗
77. Reprecipitation behavior in Al–Cu binary alloy after severe plastic deformation-induced dissolution of θ′ particles10.1016/j.msea.2012.03.010 ↗
78. Diffusion-limited phase transformations: a comparison and critical evaluation of the mathematical approximations10.1063/1.1658474 ↗
79. Deformation enhanced diffusion in aluminium alloys10.1007/s11661-020-05960-5 ↗
80. The effect of vacancy generation on plastic deformation10.1016/0036-9748(80)90295-1 ↗
81. Modelling the effect of deformation-induced vacancies on segregation and precipitation10.1016/0956-7151(94)90056-6 ↗
82. Meyers · 2008
83. Experimental and modelling assessment of precipitation kinetics in an Al–Li–Mg alloy10.1016/j.actamat.2012.01.010 ↗
84. Damask · 1963
85. Solute diffusion in metals: larger atoms can move faster10.1103/PhysRevLett.92.085901 ↗
86. Solute-vacancy clustering in aluminum10.1016/j.actamat.2020.06.062 ↗
87. Modelling the overlap of nucleation, growth and coarsening during precipitation10.1016/j.actamat.2004.06.024 ↗
88. Stored energy of 78 K tensile deformed copper crystals10.1016/0001-6160(75)90105-4 ↗
89. The nucleation of precipitates: the system Al–Zn–Mg10.1016/0001-6160(65)90067-2 ↗
90. Microstructure and flow stress of polycrystals and single crystals10.1016/S1359-6454(97)00365-0 ↗
91. Dislocation density evolution of aa 7020-t6 investigated by in-situ synchrotron diffraction under tensile load10.1016/j.matchar.2015.09.004 ↗
92. Microstructure and mechanical properties of Al–xMg alloys processed by room temperature ECAP10.1016/j.msea.2012.03.012 ↗
93. Effect of Mg on microstructure and mechanical properties of Al–Mg alloys produced by high pressure torsion10.1016/j.scriptamat.2018.09.033 ↗
94. Role of Mg in simultaneously improving the strength and ductility of Al–Mg alloys10.1016/j.msea.2016.01.089 ↗
95. Study of work hardening of quenched and naturally aged Al–Mg and Al–Cu alloys10.1016/j.msea.2008.10.010 ↗
96. Enhancement of strength and stability of nanostructured Ni by small amounts of solutes10.1016/j.scriptamat.2011.06.003 ↗
97. The superposition of strengthening contributions in engineering alloys10.1016/j.msea.2013.06.032 ↗
98. Dislocation glide through non-randomly distributed point obstacles10.1080/14786435.2013.820384 ↗
99. Multi-component solid solution and cluster hardening of Al–Mn–Si alloys10.1016/j.msea.2014.12.006 ↗
100. Effect of deformation geometry on the intermittent plastic flow associated with the Portevin–Le Chatelier effect10.1016/j.actamat.2008.07.025 ↗