journal article·2022-10

T-REX: Numerical tool for tungsten damage assessment for DEMO

A. Durif, M. Richou, J.-M. Bergheau, L. Gallais, G. Kermouche, G. Pintsuk

Publisher page

Abstract

One of the R&D focus in the European fusion energy program is to establish a physical and technological basis for reliable power exhaust during entire operational situations of a DEMOstrational power plant. Following the design adopted for ITER, the baseline Plasma Facing Component for DEMO divertor is made of tungsten as armor material. The tungsten divertor target are the most thermally loaded in-vessel components in fusion reactor. The PFCs lifetime is affected by material degradations under the different loadings including High Heat Flux (HHF) and neutron irradiation. It has been reported a loss of mechanical properties due to softening (restoration/recrystallization). Latest finite element modeling developments allow to estimate component lifetime under HHF loading taking into account the progressive mechanical properties change due to softening. We propose here to take into account the influence of thermal and neutron loadings on the tungsten mechanical properties change for PFC lifetime assessment. For this, up to date mechanical properties of tungsten, softened tungsten, and neutron-irradiated tungsten are used as input data in the tool named T-REX (for Tungsten-Response based on EXperimental data). This tool is implemented as a user subroutine in a finite elements code. The influence of the neutron irradiation is studied as function of the dpa dose, the incident heat flux intensity and the current defined divertor component geometries (ITER and DEMO). With the study performed, it is shown that the geometry may be optimized to reduce the damage induced by plasticity. The numerical results also highlights that the plastic strain increment obtained after each thermal cycle reduces with the dpa dose.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. The WEST programme: minimizing technology and operational risks of a full actively cooled tungsten divertor on ITER10.1016/j.fusengdes.2013.02.039 ↗
2. European DEMO design strategy and consequences for materials10.1088/1741-4326/57/9/092002 ↗
3. A full tungsten divertor for ITER: physics issues and design status10.1016/j.jnucmat.2013.01.008 ↗
4. Progress in the initial design activities for the european DEMOdivertor: subproject “cassette”10.1016/j.fusengdes.2017.03.018 ↗
5. In situ observation of tungsten plasma-facing components after the first phase of operation of the WEST tokamak10.1088/1741-4326/ac1dc6 ↗
6. Recrystallization at high temperature of two tungsten materials complying with the ITER specifications10.1016/j.jnucmat.2020.152418 ↗
7. Predicting the performance of tungsten in a fusion environment: a literature review10.1080/02670836.2016.1185260 ↗
8. Experimental investigation of the microstructural changes of tungsten monoblocks exposed to pulsed high heat loads10.1016/j.nme.2019.100716 ↗
9. Recrystallization kinetics of warm-rolled tungsten in the temperature range 1150–1350 c10.1016/j.jnucmat.2014.08.037 ↗
10. An attempt to assess recovery/recrystallization kinetics in tungsten at high temperature using statistical nanoindentation analysis10.3390/cryst11010037 ↗
11. ITER structural design criteria for in-vessel components (SDC-IC) appendix a: Materials design limit data, g74ma, 8 01-05-28w0.2, 2013.
12. Impact of tungsten recrystallization on ITER-like components for lifetime estimation10.1016/j.fusengdes.2018.11.003 ↗
13. W. Bahm, Nuclear fusion programme annual report of the assiociation forschungszentrum karlsruhe / euratom, January 2004 - December 2004. Technical report. 31.00.00; LK 01; Wissenschaftliche Berichte, FZKA-7117 (May 2005) EUR-21526-EN.
14. Fatigue behavior of rolled and forged tungsten at 25, 280 and 480 c10.1016/j.jnucmat.2015.06.032 ↗
15. Interpretation of the deep cracking phenomenon of tungsten monoblock targets observed in high-heat-flux fatigue tests at 20 MW/m210.1016/j.fusengdes.2015.09.008 ↗
