journal article·2018-12

Japanese activities of the R&D on silicon carbide composites in the broader approach period and beyond

Takashi Nozawa, Kazumi Ozawa, ChangHo Park, Joon-Soo Park, Akira Kohyama, Akira Hasegawa, Shuhei Nogami, Tatsuya Hinoki, Sosuke Kondo, Toyohiko Yano, Tamaki Shibayama, Bun Tsuchiya, Tatsuo Shikama, Shinji Nagata, Teruya Tanaka, Hirotomo Iwakiri, Yasushi Yamamoto, Satoshi Konishi, Ryuta Kasada, Masatoshi Kondo, Tomoaki Kunugi, Takehiko Yokomine, Yoshitaka Ueki, Nariaki Okubo, Tomitsugu Taguchi, Hiroyasu Tanigawa

Publisher page

Abstract

Abstract The R&D on SiC/SiC composites under the broader approach (BA) activities between Japan and the EU for fusion DEMO developed a fundamental database of mechanical (Task-1) and physical/chemical (Task-2) properties, with a primary target of the application of SiC/SiC composites as functional structure to be used in the dual coolant breeding blanket concept. This paper aims to summarize previous 10-years activities of the R&D of Japan and to provide the key deliverables toward the DEMO design. In Task-1, good creep and fatigue durability were first demonstrated. Besides, in-plane and inter-laminar strength anisotropy maps at elevated temperatures were comprehensively identified. In parallel, the irradiation effects of SiC materials were specifically determined as input parameters of the analytical model to provide for the irradiation-induced residual stresses. In Task-2, the apparent dose-dependence of the radiation-induced electrical conductivity and the indicative radiation-induced electrical degradation was identified by various irradiation sources. In addition, good gas confinement was identified. Furthermore, no accelerated corrosion for duration of 3000 h at below 1173 K was first demonstrated. With these achievements, it is suggested that the in-vessel component technology, e.g., material corrosion database development, activated corrosion product evaluation code development, compact module tests for validation of the key functions of the components, technology integration assessment for fusion nuclear tests, etc., should be further developed toward DEMO in near-term.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Fusion materials and technologies · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. DEMO and fusion power plant conceptual studies in Europe10.1016/j.fusengdes.2005.08.055 ↗
2. Status of the design and performances of the WCLL test blanket module for ITER-FEAT10.1016/S0920-3796(02)00108-4 ↗
3. The European power plant conceptual study: helium-cooled lithium–lead reactor concept10.1016/j.fusengdes.2006.07.056 ↗
4. Evaluation of tensile properties of SiC/SiC composites with miniaturized specimens10.2320/matertrans.46.543 ↗
5. Tensile test technique for composites using small notched specimens10.1016/j.jnucmat.2011.01.070 ↗
6. Cracking resistance of silicon carbide composites by single- and double-notched specimen techniques10.1111/j.1744-7402.2009.02469.x ↗
7. Determination and prediction of axial/off-axial mechanical properties of SiC/SiC composites10.1016/j.fusengdes.2012.02.026 ↗
8. Tensile, compressive and in-plane/inter-laminar shear failure behavior of CVI- and NITE-SiC/SiC composites10.1088/1757-899X/18/16/162011 ↗
9. Transthickness tensile strength of SiC/SiC composites10.1002/9780470294826.ch58 ↗
10. High-temperature interlaminar tension test method development for ceramic matrix composites
11. Stress envelope of silicon carbide composites at elevated temperatures10.1016/j.fusengdes.2013.12.032 ↗
12. Circumferential tensile test method for mechanical property evaluation of SiC/SiC tube10.1016/j.fusengdes.2015.12.047 ↗
13. Characterization of failure behavior of silicon carbide composites by acoustic emission10.1002/9781118217535.ch7 ↗
14. Re-defining failure envelopes for silicon carbide composites based on damage process analysis by acoustic emission10.1016/j.fusengdes.2013.05.054 ↗
