Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials
Source abstract
Abstract
Abstract This paper presents a review of recent experimental evidence and simulation results enumerating the development of the hydrogen-enhanced localized plasticity (HELP) mechanism as a viable hydrogen embrittlement mechanism for structural materials. A wide range of structural materials, including ferritic, martensitic, and austenitic steels, iron, and nickel are covered by the studies reviewed here, as are a variety of mechanical loading conditions and hydrogen charging conditions, supporting the concept that, despite differences in failure mode, there is a universality to the HELP mechanism.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. 2017
2. On some remarkable changes produced in iron and steel by the action of hydrogen and acids10.1098/rspl.1874.0024 ↗
3. Understanding how hydrogen influences the mechanical properties of iron and steel
4. Hydrogen embrittlement: mechanisms
5. “A new model for hydrogen-assisted cracking (hydrogen ‘embrittlement’)10.1007/BF02642048 ↗
6. An HVEM study of hydrogen effects on the deformation and fracture of nickel10.1016/0001-6160(86)90071-4 ↗
7. The influence of hydrogen on deformation and fracture processes in high-strength aluminum alloys10.1016/0001-6160(87)90076-9 ↗
8. Hydrogen embrittlement and grain boundary fracture10.1016/0036-9748(84)90407-1 ↗
9. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
10. Hydrogen effects on the character of dislocations in high-purity aluminum10.1016/S1359-6454(99)00156-1 ↗
11. Hydrogen interactions with defects in crystalline solids10.1103/RevModPhys.64.559 ↗
12. Atomistic simulations of hydrogen embrittlement10.1016/j.ijhydene.2009.09.052 ↗
13. Hydrogen-enhanced localized plasticity-a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
14. Mechanics of the hydrogen-dislocation-impurity interactions—I. Increasing shear modulus10.1016/0022-5096(94)00056-B ↗
15. Anomalous strain rate dependence of the serrated flow in Ni-H and Ni-C-H alloys10.1016/0956-7151(90)90206-V ↗
16. The portevin-Le chatelier effect in hydrogenated nickel alloys10.1007/BF02819254 ↗
17. Mechanisms of hydrogen related fracture―a review
18. Direct observations of the effect of hydrogen on the behavior of dislocations in iron10.1016/0036-9748(83)90268-5 ↗
19. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(01)00011-X ↗
20. Transmission electron microscopy observations and micromechanical/continuum models for the effect of hydrogen on the mechanical behaviour of metals10.1080/01418610208240451 ↗
21. Effects of hydrogen and carbon on thermally activated deformation in nickel10.1016/0956-7151(92)90438-K ↗
22. Effects of hydrogen on activation volume and density of mobile dislocations in iron-based alloy10.1016/j.msea.2012.10.100 ↗
23. The effect of hydrogen on the mechanical properties of high purity iron I. Softening and hardening of high purity iron by hydrogen charging during tensile deformation10.1016/0025-5416(79)90191-5 ↗
24. The effect of hydrogen on the mechanical properties of high purity iron II. Effect of quenched-in hydrogen below room temperature10.1016/0025-5416(79)90192-7 ↗
25. The effect of hydrogen on the mechanical properties of high purity iron III. The dependence of softening on specimen size and charging current density10.1016/0025-5416(79)90193-9 ↗
26. Hydrogen-enhanced localization of plasticity in an austenitic stainless steel10.1007/BF02669644 ↗
27. The effect of hydrogen on the solid solution strengthening and softening of nickel10.1016/0001-6160(82)90178-X ↗
28. Hydrogen embrittlement of metals10.1016/0025-5416(72)90109-7 ↗
29. Effect of impurity hydrogen on the deformation and fracture in an Al-5 mass pct Mg alloy10.1007/s11661-997-0186-3 ↗
30. Hydrogen embrittlement of α titanium: in situ TEM studies10.1016/0001-6160(88)90032-6 ↗