16. Degradation of tungsten monoblock divertor under cyclic high heat flux loading10.1016/j.fusengdes.2017.04.102 ↗
17. Towards reliable design-by-analysis for divertor plasma facing components – guidelines for inelastic assessment (part 1: unirradiated)10.1016/j.fusengdes.2019.06.007 ↗
18. Numerical study of the influence of tungsten recrystallization on the divertor component lifetime
19. Irradiation hardening of pure tungsten exposed to neutron irradiation10.1016/j.jnucmat.2016.08.024 ↗
20. Neutron irradiation hardening across ITER diverter tungsten armor10.1016/j.ijrmhm.2020.105437 ↗
21. Neutron irradiation effects on the mechanical properties of powder metallurgical processed tungsten alloys10.1016/j.jnucmat.2019.151910 ↗
22. Tensile properties of powder-metallurgical-processed tungsten alloys after neutron irradiation near recrystallization temperatures10.1016/j.jnucmat.2020.152505 ↗
23. Effects of neutron irradiation on the brittle to ductile transition in single crystal tungsten10.1016/j.jnucmat.2019.151799 ↗
24. Fracture-mechanical properties of neutron irradiated ITER specification tungsten10.1016/j.jnucmat.2020.152761 ↗
25. Thermal diffusivity of tungsten irradiated with protons up to 5.8 dpa10.1016/j.jnucmat.2018.06.041 ↗
26. Materials testing facilities and programmes for fission and ion implantation damage10.1088/1741-4326/aa6a67 ↗
27. Towards a programme of testing and qualification for structural and plasma-facing materials in ‘fusion neutron’ environments10.1088/1741-4326/aa60af ↗
28. Mechanical properties of tungsten: recent research on modified tungsten materials in japan10.1016/j.jnucmat.2020.152506 ↗
29. Nuclear analyses for the design of the ITER-like plasma facing components vertical targets of the DEMO divertor10.1016/j.fusengdes.2020.111730 ↗
30. Need for and requirements for a neutron irradiation facility for fusion materials testing
31. Microscopic damage of tungsten exposed to deuterium–helium mixture plasma in PISCES and its impacts on retention property10.1016/j.jnucmat.2011.01.008 ↗
32. Helium effects on recovery and recrystallization of powder metallurgically processed tungsten
33. Thermal conductivity reduction of tungsten plasma facing material due to helium plasma irradiation in PISCES using the improved 3-omega method10.1016/j.jnucmat.2017.01.023 ↗
34. Temperature dependence of retarded recrystallisation in helium plasma-exposed tungsten
35. Retarded recrystallization of helium-exposed tungsten
36. Investigation of mechanical properties of stress-relieved and electron irradiated tungsten after hydrogen charging10.1016/j.nme.2018.08.003 ↗
37. Bergheau · 2014
38. Inverse identification of tungsten static recrystallization kinetics under high thermal flux10.1016/j.fusengdes.2019.02.141 ↗
39. Characterization of ITER tungsten qualification mock-ups exposed to high cyclic thermal loads
40. High heat flux testing of newly developed tungsten components for WEST10.1016/j.fusengdes.2021.112835 ↗
41. Progress of ITER full tungsten divertor technology qualification in japan10.1016/j.fusengdes.2015.03.009 ↗
42. High heat flux testing of mock-ups for a full tungsten ITER divertor10.1016/j.fusengdes.2011.02.012 ↗
43. Qualification and post-mortem chracterization of tungsten mock-ups exposed to cyclic high heat flux loading10.1016/j.fusengdes.2013.05.091 ↗
44. Self-castellation of tungsten monoblock under high heat flux loading and impact of material properties10.1016/j.nme.2016.10.025 ↗
45. J. Lemaitre, J. Chaboche, Sciences SUP. Science de l’ingénieur. Dunod(2004) Mécanique des matrériaux solides.
46. Tabor · 1951
47. High-heat-flux technologies for the european demo divertor targets: state-of-the-art and a review of the latest testing campaign10.1016/j.jnucmat.2020.152670 ↗
48. Assessment of the high heat flux performance of european DEMO divertor mock-ups
49. Structural lifetime assessment for the DEMO divertor targets: design-by-analysis approach and outstanding issues10.1016/j.fusengdes.2020.112203 ↗
50. Controlled irradiation hardening of tungsten by cyclic recrystallization