Effect of potassium doping and exposure temperature on the deuterium behavior in large-scale potassium-doped tungsten
Source abstract
Abstract
In order to meet the needs of future fusion power plants in engineering application, a newly large-volume potassium-doped tungsten (WK) plate with a thickness of 15 mm was prepared by powder metallurgy and hot rolling technology. Pure tungsten (PW) as a comparison material was prepared using the same preparation process. To figure out the effect of K doping and exposure temperature on D retention and blistering morphology in WK and PW, the high-flux (∼10 22 m −2 s −1) and low energy (∼ 50 eV) D plasma exposure with different temperatures (423, 473, 523 and 573 K) was performed. The results show that there is serious surface blistering in both PW and WK at all exposure temperatures and PW forms D blisters larger in size but smaller in number compared with WK. The D retention in PW is significantly lower than that in WK at all exposure temperatures. Moreover, the evolution of D blisters and retention in WK is more sensitive to exposure temperature compared to PW. The effects of K doping and exposure temperature on blistering morphology and D retention were analyzed and discussed in detail.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (76)
Show source-provided references
1. Tungsten as material for plasma-facing components in fusion devices10.1016/j.jnucmat.2011.01.110 ↗
2. Use of tungsten material for the ITER divertor10.1016/j.nme.2016.07.003 ↗
3. Preparation of ultrafine-grained/nanostructured tungsten materials: an overview10.1016/j.jallcom.2018.11.279 ↗
4. Recent progress in research on tungsten materials for nuclear fusion applications in Europe10.1016/j.jnucmat.2012.08.018 ↗
5. Effect of hot working process on the mechanical properties of tungsten materials10.1016/j.jnucmat.2013.01.307 ↗
6. Microstructure and helium irradiation performance of high purity tungsten processed by cold rolling10.1016/j.jnucmat.2016.07.038 ↗
7. Tungsten foil laminate for structural divertor applications - Analyses and characterisation of tungsten foil10.1016/j.jnucmat.2012.02.030 ↗
8. Plastic flow localization in bulk tungsten with ultrafine microstructure10.1063/1.1875754 ↗
9. Microstructure and mechanical properties of super-strong nanocrystalline tungsten processed by high-pressure torsion10.1016/j.actamat.2006.05.005 ↗
10. High temperature fracture experiments on tungsten-rhenium alloys10.1016/j.ijrmhm.2010.03.002 ↗
11. Effects of vanadium concentration on the densification, microstructures and mechanical properties of tungsten vanadium alloys10.1016/j.jnucmat.2014.04.019 ↗
12. Fracture behaviour of tungsten-vanadium and tungsten-tantalum alloys and composites10.1016/j.jnucmat.2011.04.025 ↗
13. Effect of high temperature swaging and annealing on the mechanical properties and thermal conductivity of W-Y2O310.1016/j.jnucmat.2015.04.050 ↗
14. Microstructure and mechanical properties of a W-2 wt.%Y2O 3 composite produced by sintering and hot forging10.1016/j.jnucmat.2013.01.301 ↗
15. Mechanical properties and thermal stability of pure W and W-0.5 wt%ZrC alloy manufactured with the same technology10.1016/j.msea.2017.12.112 ↗
16. Mechanical properties and thermal stability of rolled W-0.5 wt% TiC alloys10.1016/j.msea.2016.06.049 ↗
17. Enhanced toughness and stable crack propagation in a novel tungsten fibre-reinforced tungsten composite produced by chemical vapour infiltration
18. Behavior of tungsten fiber-reinforced tungsten based on single fiber push-out study10.1016/j.nme.2016.04.010 ↗
19. Correlation between the microstructure, mechanical/thermal properties, and thermal shock resistance of K-doped tungsten alloys10.1016/j.jnucmat.2019.03.056 ↗
