Fundamental effects of copper on dislocation loops and mechanical property of tungsten under irradiation
Source abstract
Abstract
Abstract Molecular dynamics simulations have been conducted to investigate the effects of Cu on point defects, dislocation loops, and mechanical properties of W under irradiation. A realistic n-body potential of W-Cu is first corrected by the universal short-range potential of Ziegler, Biersack and Littmark for the irradiation process. Based on this potential, the point defects and mechanical properties of W and W80Cu20 solid solutions under irradiation are derived and compared with each other. It is revealed that the addition of Cu could induce the uniform distribution of point defects of W, impede the formation of dislocation loops in W under irradiation, and fundamentally improve the irradiation resistance of W in terms of mechanical properties. The simulation results are in good agreement with relevant experimental and theoretical observations in the literature, and could provide a deep understanding of points defects and mechanical properties of W and WCu solid solutions under irradiation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fusion materials and technologies · Advanced materials and composites · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Tungsten alloys as radiation protection materials10.1016/S0168-9002(97)00392-6 ↗
2. Multimodal options for materials research to advance the basis for fusion energy in the ITER era10.1088/0029-5515/53/10/104024 ↗
3. Damage accumulation in ion-irradiated Ni-based concentrated solid-solution alloys10.1016/j.actamat.2016.02.048 ↗
4. Molecular dynamics simulation of ion ranges in the 1–100 keV energy range10.1016/0927-0256(94)00085-Q ↗
5. Coherent displacement of atoms during ion irradiation10.1038/17983 ↗
6. Materials challenges in nuclear energy10.1016/j.actamat.2012.11.004 ↗
7. The nature of high-energy radiation damage in iron10.1088/0953-8984/25/12/125402 ↗
8. Mechanical behavior of Cu-W interface systems upon tensile loading from molecular dynamics simulations10.1016/j.commatsci.2018.05.030 ↗
9. Strain-stress relationship and dislocation evolution of W–Cu bilayers from a constructed n-body W–Cu potential
10. From solid solutions to fully phase separated interpenetrating networks in sputter deposited “immiscible” W–Cu thin films10.1016/j.actamat.2015.07.050 ↗
11. Effect of random surface orientation on W sputtering yields10.1016/j.nme.2018.08.002 ↗
12. Modeling of thermal stresses in a graded Cu/W joint10.1016/S0022-3115(02)00820-6 ↗
13. NIST-JANAF thermochemical tables fourth edition
14. Doping of helium at Fe/W interfaces from first principles calculation10.1016/j.jallcom.2016.05.186 ↗
15. Boer · 1988 · 1
16. Metastable phase formed in immiscible Cu–W multilayers by ion mixing10.1143/JJAP.42.7009 ↗
17. Research on Cu–W homogeneous film structure prepared by ion beam sputtering10.1016/j.jallcom.2010.02.020 ↗
18. Stability of amorphous Cu/Ta and Cu/W alloys10.1063/1.335855 ↗
19. Structural, thermodynamic, and mechanical properties of WCu solid solutions10.1016/j.jpcs.2017.06.034 ↗
20. Design of tungsten/copper graded composite for high heat flux components10.1016/0920-3796(95)00432-7 ↗
21. Microstructure evolution in tungsten during low-energy helium ion irradiation10.1016/S0022-3115(00)00289-0 ↗
22. High temperature annealing of ion irradiated tungsten10.1016/j.actamat.2015.01.067 ↗
23. Research status and issues of tungsten plasma facing materials for ITER and beyond10.1016/j.fusengdes.2014.02.078 ↗
24. Simulation of neutron-induced damage in tungsten by irradiation with energetic self-ions10.1016/j.jnucmat.2015.02.004 ↗
25. Molecular dynamics simulation of irradiation damage in tungsten10.1016/j.nimb.2007.10.003 ↗
26. Structure and metastability of mesoscopic vacancy and interstitial loop defects in iron and tungsten10.1088/0953-8984/20/34/345214 ↗
27. High-flux He+ irradiation effects on surface damages of tungsten under ITER relevant conditions10.1016/j.jnucmat.2016.01.001 ↗
28. Material erosion at the vessel walls of future fusion devices10.1016/S0022-3115(02)01580-5 ↗
29. SRIM–the stopping and range of ions in matter (2010)10.1016/j.nimb.2010.02.091 ↗
30. The stopping and ranges of ions in solids
31. Fast parallel algorithms for short-range molecular dynamics10.1006/jcph.1995.1039 ↗
32. Semiempirical, quantum mechanical calculation of hydrogen embrittlement in metals10.1103/PhysRevLett.50.1285 ↗
33. Electron–ion coupling effects on radiation damage in cubic silicon carbide10.1088/0953-8984/25/23/235402 ↗
34. On the interaction of elementary particles. I
35. The Yukawa potential10.1016/0378-4371(89)90108-8 ↗
36. Very short-range interatomic potentials10.1063/1.453144 ↗
37. Interaction potentials for modeling of ion-surface scattering10.1016/j.nimb.2010.11.074 ↗
38. Defect production in collision cascades in elemental semiconductors and fcc metals10.1103/PhysRevB.57.7556 ↗
39. Thermodynamic mixing energy and heterogeneous diffusion uncover the mechanisms of radiation damage reduction in single-phase Ni-Fe alloys10.1016/j.actamat.2017.12.064 ↗
40. Mechanism of radiation damage reduction in equiatomic multicomponent single phase alloys10.1103/PhysRevLett.116.135504 ↗
41. Influence of chemical disorder on energy dissipation and defect evolution in concentrated solid solution alloys10.1038/ncomms9736 ↗
42. Automated identification and indexing of dislocations in crystal interfaces10.1088/0965-0393/20/8/085007 ↗
43. Mechanical properties of single-crystal tungsten irradiated in a mixed spectrum fission reactor10.1016/j.jnucmat.2019.02.050 ↗
44. Unprecedented irradiation resistance of nanocrystalline tungsten with equiaxed nanocrystalline grains to dislocation loop accumulation10.1016/j.actamat.2018.11.024 ↗
45. Tensile properties of powder-metallurgical-processed tungsten alloys after neutron irradiation near recrystallization temperatures10.1016/j.jnucmat.2020.152505 ↗
46. Three-dimensional scanning transmission electron microscopy of dislocation loops in tungsten10.1016/j.micron.2018.05.010 ↗
47. Ab initio scaling laws for the formation energy of nanosized interstitial defect clusters in iron, tungsten, and vanadium10.1103/PhysRevB.94.024103 ↗
48. Elastic trapping of dislocation loops in cascades in ion-irradiated tungsten foils10.1088/0953-8984/26/37/375701 ↗
49. Elastic fields, dipole tensors, and interaction between self-interstitial atom defects in bcc transition metals10.1103/PhysRevMaterials.2.033602 ↗
50. Self-interstitial atom defects in bcc transition metals: Group-specific trends10.1103/PhysRevB.73.020101 ↗
51. Multiscale modeling of crowdion and vacancy defects in body-centered-cubic transition metals10.1103/PhysRevB.76.054107 ↗
52. Pelleg · 2012