Effect of Na2O on aqueous dissolution of nuclear waste glasses
Source abstract
Abstract
Abstract Sodium oxide is present in the majority of commercial and waste glasses as a viscosity-reducing component. In some nuclear waste glasses, its source is the waste itself. As such, it can limit the waste loading because of its deleterious effect on the resistance of the glass to attack by aqueous media. The maximum tolerable content of Na2O in glass depends on the presence and concentration of components that interact with it. To assess the acceptability limits of Na2O in the composition region of nuclear waste glasses, we formulated 11 baseline compositions by varying the content of oxides of Si, B, Al, Ca, Zr, and Li. In each of these compositions, we varied the Na2O fraction from 8–16 mass% to 23–30 mass%. To each of 146 glasses thus formulated, we applied the seven-day Product Consistency Test (PCT) to determine normalized B and Na releases (ri, where i ≡ B or Na). Fitting approximation functions ln(ri/gm−2) = Σbijgj to ri data (gj is the j-th component mass fraction and bij the corresponding component coefficient), we showed that the rB (and, consequently, the initial glass alteration rate) was proportional to the glass component mass fractions in the order Al2O3
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · Recycling and utilization of industrial and municipal waste in materials production · Clay minerals and soil interactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. The fate of silicon during glass corrosion under alkaline conditions: a mechanistic and kinetic study with the international simple glass10.1016/j.gca.2014.12.009 ↗
2. Origin and consequences of silicate glass passivation by surface layers10.1038/ncomms7360 ↗
3. Current understanding and remaining challenges in modeling long-term degradation of borosilicate nuclear waste glasses10.1111/ijag.12050 ↗
4. Characteristics of alteration layers formed on simulated HLW glass under silica-saturated solutions
5. Crystalline-like ordering in melt-quenched network glasses?10.1016/j.jnoncrysol.2013.12.012 ↗
6. An hypothesis on the nature of griffith's cracks in alkali silicate and silica glasses
7. Effect of composition on the short-term and long-term dissolution rates of ten borosilicate glasses of increasing complexity from 3 to 30 oxides10.1016/j.jnoncrysol.2012.05.024 ↗
8. Resumption of nuclear glass alteration: State of the art10.1016/j.jnucmat.2014.02.022 ↗
9. Present understanding of R7T7 glass alteration kinetics and their impact on long-term behavior modeling10.1016/S0022-3115(01)00643-2 ↗
10. Vienna · 2013
11. An international initiative on long-term behavior of high-level nuclear waste glass10.1016/j.mattod.2013.06.008 ↗
12. C1285 e 14 ASTM · 2008
13. Leaching of borosilicate glasses, I. Experiments10.1016/j.jnoncrysol.2004.06.006 ↗
14. The effect of composition on the leaching of three nuclear waste glasses: R7T7, AVM and VRZ
15. High-temperature viscosity of many-component glass melts10.1016/j.jnoncrysol.2016.01.007 ↗
16. Nonlinear relationship between the Product Consistency Test (PCT) response and the Al/B ratio in a soda-lime aluminoborosilicate glass10.1016/j.jnucmat.2016.02.017 ↗
17. Bellman · 2003