Abstract High resolution transmission electron microscopy (HRTEM) with nanometer-scaled energy-dispersive X-ray (EDX) was employed to investigate the transformation mechanisms of the GP zone → η′ → η precipitation sequence of AA7050, an Al-Zn-Mg-Cu alloy. Serial in-situ HRTEM frames revealed that separated nucleation of an η′ precipitate occurred elsewhere as the adjacent GPII zone dissolved. Evidence from HRTEM coupled with EDX showed that in-situ nucleation of a new η2 precipitate (one form of η) took place, wherein it gradually developed from the original η′ precipitate via a similar hexagonal structure with different compositions. The in-situ transition product was composed of two distinctive regions; one was identified as η′, and the other, as η.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Evolution of precipitate microstructure during stress aging of an Al–Zn–Mg–Cu alloy10.1016/j.msea.2015.03.047 ↗
2. Transformations and structures in the Al–Zn–Mg alloy system: a diffraction study using synchrotron radiation and electron precession10.1016/j.msea.2010.10.001 ↗
3. A preliminary study on optimizing the heat treatment of high strength Al–Cu–Mg–Zn alloys10.1016/j.matdes.2013.11.078 ↗
4. Experimental studies and constitutive modelling of the hardening of aluminium alloy 7055 under creep age forming conditions10.1016/j.ijmecsci.2011.05.006 ↗
5. Aging behavior and precipitate characterization of a high Zn-containing Al-Zn-Mg-Cu alloy with various tempers10.1016/j.matdes.2016.03.150 ↗
6. Effects of pre-treatments on aging precipitates and corrosion resistance of a creep-aged Al–Zn–Mg–Cu alloy10.1016/j.matdes.2015.06.029 ↗
7. Influence of retrogression and re-aging treatment on corrosion behaviour of an Al–Zn–Mg–Cu alloy10.1016/j.matdes.2010.11.036 ↗
8. An integrated process for modelling of precipitation hardening and springback in creep age-forming10.1016/j.ijmachtools.2006.01.026 ↗
9. Decomposition processes in an Al-5%Zn-1%Mg alloy. II.–Electromicroscopic investigation
10. Decomposition processes in Al-Zn-Mg alloys10.1007/BF00541825 ↗
11. An electron microscope investigation of the microstructure in an aluminium-zinc-magnesium alloy10.1016/0001-6160(70)90016-7 ↗
12. HREM study and structure modeling of the η′ phase, the hardening precipitates in commercial Al–Zn–Mg alloys10.1016/S1359-6454(99)00138-X ↗
13. Investigation of mechanical and corrosion properties of an Al–Zn–Mg–Cu alloy under various ageing conditions and interface analysis of η′ precipitate10.1016/j.matdes.2015.06.183 ↗
14. Influence of alloy composition and heat treatment on precipitate composition in Al–Zn–Mg–Cu alloys10.1016/j.actamat.2009.09.003 ↗
15. Structure of age-hardened aluminium-copper alloys10.1038/142569b0 ↗
16. The diffraction of x-rays by age-hardening aluminium copper alloys10.1098/rspa.1938.0152 ↗
17. Röntgenographische Untersuchungen über die Aushärtung einer Aluminium-Kupfer-Legierung mit Kleinwinkel-Schwenkaufnahmen
18. The structure of Guinier–Preston zones. I. The Fourier transform of the diffuse intensity diffracted by a Guinier–Preston zone10.1107/S0365110X55001813 ↗
19. The structure of Guinier-Preston zones in aluminum-copper alloys10.1107/S0365110X5800058X ↗
20. Direct observation of the strain field produced by coherent precipitated particles in an age-hardened alloy10.1080/14786435808244578 ↗
21. Chang · 1993
22. The early stages of GP zone formation in naturally aged Ai-4 wt pct cu alloys10.1007/BF02643840 ↗
23. The influence of zirconium on the early stages of aging of a ternary Al-Zn-Mg alloy10.1016/0956-7151(94)90406-5 ↗
24. The chemistry of precipitates in an aged Al-2.1Zn-1.7Mg at.% alloy10.1016/S1359-6462(99)00253-5 ↗
25. GP-zones in Al–Zn–Mg alloys and their role in artificial aging10.1016/S1359-6454(01)00251-8 ↗
26. Early-stage precipitation in Al–Zn–Mg–Cu alloy (7050)10.1016/j.actamat.2004.06.025 ↗
27. Secondary ageing in an aluminium alloy 705010.1016/j.msea.2008.02.039 ↗
28. Modeling of GP(I) zone formation during quench in an industrial AA7449 75mm thick plate10.1016/j.matdes.2016.09.052 ↗
29. On the kinetics of the growth of Guinier-Preston zones (GPZ) in AlZn (2.5 at%) Mg (X) alloys10.1002/pssa.2210210154 ↗
30. High-resolution characterization of the precipitation behavior of an Al–Zn–Mg–Cu alloy10.1080/09500839.2011.652682 ↗
