Reductive precipitation of neptunium on iron surfaces under anaerobic conditions
Source abstract
Abstract
Abstract Reductive precipitation of the radiotoxic nuclide 237Np from nuclear waste on the surface of iron canister material at simulated deep repository conditions was investigated. Pristine polished as well as pre-corroded iron specimens were interacted in a deoxygenated solution containing 10–100 μM Np(V), with 10 mM NaCl and 2 mM NaHCO3 as background electrolytes. The reactivity of each of the two different systems was investigated by analyzing the temporal evolution of the Np concentration in the reservoir. It was observed that pre-oxidized iron specimen with a 40 μm Fe3O4 corrosion layer are considerably more reactive regarding the reduction and immobilization of aqueous Np(V) as compared to pristine polished Fe(0) surfaces. 237Np immobilized by the reactive iron surfaces was characterized by scanning electron microscopy as well as synchrotron-based micro-X-ray fluorescence and X-ray absorption spectroscopy. At the end of experiments, a 5–8 μm thick Np-rich layer was observed to be formed ontop of the Fe3O4 corrosion layer on the iron specimen. The findings from this work are significant in the context of performance assessments of deep geologic repositories using iron as high level radioactive waste (HLW) canister material and are of relevance regarding removing pollutants from contaminated soil or groundwater aquifer systems.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Radioactive element chemistry and processing · Nuclear Materials and Properties · Environmental remediation with nanomaterials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. 2015
2. 2010
3. The Swedish KBS project: a last word in nuclear fuel safety prepares to conquer the world?10.1080/13669870903126077 ↗
4. Methodology to make a robust estimation of the carbon steel overpack lifetime with respect to the Belgian Supercontainer design10.1016/j.jnucmat.2008.06.020 ↗
5. Water worldwide: pilot study of radionuclide removal using conventional iron- and manganese-removal equipment10.1002/j.1551-8833.2008.tb09673.x ↗
6. Chemical effects at the reaction front in corroding spent nuclear fuel
7. Processes controlling radionuclide release from spent fuel
8. Solubility of mixed-valence U(IV–VI) and Np(IV–V) hydroxides in simulated groundwater and 0.1 M NaClO4 solutions10.1134/S1066362206050122 ↗
9. The reduction of U(VI) on corroded iron under anoxic conditions10.1524/ract.2002.90.9-11_2002.623 ↗
10. Reductive immobilization of Se-79 by iron canister under simulated repository environment10.1007/s10967-009-0328-8 ↗
11. Immobilization of selenate by iron in aqueous solution under anoxic conditions and the influence of uranyl10.1016/j.jnucmat.2009.04.016 ↗
12. Nitrate reduction by zerovalent Iron: effects of formate, oxalate, citrate, chloride, sulfate, borate, and phosphate10.1021/es034650p ↗
13. Iop, Speciation of neptunium during sorption and diffusion in natural clay
14. ATHENA, ARTEMIS, HEPHAESTUS: data analysis for X-ray absorption spectroscopy using IFEFFIT10.1107/S0909049505012719 ↗
15. Assessment of the relevance of Coffinite formation within the near-field environment of spent nuclear fuel geological disposals
16. Np(IV)/Np(V) valence determinations from Np L3 edge XANES/EXAFS10.1016/j.talanta.2004.08.034 ↗
17. Spectroscopic investigations of Np(V/VI) redox speciation in hyperalkaline TMA-(OH, Cl) solutions10.1524/ract.2012.1948 ↗