Abstract For ITER divertor Plasma Facing Components (PFCs), tens of thousands of armor/heat sink interfaces will be produced by the industry. Statistically, there is a probability that interfaces with defects be delivered. The defect detection with Non Destructive Techniques (NDT) is then a major challenge. NDT should provide a detectability threshold below the critical defect size. For a defect located all along the axial length of a component, the critical defect size at interface is about 50° for W monoblock (resp. 6 mm for W flat tile). It is defined with thermo-mechanical fatigue behaviour under 10 MW m−2 for W monoblock (resp. 5 MW m−2 for W flat tile). The purpose of this paper is to study the armor/heat sink defect detection of tungsten components (flat tile and monoblock geometries) with SATIR test bed (Infrared thermography NDT). We demonstrate that SATIR is a relevant NDT to detect defect of W components.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (7)
Show source-provided references
1. R Raffray · Fusion Eng. Des. · 2010 · 85 · 9310.1016/j.fusengdes.2009.08.002 ↗
2. Merola · Fusion Eng. Des. · 2005 · 75–79 · 32510.1016/j.fusengdes.2005.06.139 ↗
3. Schlosser · Fusion Eng. Des. · 2001 · 56–57 · 30910.1016/S0920-3796(01)00317-9 ↗
4. Missirlian · Fusion Eng. Des. · 2005 · 75–79 · 43510.1016/j.fusengdes.2005.06.168 ↗
5. Escourbiac · Fusion Eng. Des. · 2009 · 84 · 74710.1016/j.fusengdes.2009.01.072 ↗
6. Durocher · Fusion Eng. Des. · 2009 · 84 · 31410.1016/j.fusengdes.2008.12.095 ↗
7. Richou · Fusion Eng. Des. · 2009 · 84 · 159310.1016/j.fusengdes.2008.12.121 ↗