Enhancement of creep resistance through Ti-induced MX precipitation and lower tempering/post-weld heat treatment temperatures in gas tungsten arc and electron beam welded RAFM steels for nuclear fusion reactors
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Fusion materials and technologies · Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Nuclear fusion, an energy source10.1016/S0920-3796(97)00007-0 ↗
2. Is nuclear fusion a sustainable energy form?10.1016/j.fusengdes.2010.11.040 ↗
3. Back to the future: revisiting the perspectives on nuclear fusion and juxtaposition to existing energy sources10.1016/j.energy.2023.129150 ↗
4. Recent progress of R&D activities on reduced activation ferritic/martensitic steels10.1016/j.jnucmat.2012.12.039 ↗
5. Materials research for fusion10.1038/nphys3735 ↗
6. Influence of oxide inclusions on the creep properties of electron beam welds in Ti-added reduced activation ferritic/martensitic steel10.5781/JWJ.2024.42.3.6 ↗
7. Low-activation ferritic and martensitic steels for fusion application10.1016/S0022-3115(96)00327-3 ↗
8. Low cycle fatigue of EUROFER97 investigated for test blanket modules of ITER: an interlaboratory study10.1016/j.jnucmat.2024.155127 ↗
9. M. Rieth, M. Schirra, A. Falkenstein, P. Graf, S. Heger, H. Kempe, R. Lindau, H. Zimmermann, EUROFER 97. Tensile, charpy, creep and structural tests. Eurofusion Programme, Technical Report FZKA-6911, Germany, 2003.
10. Structural, thermal, electrical and magnetic properties of Eurofer 97 steel10.1016/j.jnucmat.2007.03.267 ↗
11. Mechanical properties and microstructure characterization of Eurofer97 steel variants in EUROfusion program10.1016/j.fusengdes.2019.03.158 ↗
12. Technological aspects in blanket design: effects of micro-alloying and thermo-mechanical treatments of EUROFER97 type steels after neutron irradiation10.1016/j.fusengdes.2021.112645 ↗
13. Ultra-fine grained EUROFER97 steel for nuclear fusion applications10.1016/j.jmrt.2024.10.069 ↗
14. Mechanical properties and microstructures of China low activation martensitic steel compared with JLF-110.1016/j.jnucmat.2007.03.012 ↗
15. An overview of the welding technologies of CLAM steels for fusion application10.1016/j.fusengdes.2012.06.009 ↗
16. Creep deformation and rupture behavior of CLAM steel at 823 K and 873 K10.1016/j.jnucmat.2014.08.041 ↗
17. Development status of CLAM steel for fusion application10.1016/j.jnucmat.2014.08.055 ↗
18. Effects of thermal aging on the mechanical behavior of F82H weldments10.1016/S0022-3115(00)00100-8 ↗
19. Microstructure of welded and thermal-aged low activation steel F82H IEA heat10.1016/S0022-3115(00)00089-1 ↗
20. Development of an extensive database of mechanical and physical properties for reduced-activation martensitic steel F82H10.1016/S0022-3115(02)01075-9 ↗
21. Swelling behavior of TIG-welded F82H IEA heat10.1016/S0022-3115(02)01200-X ↗
22. Physical properties of F82H for fusion blanket design10.1016/j.fusengdes.2013.12.005 ↗
23. Material properties of the F82H melted in an electric arc furnace10.1016/j.fusengdes.2015.06.103 ↗
24. Development of filler wires for welding of reduced activation ferritic martenstic steel for India’s test blanket module of ITER10.1016/j.fusengdes.2011.04.003 ↗
25. Development of India-specific RAFM steel through optimization of tungsten and tantalum contents for better combination of impact, tensile, low cycle fatigue and creep properties10.1016/j.jnucmat.2013.03.073 ↗
26. Development of IN-RAFM steel and fabrication technologies for Indian TBM10.1016/j.fusengdes.2015.12.005 ↗
27. Suppression of austenite grain coarsening by using Nb–Ti microalloying in high temperature carburizing of a gear steel10.1002/adem.201900132 ↗
28. Improving strength and ductility of low activation martensitic (LAM) steel by alloying with titanium and tempering10.1016/j.msea.2020.140152 ↗
29. Hot-deformation induced static recrystallization and nano-MX precipitation in a low activation martensitic steel10.1016/j.jnucmat.2021.153190 ↗
30. Review of candidate welding processes of RAFM steels for ITER test blanket modules DEMO10.1016/j.jnucmat.2010.12.248 ↗
31. Microstructural stability and mechanical property of novel high-Si high-Cr reduced activation ferritic/martensitic steels at high temperatures10.1016/j.jnucmat.2024.155602 ↗
