The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: Overview

Michihiko Nagumo, Kenichi Takai

Acta Materialia· Volume 165
Publisher page

Abstract

Abstract Recent studies on hydrogen enhancement of the strain-induced generation of vacancies, i.e. the HESIV mechanism, and its role in hydrogen embrittlement (HE) of steels are overviewed. A high density of vacancies and their clustering have been detected by newly developed low temperature hydrogen thermal desorption spectroscopy and positron lifetime measurements. The promotion of crack nucleation and growth is ascribed to the evolution of damage associated with intense strain localization, and characteristic features of HE such as dependence on the microstructures of steels and test conditions are consistent with the HESIV mechanism. The predominant and supplementary roles of vacancies and hydrogen, respectively, in premature fracture are demonstrated by experiments devised to separate each contribution. A constitutive relation for porous materials is applicable to describe mechanistic effects of the HESIV mechanism on crack growth resistance and strain localization. The sequential void nucleation, growth and link mechanism in nanoscale are suggested.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (66)

Show source-provided references
1. The role of hydrogen in enhancing plastic instability and degrading fracture toughness in steels
2. Environmentally assisted cracking: overview of evidence for an adsorption-induced localized-slip process10.1016/0001-6160(88)90113-7 ↗
3. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗
4. Deformation induced defects in iron revealed by thermal desorption spectroscopy of tritium10.1016/S1359-6462(98)00436-9 ↗
5. Hydrogen thermal desorption relevant to delayed-fracture susceptibility of high-strength steels10.1007/s11661-001-0265-9 ↗
6. Hydrogen related failure of steels – a new aspect (overview)10.1179/026708304225019687 ↗
7. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation I. Theoretical background10.1016/j.actamat.2007.05.047 ↗
8. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation II. Experimental evidence and consequences10.1016/j.actamat.2007.05.033 ↗
9. Ductile fracture by vacancy condensation in F.C.C. single crystals10.1016/1359-6454(95)00220-0 ↗
10. Annihilation of dislocations during tensile and cyclic deformation and limits of dislocation densities10.1080/01418617908234871 ↗
11. Generation and accumulation of atomic vacancies due to dislocation movement and pair annihilation10.1080/14786435.2018.1478142 ↗
12. In-situ TEM observations of nucleation and bluntness of nanocracks in thin crystals of 310 stainless steel10.1016/0956-7151(95)00122-C ↗
13. Defect trapping of ion-implanted deuterium in Fe10.1063/1.326761 ↗
14. Hydrogen trapping characteristics of cold-drawn pure iron and eutectoid steel evaluated by thermal desorption spectroscopy10.2320/jinstmet1952.62.3_267 ↗
15. Function of hydrogen in intergranular fracture of martensitic steels10.1080/01418610208240452 ↗
16. Effect of grain size on the susceptibility of martensitic steel to hydrogen embrittlement10.1080/09500830500482316 ↗
17. Lattice defects dominating hydrogen-related failure of metals10.1016/j.actamat.2008.06.031 ↗
18. Nagumo · 2016 · 15
19. Identification of hydrogen trapping sites, binding energies, and occupation ratios at vacancies, dislocations and grain boundaries in iron of varying carbon content
20. Evaluation of lattice defects near hydrogen-related fracture surfaces of tempered martensitic steel
21. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
22. Hydrogen desorption spectra of hydrogen-enhanced strain-induced vacancies in pure iron
23. Atomistic study of hydrogen effects on stability and mobility of vacancy and vacancy-clusters
24. Vacancies and carbon impurities in α-iron: electron irradiation10.1103/PhysRevB.25.762 ↗
25. First-principles calculation of hydrogen effects on the formation and diffusion of vacancies on alpha iron: discussion of the hydrogen-enhanced strain-induced vacancy mechanism10.2472/jsms.63.182 ↗
26. The effect of hydrogen on vacancy generation in iron by plastic deformation10.1016/j.scriptamat.2006.08.030 ↗
27. Effects of grain size and deformation temperature on hydrogen-enhanced vacancy formation in Ni alloys10.1016/j.actamat.2017.02.016 ↗
28. Structure of dislocations in Al and Fe as studied by positron-annihilation spectroscopy10.1103/PhysRevB.45.7017 ↗
29. The interaction of dislocations and hydrogen-vacancy complexes and its importance for deformation-induced proto nano-voids formation in α-Fe10.1016/j.ijplas.2015.05.017 ↗
30. Equilibrium aspects of hydrogen-induced cracking of steels10.1016/0001-6160(74)90061-3 ↗
