Abstract

The white bright band (WBB) in the 52M/SA508–3 pulsed TIG joint is clearly visible after metallographic etching. Increased pulse frequency leads to enhancing oscillation of the molten pool and promoting deeper heat penetration. This results in the formation of the δ/γ phase boundary, facilitating martensite and Type II boundary formation within the WBB. High-frequency pulsing refines grain structure and increases grain boundaries, inhibiting helium bubble diffusion and growth. As frequency rises from 15 kHz to 50 kHz, WBB width increases from 20 μm to 35 μm, martensite proportion from 0 % to 77.1 %, and austenite grain size decreases 26.1 %.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Hydrogen embrittlement and corrosion behaviors in metals · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Study of type-II boundary behavior during SA508-3/EQ309L overlay weld interfacial failure process10.1016/j.jmatprotec.2017.04.009 ↗
2. Fusion boundary microstructure evolution associated with embrittlement of Ni-base alloy overlays applied to carbon steel10.1007/s40194-012-0007-1 ↗
3. Microstructural evolution and high temperature failure of ferritic to austenitic dissimilar welds10.1179/1743280412Y.0000000006 ↗
4. Microstructure and mechanical property of the fusion boundary region in an Alloy 182-low alloy steel dissimilar weld joint10.1007/s10853-010-4581-6 ↗
5. Carbon migration in 5Cr-0.5 Mo/21Cr-12Ni dissimilar metal welds10.1007/s11661-998-0211-1 ↗
6. Dissimilar welding of superduplex stainless steel/HSLA steel for offshore applications joined by GTAW10.4236/eng.2010.27069 ↗
7. Numerical investigation on residual stresses of the safe-end/nozzle dissimilar metal welded joint in CAP1400 nuclear power plants10.1007/s40195-018-0803-8 ↗
8. Experimental characterisation and numerical modelling of residual stresses in a nuclear safe-end dissimilar metal weld joint10.3390/met11081298 ↗
9. Role of A-TIG process in joining of martensitic and austenitic steels for ultra-supercritical power plants -a state of the art review10.1016/j.net.2022.03.003 ↗
10. Effect of welding parameters on mechanical properties and optimization of pulsed TIG welding of Al-Mg-Si alloy10.1007/s00170-008-1572-8 ↗
11. Methods to Improve TIG Welding Efficiency10.1007/s12666-024-03323-x ↗
12. Effect of fast-frequency pulsed waveforms on the microstructure and mechanical properties of Ti-6Al-4V alloy welded by FFP-TIG10.1016/j.jmrt.2022.07.126 ↗
13. Microstructure and high-temperature mechanical properties of Inconel 718 superalloy weldment affected by fast-frequency pulsed TIG welding10.1016/j.jmapro.2023.01.076 ↗
14. Refined weld microstructure and enhanced joint mechanical property of 1460 Al-Li alloys via double-pulsed variable polarity TIG arc welding10.1016/j.jmapro.2022.08.044 ↗
15. Microstructure and stress corrosion cracking of the fusion boundary region in an alloy 182-A533B low alloy steel dissimilar weld joint10.1016/j.corsci.2010.08.002 ↗
16. A thermo-kinetic model for martensitic transformation kinetics in low-alloy steels10.1016/j.jallcom.2015.05.266 ↗
17. Microstructure evolution during tempering of martensitic Fe-C-Cr alloys at 700 A °C10.1007/s10853-018-2036-7 ↗
18. Microstructure, residual stress and mechanical properties of a high strength steel weld using low transformation temperature welding wires10.1016/j.matdes.2014.10.013 ↗
19. Ferritic-Austenitic Solidification Mode in Austenitic Stainless-Steel Welds10.1007/BF02661201 ↗
20. Nature and evolution of the fusion boundary in ferritic-austenitic dissimilar weld metals, Part 1 - Nucleation and growth
21. Nature and evolution of the fusion boundary in ferritic-austenitic dissimilar metal welds - Part 2: on-cooling transformations
22. Penetration increase of AISI 304 using ultrasonic assisted tungsten inert gas welding10.1179/136217109X12505932584772 ↗
23. Effects of Fe concentration on helium bubble formation in NiFe single-phase concentrated solid solution alloys10.1016/j.mtla.2018.100183 ↗
24. Investigating effects of alloy chemical complexity on helium bubble formation by accurate segregation measurements using atom probe tomography10.1017/S1431927619008523 ↗