Morphological and microstructural characterizations of the fresh fuel plates for the SEMPER FIDELIS in-pile test
Source abstract
Abstract
The UMo/Al dispersion fuel in plate form is considered for the conversion of high-performance research reactors in Europe. In the framework of the UMo fuel qualification program, the adequate margin of safety performance by considering several technological solutions associated with the fabrication parameters, such as heat-treatment of the UMo particles, coating with a diffusion barrier material and powder size distribution as some examples. All these parameters, along with the effect of the hot-rolling process were evaluated by means of image processing and detailed microstructural characterizations for fresh samples i.e. prior to irradiation tests. Principle macroscopic features of powder batches include the size and shape distributions and coating surface examinations. Microscale investigations explored both the coating and kernel microstructures as well as the interface layer between them. Finally, nanoscale analyses examined the UMo–coating interface. The extensive stresses associated with the hot-rolling process have a significant impact on the deformation of the UMo kernels and the degradation of the coated film. The UMo kernels mostly lost their spherical shape for faceted and elongated shapes whereas three types of film degradations were identified including cracks, chippings and delamination.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Development of very-high-density low-enriched-uranium fuels10.1016/S0029-5493(97)00217-3 ↗
2. Review of 15 years of high-density lowenriched UMo dispersion fuel development for research reactors in Europe10.5516/NET.07.2014.703 ↗
3. Low-temperature irradiation behavior of uranium-molybdenum alloy dispersion fuel10.1016/S0022-3115(02)00850-4 ↗
4. Full-sized plates irradiation with high UMo fuel loading - final results Of IRIS 1 experiment
5. Transmission electron microscopy investigation of irradiated U-7 wt%Mo dispersion fuel10.1016/j.jnucmat.2007.12.006 ↗
6. Swelling of U(Mo)-Al(Si) dispersion fuel under irradiation-non-destructive analyses of the LEONIDAS e-future plates10.1016/j.jnucmat.2012.06.045 ↗
7. The effect of Si-rich layer coating on U-Mo vs. Al interdiffusion10.5516/NET.2011.43.2.159 ↗
8. Fuel swelling and interaction layer formation in the SELENIUM Si and ZrN coated U(Mo) dispersion fuel plates irradiated at high power in BR210.1016/j.jnucmat.2014.12.073 ↗
9. TEM analysis of irradiation-induced interaction layers in coated UMo/X/Al trilayer systems (X= Ti, Nb, Zr, and Mo)10.1016/j.jnucmat.2017.12.015 ↗
10. Effectiveness of the metal coating on U–7Mo dispersion fuel in Al during irradiation
11. High burn-up structure of U(Mo) dispersion fuel10.1016/j.jnucmat.2016.04.035 ↗
12. 3D reconstructions of irradiated U–Mo fuel to understand breaching effects in ZrN diffusion barriers10.1016/j.jnucmat.2018.08.016 ↗
13. Transmission electron microscopy investigation of neutron irradiated Si and ZrN coated UMo particles prepared using FIB10.1016/j.jnucmat.2017.10.016 ↗
14. Microstructural characterization of as-fabricated and irradiated U-Mo fuel using SEM/EBSD10.1016/j.jnucmat.2018.06.007 ↗
15. Stepnik · 2018
16. ZrN coating as diffusion barrier in U(Mo) dispersion fuel systems10.1016/j.jnucmat.2021.153000 ↗
17. Morphological characterization of the fresh ZrN coated UMo powders used in EMPIrE irradiation experiment: a practical approach
18. Characterization of fresh EMPIrE and SEMPER FIDELIS U(Mo)/Al fuel plates made with PVD-coated U(Mo) particles10.1051/epjn/2018048 ↗
19. Characterization of U-2 wt% Mo and U-10 wt% Mo alloy powders prepared by centrifugal atomization10.1016/S0022-3115(97)00011-1 ↗
20. Schenk · 2013
21. Surface engineering of low enriched uranium-molybdenum10.1016/j.jnucmat.2013.04.068 ↗
22. NIH Image to ImageJ : 25 years of image analysis10.1038/nmeth.2089 ↗
23. Recent developments of the program FULLPROF
24. Comparative analysis of the coating thickness on single particles using X-ray micro-computed tomography and confocal laser-scanning microscopy10.1016/j.powtec.2015.09.039 ↗
25. Dependence of thickness, morphology, and crystallographic properties of Mo and ZrN coatings on U-Mo substrate size10.1016/j.jnucmat.2018.10.012 ↗
26. Microstructural characterization of a thin film ZrN diffusion barrier in an As-fabricated U-7Mo/Al matrix dispersion fuel plate10.1016/j.jnucmat.2014.12.036 ↗
27. Effect of coating thickness and annealing temperature on ZrN coating failure of U-Mo particles under heat treatment10.1016/j.jnucmat.2018.05.019 ↗
28. STEM-EDS/EELS and APT characterization of ZrN coatings on UMo fuel kernels10.1016/j.jnucmat.2018.09.004 ↗
29. Neutron diffraction analyses of U-(6-10 wt.%)Mo alloy powders fabricated by centrifugal atomization10.1016/j.jnucmat.2009.11.026 ↗
30. Microstructure of as atomized and annealed U-Mo7 particles: a SEM/EBSD study of grain growth10.1016/j.jnucmat.2017.07.056 ↗
31. Microstructure of as-fabricated UMo/Al(Si) plates prepared with ground and atomized powder10.1016/j.jnucmat.2013.03.021 ↗
32. Crystallographic study of Si and ZrN coated U-Mo atomised particles and of their interaction with Al under thermal annealing10.1016/j.jnucmat.2013.08.050 ↗
33. Nanocrystalline ZrN thin film development via atomic layer deposition for U-Mo powder10.1016/j.jnucmat.2019.151770 ↗
34. A critical review of the microstructure of U–Mo fuels10.1016/j.jnucmat.2020.152386 ↗
35. Hydrogen accumulation in and at the perimeter of U-C-N-O inclusions in uranium - A SIMS analysis10.1016/j.jallcom.2015.01.050 ↗
36. Thermal expansion in UO2 determined by high-energy X-ray diffraction10.1016/j.jnucmat.2016.06.042 ↗
37. High-temperature thermal lattice expansion of mixed carbo-nitride and uranium carbo-nitride10.1016/0022-3115(71)90150-4 ↗
38. Austin · 1958