31. Crack growth from internal hydrogen – temperature and microstructural effects in 4340 steel10.1007/BF02662593 ↗
32. Microscopic process of failure and mechanism of hydrogen embrittlement of iron10.2320/jinstmet1952.45.12_1309 ↗
33. Hydrogen-assisted failure in Ni-based superalloy 718 studied under in situ hydrogen charging: the role of localized deformation in crack propagation10.1016/j.actamat.2017.02.059 ↗
34. The nature of quasicleavage fracture in tempered 5.5Ni steel after hydrogen charging10.1007/BF02645559 ↗
35. Crystallographic features of hydrogen-related fracture surfaces in tempered martensitic steel
36. Hydrogen embrittlement of ferritic steels: observations on deformation microstructure, nanoscale dimples and failure by nanovoiding10.1016/j.actamat.2012.06.014 ↗
37. Equilibrium and growth characteristics of hydrogen-induced intergranular cracking in phosphorus-doped and high purity steels10.1016/0001-6160(86)90119-7 ↗
38. Characterization of hydrogen-related fracture behavior in as-quenched low-carbon martensitic steel and tempered medium-carbon martensitic steel10.1007/s11661-015-3176-x ↗
39. Hydrogen-induced slip localization around a quasi-brittle fatigue crack observed by high-voltage electron microscopy10.1016/j.scriptamat.2009.03.020 ↗
40. Hydrogen embrittlement of austenitic stainless steels revealed by deformation microstructures and strain-induced creation of vacancies10.1016/j.actamat.2013.12.039 ↗
41. Alloying effects on the stacking fault energy in austenitic stainless steels from first-principles theory10.1016/j.actamat.2006.04.013 ↗
42. Effects of alloying elements on delayed fracture
43. Hydrogen in trapping states innocuous to environmental degradation of high-strength steels10.2355/isijinternational.43.520 ↗
44. The role of hydrogen: is the story any clearer?
45. Dependence of hydrogen-induced lattice defects and hydrogen embrittlement of cold-drawn pearlitic steels on hydrogen trap state, temperature, strain rate and hydrogen content10.1016/j.actamat.2014.07.008 ↗
46. The role of hydrogen-enhanced strain-induced lattice defects on hydrogen embrittlement susceptibility of X80 pipeline steel10.1007/s11837-017-2371-1 ↗
47. Lattice defect formation behavior of cold-drawn pearlitic steel fractured under elastic and plastic region in the presence of hydrogen10.2355/tetsutohagane.TETSU-2017-036 ↗
48. Fatigue damage and its interaction with hydrogen in martensitic steels10.1016/S0921-5093(02)00745-1 ↗
49. Enhanced susceptibility to delayed fracture in pre-fatigued martensitic steel10.1016/S0921-5093(02)00403-3 ↗
50. Hydrogen-enhanced lattice defect formation and hydrogen embrittlement of cyclically prestressed tempered martensitic steel10.1016/j.actamat.2013.09.015 ↗
51. Towards proper design and assessment of materials against hydrogen embrittlement
52. Enhanced lattice defect formation associated with hydrogen and hydrogen embrittlement under elastic stress of a tempered martensitic steel10.2355/isijinternational.52.198 ↗
53. Deformation-induced defects controlling fracture toughness of steel revealed by tritium desorption behaviors10.1016/S1359-6454(99)00392-4 ↗
54. FEM analysis of ductile crack growth in fracture transition region for steels with different void nucleation frequencies10.2355/isijinternational.38.196 ↗
55. An analysis of ductile rupture modes at a crack tip10.1016/0022-5096(87)90034-2 ↗
56. Ductile crack growth resistance in hydrogen-charged steels10.2320/matertrans.42.132 ↗
57. Hydrogen effect against hydrogen embrittlement10.1007/s11661-010-0275-6 ↗
58. Effect of hydrogen and frequency on fatigue behavior of SCM 435 steel for storage cylinder of hydrogen station10.1299/kikaia.73.1358 ↗
59. Hydrogen-induced strain localization and failure of austenitic stainless steels at high hydrogen concentrations10.1016/0956-7151(91)90211-I ↗
60. Hydrogen-enhanced localization of plasticity in an austenitic stainless steels10.1007/BF02669644 ↗
61. Interpretation of hydrogen-assisted fatigue crack propagation in BCC iron based on dislocation structure evolution around the crack wake10.1016/j.actamat.2018.06.041 ↗
62. Detecting stable crack onset at ductile-brittle transition in steels10.1007/BF02648425 ↗
63. Conditions for the localization of deformation in pressure-sensitive dilatant materials10.1016/0022-5096(75)90001-0 ↗
64. Investigation on dislocation-based mechanisms of void growth and coalescence in single crystal and nanotwinned nickels by molecular dynamics simulation10.1080/14786435.2017.1352108 ↗
65. Void growth in single crystal copper-an atomistic modeling and statistical analysis study10.1080/14786435.2017.1412591 ↗
66. Void growth in metals: atomistic calculations10.1016/j.actamat.2008.03.047 ↗