15. Evaluation of damage accumulation behavior and strength anisotropy of NITE SiC/SiC composites by acoustic emission, digital image correlation and electrical resistivity monitoring10.1016/j.jnucmat.2014.08.043 ↗
16. Fatigue properties of SiC/SiC composites under various loading modes
17. K. Toyoshima, doctoral thesis, (2012) Kyoto University ((in Japanese)).
18. Creep and fatigue behavior in an enhanced SiC/SiC composite at high temperature10.1111/j.1151-2916.1998.tb02621.x ↗
19. Study on stress relaxation behavior of silicon carbide by BSR method10.1016/j.jnucmat.2011.02.004 ↗
20. Analysis of properties of fiber composites with anisotropic constituents10.1115/1.3424603 ↗
21. Chou · 1992
22. Mechanical properties of advanced SiC fiber composites irradiated at very high temperatures10.1016/j.jnucmat.2011.02.006 ↗
23. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
24. Microstructural analysis of secondary phases in silicon carbide fabricated with SiC nano-powder and sintering additives
25. Recovery behavior of point defects after low-dose neutron irradiation of sintered SiC by thermal diffusivity and swelling measurements10.1016/j.jnucmat.2010.12.178 ↗
26. Estimation of neutron-irradiation-induced defect in 3C-SiC from change in XRD peak shift and DFT study10.1016/j.jnucmat.2010.12.180 ↗
27. Recovery behavior of point defects after low-dose neutron irradiation at ∼423K of sintered 6H-SiC by lattice parameter and macroscopic length measurements10.1016/j.jnucmat.2013.01.296 ↗
28. Irradiation creep of 3C-SiC and microstructural understanding of the underlying mechanisms10.1016/j.jnucmat.2013.09.004 ↗
29. Electrical insulating performances of SiC materials under gamma-ray irradiation
30. Radiation induced changes in electrical conductivity of chemical vapor deposited silicon carbides under fast neutron and gamma-ray irradiations10.1016/j.fusengdes.2011.03.065 ↗
31. Dynamic measurements of radiation-induced electrical-property modifications in CVD-SiC under fast-neutron irradiation10.1016/j.jnucmat.2014.08.057 ↗
32. Radiation induced electrical degradation of CVD-SiC under gamma-ray and neutron irradiations
33. Evaluation of hydrogen isotope absorption/diffusion coefficient of CVD-SiC in high temperature10.1016/j.fusengdes.2014.01.039 ↗
34. Re-evaluation of SiC permeation coefficient at high temperature10.1016/j.fusengdes.2015.12.041 ↗
35. Deuterium permeation behavior of erbium oxide coating on austenitic, ferritic, and ferritic/martensitic steels10.1016/j.fusengdes.2008.12.030 ↗
36. Surface effects in diffusion measurements: deuterium permeation through Martensitic steel10.1238/Physica.Topical.094a00121 ↗
37. Retention and thermal release behavior of deuterium and helium implanted in SiC10.1016/j.jnucmat.2014.08.015 ↗
38. Linear-scaling ab-initio calculations for large and complex systems10.1002/(SICI)1521-3951(199909)215:1<809::AID-PSSB809>3.0.CO;2-0 ↗
39. Characterization of functional materials for liquid blanket systems by cathodoluminescence measurement10.1016/j.fusengdes.2017.04.095 ↗
40. C. Park, T. Nozawa, R. Kasada, S. Tosti, S. Konishi and H. Tanigawa, The Effect of wall Flow Velocity on Compatibility of SiC Materials with Liquid Pb-li alloy by Rotating Disc Testing for 3000 H up to 900 °C, Fusion Eng. Des. in press, Available online 21 March 2018.10.1016/j.fusengdes.2018.03.042 ↗
41. Study on fabrication method of lithium alloys with metal grains10.1016/j.fusengdes.2015.06.184 ↗
42. Experimental study on chemical behaviors of non-metal impurities in Pb, Pb-Bi and Pb-Li by temperature programmed desorption mass spectrometer analysis10.1585/pfr.11.2405076 ↗
43. Evaluation of thermal conductivity for liquid lead lithium alloys at various Li concentrations based on measurement and evaluation of density, thermal diffusivity and specific heat of alloys10.1016/j.fusengdes.2015.12.029 ↗