31. The influence of mobility of dissolved hydrogen on the elastic response of a metal10.1016/0022-5096(95)00037-J ↗
32. The influence of hydrogen on the stacking fault energy of an austenitic stainless steel10.4028/www.scientific.net/MSF.207-209.93 ↗
33. Increase in dislocation density in cold-deformed Pd using H as a temporary alloying addition10.1016/j.scriptamat.2013.01.005 ↗
34. Revisiting hydrogen embrittlement models and hydrogen-induced homogeneous nucleation of dislocations10.1016/j.scriptamat.2009.09.037 ↗
35. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation. I. Theoretical background10.1016/j.actamat.2007.05.047 ↗
36. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation II. Experimental evidence and consequences10.1016/j.actamat.2007.05.033 ↗
37. Hydrogen-enhanced local plasticity in aluminum: an ab initio study10.1103/PhysRevLett.87.095501 ↗
38. Atomistic simulations of effect of hydrogen on kink-pair energetics of screw dislocations in bcc iron10.1016/S1359-6454(02)00575-X ↗
39. Hydrogen-enhanced dislocation activity and vacancy formation during nanoindentation of nickel10.1103/PhysRevB.80.094113 ↗
40. Environmental effects on the dislocation arrangement of fatigued low alloy steel10.1016/0956-716X(90)90578-5 ↗
41. Ultrasonic investigation of the interaction of hydrogen-dislocations in copper crystals10.1016/j.msea.2011.02.033 ↗
42. Hydrogen Snoek-Koster relaxation in iron10.1088/0305-4608/17/4/011 ↗
43. Hydrogen effects on plasticity10.1016/S1572-4859(09)01504-6 ↗
44. Hydrogen diffusivities as a measure of relative dislocation densities in palladium and increase of the density by plastic deformation in the presence of dissolved hydrogen10.1016/j.actamat.2014.09.013 ↗
45. Influence of hydrogen on dislocation self-organization in Ni10.1016/j.actamat.2017.05.073 ↗
46. “Influence of hydrogen on the deformation morphology of vanadium (100) micropillars in the α-phase of the vanadium–hydrogen system10.1016/j.scriptamat.2012.09.020 ↗
47. Hydrogen effects on the plasticity of Fcc crystals
48. Hydrogen-enhanced plasticity and failure revisited
49. Mechanical properties of high-purity iron-carbon alloy at low temperature
50. Interpreting hydrogen-induced fracture surfaces in terms of deformation processes: a new approach10.1016/j.actamat.2011.03.002 ↗
51. The effect of diffusive hydrogen segregation on fracture of polycrystalline nickel10.1016/0001-6160(86)90010-6 ↗
52. Intergranular fracture of nickel: the effect of hydrogen-sulphur Co-segregation10.1016/0001-6160(87)90127-1 ↗
53. In-situ TEM observation of aluminum embrittlement by liquid gallium10.1016/S1359-6462(97)00464-8 ↗
54. Equilibrium aspects of hydrogen-induced cracking of steels10.1016/0001-6160(74)90061-3 ↗
55. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
56. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
57. Martin · 2012
58. Microstructural size effects on mechanical properties of high purity nickel10.1016/j.ijplas.2010.08.002 ↗
59. Hydrogen effect against hydrogen embrittlement10.1007/s11661-010-0275-6 ↗
60. A microstructural based understanding of hydrogen-enhanced fatigue of stainless steels10.1016/j.ijfatigue.2012.08.009 ↗
61. Effect of environment on fatigue crack wake dislocation structure in Al-Cu-Mg10.1007/s11661-012-1089-5 ↗
62. The kinetics and mechanism of titanium hydride formation10.1016/0022-5088(89)90529-8 ↗
63. “Microbeam analysis of hydrogen near a crack tip in titanium,” nucl10.1016/j.nimb.2007.03.035 ↗
64. Modeling hydrogen transport by dislocations10.1016/j.jmps.2015.03.002 ↗
65. Hydrogen embrittlement of high strength steels
66. Environment assisted cracking of steam turbine blade steels - a consistent rationalization based on hydrogen assisted cracking
67. Nagumo · 2016
68. Hydrogen embrittlement in ultrafine elongated grain structure steel processed by warm tempforming
