journal article·2018-05

Complexions in WC-Co cemented carbides

Xingwei Liu, Xiaoyan Song, Haibin Wang, Xuemei Liu, Fawei Tang, Hao Lu

Acta Materialia· Volume 149
Publisher page

Abstract

Abstract The studies are focused on the complexions in the WC-Co cemented carbides, which represent the phase-like interfacial state at the WC/Co interfaces. A series of experiments were designed to investigate the formation, growth and transformation behaviors of the complexions. It was found that the complexions with cubic structure can be stabilized by quenching or by dissolution of specific elements added in form of carbides as grain growth inhibitors. The characteristics and stabilization conditions of the complexions, as well as their influences on the interfacial structures and mechanical properties of the cemented carbides, were studied in detail for additions of various inhibitors such as VC, Cr3C2, TiC, TaC and NbC. The results disclose that the existence of complexions is dominated by their formation energy and misfit at the interface between the complexion and WC. The stabilization of complexions, on one hand, inhibits WC grain growth effectively, on the other hand separates the bonding of WC and Co, thus causes decrease of the resistance against intergranular fracture of the cemented carbides. It is proposed that tailoring the stability of complexions by matching inhibitor and carbon content can lead to both the high fracture toughness and high strength of the cemented carbides.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Tunneling and Rock Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Deformation and fracture processes and the physical metallurgy of WC–Co hardmetals10.1179/imr.1988.33.1.90 ↗
2. Characterization and properties of sintered WC–Co and WC–Ni–Fe hard metal alloys10.1016/j.jallcom.2013.09.188 ↗
3. Physical and chemical nature of cemented carbides
4. A history of fine grained hardmetal10.1016/0263-4368(95)92671-6 ↗
5. Friction and wear behaviour of WC–Co–Cr3C2–VC cemented carbides obtained from nanocrystalline mixtures10.1016/j.wear.2011.07.012 ↗
6. Effect of interfacial characteristics on toughness of nanocrystalline cemented carbides10.1016/j.actamat.2012.12.036 ↗
7. Comparison between V8C7 and Cr3C2 as grain refiners for WC-Co10.1016/S0261-3069(01)00004-8 ↗
8. Cr-rich layer at the WC/Co interface in Cr-doped WC–Co cermets: segregation or metastable carbide?10.1016/j.jcrysgro.2004.05.101 ↗
9. Computational study of thin cubic carbide films in WC/Co interfaces10.1016/j.actamat.2010.09.021 ↗
10. Three-dimensional morphology of (W, V) Cx in VC-doped WC–Co hard metals10.1016/j.scriptamat.2013.06.002 ↗
11. A new approach to control the segregation of (Ta,W)C cubic phase in ultrafine WC–10Co–0.5Ta cemented carbides10.1016/j.scriptamat.2014.12.009 ↗
12. Influence of NbC and VC on microstructures and mechanical properties of WC–Co functionally graded cemented carbides10.1016/j.matdes.2015.10.156 ↗
13. Reinforcement of tungsten carbide grains by nanoprecipitates in cemented carbides10.1088/0957-4484/27/41/415710 ↗
14. Effects of NbC additions on the microstructure and properties of nonuniform structure WC-Co cemented carbides10.1016/j.msea.2017.01.077 ↗
15. Grain and phase boundary segregation in WC–Co with small V, Cr or Mn additions10.1016/j.actamat.2010.03.038 ↗
16. Grain and phase boundary segregation in WC–Co with TiC, ZrC, NbC or TaC additions10.1016/j.ijrmhm.2010.06.010 ↗
17. First-principles derived complexion diagrams for phase boundaries in doped cemented carbides10.1016/j.cossms.2016.05.009 ↗
18. Grain boundary complexions10.1016/j.actamat.2013.07.037 ↗
19. Carter · 2012
20. The role of grain boundary energy in grain boundary complexion transitions10.1016/j.cossms.2016.03.001 ↗
21. Microstructural characterization of high-thermal-conductivity aluminum nitride ceramic10.1111/j.1151-2916.2002.tb00587.x ↗
22. Battery materials for ultrafast charging and discharging10.1038/nature07853 ↗
23. Grain growth anomaly and dielectric response in Ti-rich strontium titanate ceramics10.1021/jp4035437 ↗
24. Interfacial control of magnetic properties at LaMnO3/LaNiO3 interfaces10.1021/acs.nanolett.5b02720 ↗
25. Manipulating the interfacial structure of nanomaterials to achieve a unique combination of strength and ductility10.1038/ncomms10802 ↗
26. Preparation and mechanisms of cemented carbides with ultrahigh fracture strength10.1107/S1600576715012832 ↗
27. Indentation fracture of WC-Co cermets10.1007/BF00555296 ↗
28. Superconductivity of the transition-metal carbides10.1103/PhysRev.159.327 ↗
29. Tungsten carbides and WC phase diagram10.1134/S0020168506020051 ↗
30. Effect of sintering cooling rate on V segregation amount at WC/Co interface in VC-doped WC-Co fine-grained hardmental10.2497/jjspm.51.576 ↗
31. Weidow · J. Am. Ceram. Soc. · 2011 · 94 · 60510.1111/j.1551-2916.2010.04122.x ↗
32. Stabilizing nanocrystalline materials with dopants10.1016/j.actamat.2006.11.028 ↗
33. Structural analysis on planar defects formed in WC platelets in Ti-doped WC–Co10.1111/j.1551-2916.2006.01218.x ↗
34. High resolution STEM investigation of interface layers in cemented carbides
35. HRTEM study for cemented carbides doped with transition metal carbides of VC, NbC and ZrC
36. Electronic structure, properties, and phase stability of inorganic crystals: a pseudopotential plane-wave study10.1002/(SICI)1097-461X(2000)77:5<895::AID-QUA10>3.0.CO;2-C ↗
37. Restoring the density-gradient expansion for exchange in solids and surfaces10.1103/PhysRevLett.100.136406 ↗
38. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
39. Thin intergranular films and solid-state activated sintering in nickel-doped tungsten10.1016/j.actamat.2007.01.017 ↗
40. Complexion: a new concept for kinetic engineering in materials science10.1016/j.actamat.2007.07.029 ↗
41. Simultaneously high fracture toughness and transverse rupture strength in ultrafine cemented carbide10.1039/c3ce40211h ↗
42. Effect of WC/Co coherency phase boundaries on fracture toughness of the nanocrystalline cemented carbides
43. Solid surfaces, interfaces and thin films