20. Improvement of impact properties of tungsten by potassium doping10.1016/j.fusengdes.2019.01.130 ↗
21. Large-scale potassium-doped tungsten alloy with superior recrystallization resistance, ductility and strength induced by potassium bubbles10.1016/j.jnucmat.2021.153450 ↗
22. Effect of potassium bubbles on the thermal shock fatigue behavior of large-volume potassium-doped tungsten alloy10.1088/1741-4326/ac9a5b ↗
23. Microstructure development of dispersion-strengthened tungsten due to neutron irradiation10.1016/j.jnucmat.2013.10.012 ↗
24. Neutron irradiation tolerance of potassium-doped and rhenium-alloyed tungsten10.1016/j.jnucmat.2021.153009 ↗
25. Recent progress in the assessment of irradiation effects for in-vessel fusion materials: tungsten and copper alloys10.1088/1741-4326/ac4062 ↗
26. Refractory metals revolutionizing the lighting technology: a historical review10.1016/j.ijrmhm.2014.11.002 ↗
27. The effect of heat treatments on pure and potassium doped drawn tungsten wires: part II – fracture properties10.1016/j.msea.2018.09.029 ↗
28. Mechanical properties and microstructural characterizations of potassium doped tungsten10.1016/j.nucengdes.2011.10.008 ↗
29. Plastic deformation of recrystallized tungsten-potassium wires: constitutive deformation law in the temperature range 22–600 °C10.1016/j.ijrmhm.2018.01.012 ↗
30. Thermo-mechanical and thermal shock characterization of potassium doped tungsten10.1016/j.ijrmhm.2010.03.001 ↗
31. ITER tungsten divertor design development and qualification program10.1016/j.fusengdes.2013.05.010 ↗
32. Irradiation hardening behaviors of large-scale hot rolling potassium-doped tungsten alloy under synergistic irradiations of Fe11+ ion combined with deuterium and helium plasmas
33. Effect of Fe11+ ion combined with helium and deuterium plasmas irradiation on the transient thermal shock behaviors of pure and potassium-doped tungsten10.1016/j.jnucmat.2022.154100 ↗
34. Surface modification of molten W exposed to high heat flux helium neutral beams10.1016/j.jnucmat.2013.02.043 ↗
35. Deuterium occupation of vacancy-type defects in argon-damaged tungsten exposed to high flux and low energy deuterium plasma10.1088/0029-5515/56/3/036010 ↗
36. A review of modelling and simulation of hydrogen behaviour in tungsten at different scales10.1088/0029-5515/54/8/086001 ↗
37. Temperature dependence of surface morphology and deuterium retention in polycrystalline ITER-grade tungsten exposed to low-energy, high-flux D plasma10.1016/j.jnucmat.2011.11.003 ↗
38. Temperature dependence of surface topography and deuterium retention in tungsten exposed to low-energy, high-flux D plasma10.1016/j.jnucmat.2011.01.088 ↗
39. Development and optimization of STEP-A linear plasma device for plasma-material interaction studies10.13182/FST16-115 ↗
40. Air exposure and sample storage time influence on hydrogen release from tungsten10.1016/j.jnucmat.2010.07.011 ↗
41. Blister bursting and deuterium bursting release from tungsten exposed to high fluences of high flux and low energy deuterium plasma10.1088/0029-5515/47/3/006 ↗
42. Subsurface morphology changes due to deuterium bombardment of tungsten
43. Mechanism for orientation dependence of blisters on W surface exposed to D plasma at low temperature10.1016/j.jnucmat.2016.05.011 ↗
44. Surface morphology and deuterium retention in tungsten exposed to high flux D plasma at high temperatures10.1016/j.jnucmat.2014.11.079 ↗
45. Effect of initial exposure temperature on the deuterium retention and surface blistering in tungsten
46. (001) edge dislocation nucleation mechanism of surface blistering in tungsten exposed to deuterium plasma10.1088/1741-4326/aaf32e ↗
