Microstructure evolution during friction-stir welding of AZ31 magnesium alloy
Source abstract
Abstract
Abstract The microstructure evolution of a typical hexagonal close-packed (HCP) material (AZ31 magnesium alloy) during friction stir welding was studied in a wide range of welding temperatures. In all cases, the grain structure development was found to be significantly influenced by the formation of a very strong {0 0 0 1} 〈 u w t v 〉 B-fiber texture. Due to limitations imposed by this texture as well as by symmetry of the HCP crystal structure, an extensive lowering of grain-boundary misorientation was found to occur during deformation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Continuous dynamic recrystallization during friction stir welding of high strength aluminum alloys10.1016/S1359-6462(00)00480-2 ↗
2. Development of grain structure during friction stir welding10.1016/j.scriptamat.2004.04.017 ↗
3. Grain structure formation during friction stir welding observed by the stop action technique10.1016/j.actamat.2005.03.044 ↗
4. Effect of welding temperature on microstructure of friction-stir welded aluminum alloy10.1007/s11661-014-2651-0 ↗
5. Structural response of superaustenitic stainless steel to friction stir welding10.1016/j.actamat.2011.05.021 ↗
6. Grain structure development during friction stir welding of single-crystal austenitic stainless steel10.1007/s11661-013-1692-0 ↗
7. Development of grain structure during friction-stir welding of Cu–30Zn brass10.1080/14786435.2014.951712 ↗
8. Microstructural evolution of pure copper during friction-stir welding10.1080/14786435.2015.1006293 ↗
9. Microstructure, texture and residual stress in a friction-stir-processed AZ31B magnesium alloy10.1016/j.actamat.2007.12.020 ↗
10. Effect of micro-texture on fracture location in friction stir weld of Mg alloy AZ61 during tensile test10.1016/S1359-6462(03)00210-0 ↗
11. Improvement of yield stress of friction-stirred Mg–Al–Zn alloys by subsequent compression10.1016/j.scriptamat.2007.01.041 ↗
12. Effect of texture on the mechanical behavior of ultrafine grained magnesium alloy10.1016/j.scriptamat.2010.11.052 ↗
13. Microstructure and properties of friction stir butt-welded AZ31 magnesium alloy10.1016/j.msea.2006.05.128 ↗
14. Grain size and texture effects on deformation behavior of AZ31 magnesium alloy10.1016/j.msea.2012.08.080 ↗
15. Material flow and microstructural evolution during friction stir spot welding of AZ31 magnesium alloy10.1016/j.msea.2012.02.075 ↗
16. High strain rate superplasticity in friction stir processed ultrafine grained Mg–Al–Zn alloys10.1016/j.msea.2012.11.026 ↗
17. Mechanisms of fracture and inhomogeneous deformation on traverse tensile test of friction-stir-processed AZ31 Mg alloy10.1016/j.msea.2012.12.053 ↗
18. Effect of subsequent tension and annealing on microstructure evolution and strength enhancement of friction stir welded Mg alloys10.1016/j.msea.2014.02.062 ↗
19. Relationship between grain size and Zener–Hollomon parameter during friction stir processing in AZ31 Mg alloys10.1016/j.scriptamat.2004.05.043 ↗
20. Texture and weak grain size dependence in friction stir processed Mg–Al–Zn alloy10.1016/j.scriptamat.2006.06.005 ↗
21. Effects of heat input on tensile properties and fracture behavior of friction stir welded Mg–3Al–1Zn alloy10.1016/j.msea.2009.09.044 ↗
22. Grain structure evolution during friction-stir welding of AZ31 magnesium alloy10.1016/j.actamat.2009.07.041 ↗
23. Influence of thermos-mechanical parameters on texture and tensile behavior of friction stir processed Mg alloy10.1016/j.scriptamat.2010.08.016 ↗
24. Characteristics of long 10–12 twin bands in sheet rolling of a magnesium alloy10.1016/j.scriptamat.2013.11.008 ↗
25. Effect of tool geometry and process conditions on static strength of a magnesium friction stir lap linear weld10.1016/j.msea.2010.12.030 ↗
26. Influence of the microstructural changes and induced residual stresses on tensile properties of wrought magnesium alloy friction stir welds10.1016/j.msea.2012.05.021 ↗
27. Changes in texture and microstructure of friction stir welded Mg alloy during post-rolling and their effect on mechanical properties10.1016/j.msea.2013.06.005 ↗
28. Effect of inhomogeneous deformation on anisotropy of AZ31 magnesium sheet10.1016/j.msea.2012.08.117 ↗
29. Texture development in a friction stir lap-welded AZ31B magnesium alloy10.1007/s11661-014-2372-4 ↗
30. Basal plane texture and flow pattern in friction stir weld of a magnesium alloy10.1007/s11661-003-0228-4 ↗
31. Development of grain structure caused by friction stir welding of a ZK60 magnesium alloy10.2320/matertrans.MRA2008192 ↗
32. Specific character of material flow in near surface layer during friction stir processing of AZ31 magnesium alloy10.1007/s11661-009-0158-x ↗
33. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
34. Ideal orientations and persistence characteristics of hexagonal close packed crystals in simple shear10.1016/j.actamat.2006.12.021 ↗
35. Microstructures and textures of pure magnesium deformed in plane-strain compression10.1016/j.scriptamat.2004.07.002 ↗