69. Crystallographic analysis of hydrogen-related fracture in medium carbon martensitic steel
70. Effect of microstructure of martensite on hydrogen embrittlement in 8Ni-0.1C steel
71. The effect of nano-sized TiC precipitates on hydrogen embrittlement of tempered Lath Martensitic steel
72. Influence of microstructure and Ti(C,N) on the susceptibility to hydrogen embrittlement of AHSS grades for the automotive industry
73. Enhanced lattice defect formation associated with hydrogen and hydrogen embrittlement under elastic stress of a tempered martensitic steel10.2355/isijinternational.52.198 ↗
74. Microstructural and crystallographic features of hydrogen-related crack propagation in low carbon martensitic steel10.2355/isijinternational.52.208 ↗
75. Effect of uniform distribution of fine cementite on hydrogen embrittlement of low carbon martensitic steel plates10.2355/isijinternational.52.213 ↗
76. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
77. Orientation of cleavage facets in tempered martensite (quasi- cleavage) by single surface trace analysis10.1007/BF02665434 ↗
78. The nature of quasicleavage fracture in tempered 5.5Ni steel after hydrogen charging10.1007/BF02645559 ↗
79. Characterization of hydrogen-related fracture behavior in as-quenched low-carbon martensitic steel and tempered medium-carbon martensitic10.1007/s11661-015-3176-x ↗
80. Hydrogen environment assisted cracking of modern ultra-high strength martensitic steels10.1007/s11661-017-4156-0 ↗
81. Fracture surface topography analysis of the hydrogen-related fracture propagation process in martensitic steel10.1007/s10704-017-0182-6 ↗
82. Interpretation of hydrogen-induced fracture surface morphologies for lath martensitic steel10.1016/j.mspro.2014.06.274 ↗
83. Visualization of hydrogen transport in high strength steels affected by stress fields and hydrogen trapping10.1016/S1359-6462(01)01154-X ↗
84. Hydrogen embrittlement of stainless steels and their welds
85. Effects of hydrogen on fatigue crack growth behavior of austenitic stainless steels10.1016/j.ijhydene.2008.02.067 ↗
86. Hydrogen embrittlement properties of stainless and low alloy steels in high pressure gaseous hydrogen environment10.2355/isijinternational.52.234 ↗
87. Hydrogen embrittlement of austenitic stainless steel10.5006/0010-9312-21.2.53 ↗
88. Hydrogen effects on the properties and fracture modes of iron-based alloys
89. The influence of austenite stability on the hydrogen embrittlement and stress- corrosion cracking of stainless steel10.1007/BF02658313 ↗
90. Hydrogen-induced strain localization and failure of austenitic stainless steels at high hydrogen concentrations10.1016/0956-7151(91)90211-I ↗
91. San Marchi · 2012
92. Effects of alloy composition and strain hardening on tensile fracture of hydrogen-precharged type 316 stainless steels10.1016/j.ijhydene.2007.10.046 ↗
93. Hydrogen-assisted crack propagation in austenitic stainless steel fusion welds10.1007/s11661-009-9922-1 ↗
94. Hydrogen-assisted crack propagation in 304L/308L and 21Cr-6Ni-9Mn/308L austenitic stainless steel fusion welds10.1016/j.corsci.2012.03.046 ↗
95. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe–Mn–C alloys10.1016/j.msea.2004.01.059 ↗
96. Phase changes related to hydrogen-induced cracking in austenitic stainless steel10.1016/0001-6160(87)90081-2 ↗
97. Brittle fracture in austenitic steel10.1016/0956-7151(94)90300-X ↗
98. Effects of low temperature on hydrogen-assisted crack growth in forged 304L austenitic stainless steel10.1007/s11661-016-3563-y ↗
99. HVEM studies of the effects of hydrogen on the deformation and fracture of AISI type 316 austenitic stainless steel10.1016/0956-7151(90)90070-W ↗
100. Hydrogen effects on dislocation activity in austenitic stainless steel10.1016/j.actamat.2006.02.007 ↗