How brittle is 'too brittle'?: Comparative mechanical assessment of silicon carbide and post-quench steam-oxidized zirconium alloy cladding
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Accident tolerant fuel cladding development: promise, status, and challenges10.1016/j.jnucmat.2017.12.043 ↗
2. Koyanagi · 2018
3. A structural model for multi-layered ceramic cylinders and its application to silicon carbide cladding of light water reactor fuel10.1016/j.jnucmat.2014.12.013 ↗
4. Mechanical performance of SiC three-layer cladding in PWRs10.1016/j.nucengdes.2016.10.008 ↗
5. Fabrication and measurement of hoop strength of SiC triplex tube for nuclear fuel cladding applications10.1016/j.jnucmat.2014.11.117 ↗
6. Fiber/matrix debonding evaluation of SiCf/SiC composites using micropillar compression technique10.1016/j.compositesb.2021.109189 ↗
7. Oxidation behavior of sintered tubular silicon carbide in pure steam Ι: experiments10.1016/j.ceramint.2015.09.161 ↗
8. Oxidation behavior of sintered tubular silicon carbide in pure steam ΙΙ: weight-loss correlation developments10.1016/j.ceramint.2015.11.117 ↗
9. Oxidation at high temperatures in steam atmosphere and quench of silicon carbide composites for nuclear application10.1016/j.nucengdes.2015.10.002 ↗
10. D.F. Wilson, Chemical compatibility issues associated with use of SiC/SiC in advanced reactor concepts, (2012) 16. http://www.ntis.gov/support/ordernowabout.htm.
11. Compatibility of CVD SiC and SiCf/SiC composites with high temperature helium simulating very high temperature gas-cooled reactor coolant chemistry10.1007/s11085-012-9346-y ↗
12. Characteristics of composite silicon carbide fuel cladding after irradiation under simulated PWR conditions10.13182/NT12-86 ↗
13. Design optimization of multi-layer Silicon Carbide cladding for light water reactors10.1016/j.nucengdes.2016.11.016 ↗
14. Development of a 2D axisymmetric SiC cladding mechanical model and its applications for steady-state and LBLOCA analysis10.1016/j.jnucmat.2021.153311 ↗
15. Response to internal pressure shock and hoop strength of SiCf/SiC cladding10.1016/j.jeurceramsoc.2024.04.002 ↗
16. Analysis of multi-scale failure behavior of SiCf/SiC composite clad tube under flexible clamping damage10.1016/j.jeurceramsoc.2024.04.016 ↗
17. Experimental investigation of probabilistic failure of SiC/SiC composite tubes under multiaxial loading10.1016/j.compstruct.2024.118002 ↗
18. Fabrication and material issues for the application of SiC composites to LWR fuel cladding10.5516/NET.07.2012.084 ↗
19. Billone
20. U.S. NRC, Regulatory guide 1.223-determing post quench ductility, 09 (2016).
21. Stress analysis and probabilistic assessment of multi-layer SiC-based accident tolerant nuclear fuel cladding10.1016/j.jnucmat.2015.08.001 ↗
22. Thermophysical properties of porous SiC ceramics fabricated by pressureless sintering10.1016/j.stam.2007.08.003 ↗
23. Farhad Mohammadi-Koumleh, silicon carbide multilayer piping for high temperature sCO 2 brayton cycle
24. Ring compression properties of SiCf/SiC composites prepared by chemical vapor infiltration10.1016/j.ceramint.2018.09.024 ↗
25. Post-quench ductility limits of coated ATF with various zirconium-based alloys and coating designs10.1016/j.jnucmat.2024.154915 ↗
26. The kinetics of oxidation of Zircaloy-4 in steam at high temperatures10.1149/1.2129227 ↗
27. High temperature oxidation of SiC under helium with low-pressure oxygen. Part 3: β-SiC-SiC/PyC/SiC10.1016/j.jeurceramsoc.2011.08.005 ↗