47. Deuterium behavior in tungsten exposed to deuterium plasma with rising or declining temperature10.1016/j.jnucmat.2020.152243 ↗
48. First-principles study of carbon effects in a tungsten grain boundary: site preference, segregation and strengthening10.1007/s11433-011-4495-6 ↗
49. Influence of near-surface blisters on deuterium transport in tungsten10.1088/1741-4326/aa7212 ↗
50. Aggravated blistering and increased deuterium retention in iron-damaged tungsten after exposure to deuterium plasma with various surface temperatures10.1088/1741-4326/aad1a0 ↗
51. Decreased surface blistering and deuterium retention in potassium-doped tungsten exposed to deuterium plasma following ion irradiation10.1088/1741-4326/aca48c ↗
52. Vacancy trapping mechanism for hydrogen bubble formation in metal10.1103/PhysRevB.79.172103 ↗
53. Controlling factors for the brittle-to-ductile transition in tungsten single crystals10.1126/science.282.5392.1293 ↗
54. High-temperature tensile and thermal shock characterization of low-temperature rolled tungsten
55. The influence of helium on the bulk properties of fusion reactor structural materials10.1088/0029-5515/24/8/009 ↗
56. Influence of the microstructure on the deuterium retention in tungsten10.1016/j.jnucmat.2010.10.045 ↗
57. Investigation of hydrogen-defect interaction in tungsten by the probe fluence method10.1016/j.jnucmat.2010.10.069 ↗
58. Deuterium trapping in tungsten damaged by high-energy hydrogen ion irradiation10.1016/j.jnucmat.2009.01.107 ↗
59. Enhanced modification of tungsten surface by nanostructure formation during high flux deuterium plasma exposure10.1016/j.jnucmat.2013.12.010 ↗
60. Deuterium-induced nanostructure formation on tungsten exposed to high-flux plasma10.1016/j.jnucmat.2014.11.039 ↗
61. Recent findings on blistering and deuterium retention in tungsten exposed to high-fluence deuterium plasma10.1016/j.jnucmat.2008.12.129 ↗
62. Microstructure dependence of deuterium retention and blistering in the near-surface region of tungsten exposed to high flux deuterium plasmas of 38 eV at 315 K10.1088/0031-8949/2007/T128/019 ↗
63. The influence of helium on the bulk properties of fusion reactor structural materials10.1088/0029-5515/24/8/009 ↗
64. E. Diagram, C. Structures, The H-K (hydrogen-potassium) system the H-K (hydrogen-potassium) system, phase diagram evaluations: Section II. 18(1997),387-389 doi: 10.1007/s11669-997-0066-y.10.1007/s11669-997-0066-y ↗
65. Ion-driven deuterium retention in tungsten10.1063/1.2828139 ↗
66. Solution and diffusion of hydrogen in tungsten10.1116/1.1492699 ↗
67. Baseline high heat flux and plasma facing materials for fusion10.1088/1741-4326/aa6b60 ↗
68. Surface modification of tungsten and tungsten-tantalum alloys exposed to high-flux deuterium plasma and its impact on deuterium retention10.1088/0029-5515/53/1/013013 ↗
69. Deuterium trapping and surface modification of polycrystalline tungsten exposed to a high-flux plasma at high fluences10.1088/1741-4326/aa5898 ↗
70. Lipschultz · 2010 · 1
71. A multi-technique analysis of deuterium trapping and near-surface precipitate growth in plasma-exposed tungsten10.1063/1.4928184 ↗
72. Deuterium retention in TiC and TaC doped tungsten under low-energy ion irradiation
73. Surface blistering and deuterium retention behaviors in pure and ZrC-doped tungsten exposed to deuterium plasma10.1088/1741-4326/abdfda ↗
74. Deuterium implantation into Y2O3-doped and pure tungsten: deuterium retention and blistering behavior10.1016/j.jnucmat.2017.02.005 ↗
75. The high-flux effect on deuterium retention in TiC and TaC doped tungsten at high temperatures10.1016/j.jnucmat.2017.07.028 ↗
76. First-principles investigation of hydrogen interaction with TiC precipitates in α-Fe10.1103/PhysRevB.93.184108 ↗