31. Precipitation behaviour of Al–Zn–Mg–Cu alloy and diffraction analysis from η′ precipitates in four variants10.1016/j.jallcom.2014.05.061 ↗
32. Precipitation in an Al-Zn-Mg-Cu alloy during isothermal aging: atomic-scale HAADF-STEM investigation10.1016/j.msea.2017.03.032 ↗
33. The structure of the metastable η′ phase in Aluminum-Zinc-Magnesium alloys
34. Structure analysis of embedded nano-sized particles by precession electron diffraction. η′-precipitate in an Al–Zn–Mg alloy as example10.1016/j.ultramic.2006.01.009 ↗
35. Crystal structure and stability of complex precipitate phases in Al–Cu–Mg–(Si) and Al–Zn–Mg alloys10.1016/S1359-6454(01)00229-4 ↗
36. Influence of equal-channel angular pressing on precipitation in an Al–Zn–Mg–Cu alloy10.1016/j.actamat.2009.03.017 ↗
37. The nature and morphology of precipitate in AL-Zn-Mg alloys
38. Age-hardening in an Al-Mg-Zn alloy
39. X-ray and electron-microscopy study of precipitation in Al-Zn-Mg and Al-Zn-Mg-Cu alloys tempered between 100 and 300 C
40. The nucleation of precipitates: the system Al-Zn-Mg10.1016/0001-6160(65)90067-2 ↗
41. Atomic structure of hardening precipitates in an Al–Mg–Zn–Cu alloy determined by HAADF-STEM and first-principles calculations: relation to η-MgZn210.1007/s10853-013-7158-3 ↗
42. Microstructural evolution and age hardening in aluminium alloys: atom probe field-ion microscopy and transmission electron microscopy studies10.1016/S1044-5803(99)00051-0 ↗
43. Precipitation sequences during quenching of the AA 7010 alloy10.1016/S1359-6454(02)00063-0 ↗
44. A high-strength Al-Zn-Mg alloy hardened by the T-phase precipitates10.1016/j.jallcom.2014.04.185 ↗
45. In-situ transformation of Fe3C to Mo2C in iron-molybdenum-carbon alloys
46. Bhadeshia · 2011 · 197
47. Microstructural examination of 2.25 Cr-1 Mo Steel Steam pipes after extended service10.1016/1044-5803(93)90011-J ↗
48. In situ transformation of cementite to M7C3 and internal defects of M7C3 in high carbon-chromium steel by tempering10.2320/matertrans1960.19.11 ↗
49. Carbide reactions (M3C→ M7C3→ M23C6→ M6C) during tempering of rapidly solidified high carbon Cr-W and Cr-Mo steels10.1007/BF02661203 ↗
50. Crystallography of M23C6 and M6C precipitated in a low alloy steel10.1016/0001-6160(85)90193-2 ↗
51. Mechanism and crystallography of ferrite precipitation from cementite in an Fe-Cr-C alloy during austenitization10.1080/01418619908210385 ↗
52. Precipitation of molybdenum and vanadium carbides in high-purity iron alloys
53. Nucleation of precipitates in aged AlCuMg (Ag) alloys with high Cu: Mg ratios10.1016/1359-6454(95)00314-2 ↗
54. The precipitation behavior of an Al–Cu–Mg–Ag alloy under ECAP10.1016/j.msea.2013.09.021 ↗
55. On the strengthening response of aluminum alloys containing shear-resistant plate-shaped precipitates10.1016/j.actamat.2008.08.023 ↗
56. Phase transformation and precipitation of an Al–Cu alloy during non-isothermal heating studied by in situ small-angle and wide-angle scattering10.1016/j.jallcom.2013.04.201 ↗
57. On the effect of stress on nucleation and growth of precipitates in an Al-Cu-Mg-Ag alloy10.1007/BF02595436 ↗
58. Microstructural evolution of 7012 alloy during the early stages of artificial ageing10.1016/S1359-6454(99)00315-8 ↗
59. The effect of reversion treatments on precipitation mechanisms in an Al-1.35 at. pct Mg2Si alloy10.1007/BF02669387 ↗
60. Williams · 2009 · 64
61. Egerton · 2011 · 389
62. Radiation damage in the TEM and SEM10.1016/j.micron.2004.02.003 ↗
63. Electron beam-assisted healing of nanopores in magnesium alloys10.1038/srep01920 ↗
64. Point-defect and threshold displacement energies in Ni3Al II. Events at the displacement threshold10.1080/01418619308207159 ↗
65. Threshold energy surface and frenkel pair resistivity for Cu10.1016/0022-3115(83)90005-3 ↗
66. Electron irradiation damage in magnesium10.1016/0001-6160(77)90144-4 ↗
67. Electron radiation damage in HCP metals—I. The determination of the threshold displacement energy in Zn, Cd, Mg and Ti10.1016/0001-6160(78)90048-2 ↗
68. Constitutive modelling of creep-ageing behaviour of peak-aged aluminium alloy 7050
69. Kinetic modeling of solid-state partitioning phase transformation with simultaneous misfit accommodation10.1016/j.actamat.2016.02.010 ↗
70. Direct measurement of precipitate induced strain in an Al-Zn-Mg-Cu alloy with aberration corrected transmission electron microscopy10.1016/j.micron.2016.07.010 ↗