32. Some studies on P91 steel and their weldments10.1016/j.jallcom.2018.01.120 ↗
33. Transition of creep damage region in dissimilar welds between Inconel 740H Ni-based superalloy and P92 ferritic/martensitic steel10.1016/j.matchar.2018.02.039 ↗
34. Review of type IV cracking of weldments in 9–12%Cr creep strength enhanced ferritic steels10.1179/1743280412Y.0000000016 ↗
35. Creep rupture behavior of 9Cr–1.8W–0.5Mo–VNb (ASME grade 92) ferritic steel weld joint10.1016/j.msea.2013.10.071 ↗
36. Effect of post weld heat treatments on microstructure evolution and type IV cracking behavior of the P91 steel welds joint10.1016/j.jmatprotec.2018.10.024 ↗
37. An investigation of microstructural evolution in electron beam welded RAFM steel and 316LN SS dissimilar joint under creep loading conditions10.1016/j.msea.2018.11.046 ↗
38. Optimization of electron beam welding joint of water-cooled ceramic breeder blanket10.3390/ma14123405 ↗
39. Role of multicomponent nanoprecipitates on strength and low-temperature toughness of simulated heat-affected zone (HAZ) in high-strength low-carbon steel10.1007/s12613-025-3245-0 ↗
40. Microstructure and tensile and charpy impact properties of reduced activation ferritic–martensitic steel with Ti10.1016/j.fusengdes.2017.05.085 ↗
41. Effects of Ti and Ta addition on microstructure stability and tensile properties of reduced activation ferritic/martensitic steel for nuclear fusion reactors10.1016/j.jnucmat.2018.01.008 ↗
42. Atomic scale identification of nano-sized precipitates of Ta/Ti-added RAFM steel and its superior creep strength10.1016/j.matchar.2020.110596 ↗
43. Influence of Ti addition on MX precipitation and creep-fatigue properties of RAFM steel for nuclear fusion reactor10.1016/j.jnucmat.2022.154001 ↗
44. Low cycle fatigue of irradiated and unirradiated Eurofer97 steel at 300 °C
45. A multi-scale microstructure to address the strength-ductility trade off in high strength steel for fusion reactors10.1038/s41467-025-58042-8 ↗
46. Tensile and charpy impact properties of reduced activation ferritic/martensitic steel with small amounts of Ta and Ti10.1016/j.jnucmat.2019.151862 ↗
47. Effect of post weld heat treatments on fracture frontier and type IV cracking nature of the crept P91 welded sample10.1016/j.msea.2018.06.038 ↗
48. Technical issues in fusion welding of reduced activation ferritic/martensitic steels for nuclear fusion reactors10.5781/JWJ.2020.38.1.5 ↗
49. The impact of weld metal creep strength on the overall creep strength of 9% Cr steel weldments10.1115/1.4003112 ↗
50. Thermal creep behaviour of the EUROFER 97 RAFM steel and two European ODS EUROFER 97 steels10.1016/j.fusengdes.2005.06.311 ↗
51. Klueh · 1996
52. Study on creep properties for TIG welded joints of CLAM steel10.1007/s10894-015-0024-3 ↗
53. H. Tanigawa, T. Nozawa, M. Ando, Summary report of joint research in Japan on BA DEMO R&D activity 2008 (Joint research), Japan Atomic Energy Agency, 2010.
54. Creep life prediction of 10CrMo9–10 steel by Larson–Miller model10.3390/ma15134431 ↗
55. Re-evaluation of tensile and creep rupture data of metals using a modified Larson–Miller approach10.1016/j.engfracmech.2025.111582 ↗
56. Type IV cracking in ferritic power plant steels10.1179/174328406X148778 ↗
57. Failure mechanisms of high temperature components in power plants10.1115/1.482794 ↗
58. Microstructure and creep strength of welds in advanced ferritic power plant steels10.1179/136217104225017107 ↗
59. Influence of microstructure on cavitation in the heat affected zone of a grade 92 steel weld during long-term high temperature creep10.1016/j.matchar.2020.110663 ↗
60. Creep cavitation in metals10.1016/S0749-6419(02)00111-0 ↗
61. Mechanism of microstructural deterioration preceding type IV failure in weldment of mod.9Cr-1Mo steel10.1007/s12540-015-4569-5 ↗
62. Dissolution of M23C6 and new phase re-precipitation in Fe ion-irradiated RAFM steel10.3390/met8050349 ↗
63. Creep behavior, deformation mechanisms, and creep life of mod. 9Cr–1Mo steel10.1007/s11661-015-3144-5 ↗
64. Strengthening mechanisms of reduced activation ferritic/martensitic steels: a review10.1007/s12613-020-2121-1 ↗