journal article·2017-06

Study of the hoop fracture behaviour of nuclear fuel cladding from ring compression tests by means of non-linear optimization techniques

F.J. Gómez, M.A. Martin Rengel, J. Ruiz-Hervias, M.A. Puerta

Publisher page

Abstract

Abstract In this work, the hoop fracture toughness of ZIRLO® fuel cladding is calculated as a function of three parameters: hydrogen concentration, temperature and displacement rate. To this end, pre-hydrided samples with nominal hydrogen concentrations of 0 (as-received), 150, 250, 500, 1200 and 2000 ppm were prepared. Hydrogen was precipitated as zirconium hydrides in the shape of platelets oriented along the hoop direction. Ring Compression Tests (RCTs) were conducted at three temperatures (20, 135 and 300 °C) and two displacement rates (0.5 and 100 mm/min). A new method has been proposed in this paper which allows the determination of fracture toughness from ring compression tests. The proposed method combines the experimental results, the cohesive crack model, finite elements simulations, numerical calculations and non-linear optimization techniques. The parameters of the cohesive crack model were calculated by minimizing the difference between the experimental data and the numerical results. An almost perfect fitting of the experimental results is achieved by this method. In addition, an estimation of the error in the calculated fracture toughness is also provided.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear and radioactivity studies · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Arsene · 1997
2. Grange · 1998
3. Effects of hydrogen content and temperature on fracture toughness of Zircaloy-410.1016/S0022-3115(03)00193-4 ↗
4. Martín-Rengel · 2009
5. Revisting the method to obtain the mechanical properties of hydride fuel cladding in hoop direction10.1016/j.jnucmat.2012.06.003 ↗
6. Determination of the hoop fracture properties of unirradiated hydrogen- charged nuclear fuel cladding from ring compression tests10.1016/j.jnucmat.2013.01.311 ↗
7. Effects of hydride morphology on the embrittlement of Zircaloy-4 cladding10.1016/j.jnucmat.2014.09.025 ↗
8. Ductile-to-brittle transition temperature for high-burnup cladding alloys exposed to simulated drying- storage conditions10.1016/j.jnucmat.2012.10.002 ↗
9. Billone · 2014 · 000052
10. Billone · 2015 · 000008
11. Hydrides reorientation investigation of high burn-up PWR fuel cladding10.1016/j.jnucmat.2015.05.003 ↗
12. Desquines · J. ASTM Int. · 2005 · 2
13. Texture development and anisotropic deformation of zircaloys10.1016/j.pnucene.2005.09.011 ↗
14. Grigoriev · ASTM Spec. Tech. Publ. · 1996 · 1295 · 431
15. Crack growth in the through-thickness direction of hydride thin-walled Zircaloy sheet10.1016/j.jnucmat.2011.09.005 ↗
16. George · J. ASTM Int. · 2005 · 2
17. A new procedure to calculate the constitutive equation of nuclear fuel cladding from ring compression tests10.1016/j.pnucene.2017.02.001 ↗
18. Ravindran · 2006
19. Buljak · 2012
20. Proper orthogonal decomposition and radial basis functions in material characterization based on instrumented indentation10.1016/j.engstruct.2010.11.006 ↗