In LWR fuel claddings the embrittlement due to hydrogen precipitates (i.e., hydrides) is a degrading mechanism that concerns in nuclear safety, particularly in dry storage. A relevant factor is the radial distribution of the hydrogen absorbed, especially the hydride rim formed. Thus, a reliable assessment of fuel performance should account for hydrogen migration. Based on the current state of modelling of hydrogen dynamics in the cladding, a 1D radial model has been derived and coupled with the FRAPCON code. The model includes the effect of the oxidation front progression on in-clad hydrogen migration, based on experimental observations found (i.e., dissolution/diffusion/re-precipitation of the hydrogen in the matrix ahead of the oxidation front). A remarkable quantitative impact of this new contribution has been shown by analyzing the hydrogen profile across the cladding of several high burnup fuel scenarios (>60 GW d/tU); other potential contributions like thermodiffusion and diffusion in the hydride phase hardly make any difference. Comparisons against PIE measurements allow concluding that the model accuracy notably increases when the effect of the oxidation front is accounted for in the hydride rim formation. In spite of the promising results, further validation would be needed
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. High burnup effects on fuel behaviour under accident conditions: the tests CABRI REP-Na10.1016/S0022-3115(98)00895-2 ↗
2. NEA · 2012
3. Cladding considerations for the transportation and storage of spent fuel
4. Ductile-to-brittle transition temperature for high-burnup cladding alloys exposed to simulated drying-storage conditions10.1016/j.jnucmat.2012.10.002 ↗
5. Hydride morphology and hydrogen embrittlement of Zircaloy fuel cladding used in NSRR/HBO experiment
6. Quantification and local distribution of hydrogen within Zircaloy-4 PWR nuclear fuel cladding tubes at the nuclear microprobe of the Pierre Süe Laboratory from μ-ERDA10.1016/j.nimb.2008.03.041 ↗
7. Hydrogen in zircaloy-2: its distribution and heat of transport10.1016/0022-3115(60)90004-0 ↗
8. A numerical calculation of the redistribution of an interstitial solute in a thermal gradient10.13182/NSE72-A22530 ↗
9. Modeling and simulation of hydrogen behavior in Zircaloy-4 fuel cladding10.1016/j.jnucmat.2014.05.013 ↗
10. Multidimensional simulations of hydrides during fuel rod lifecycle10.1016/j.jnucmat.2015.06.037 ↗
11. A new model of hydrogen redistribution in Zr alloy claddings during waterside corrosion in a temperature gradient10.1016/j.jnucmat.2016.01.032 ↗
12. Mechanism of corrosion of zirconium hydride and impact of precipitated hydrides on the Zircaloy-4 corrosion behaviour10.1016/j.corsci.2015.05.058 ↗
13. Geelhood · 2015
14. Hydride precipitation kinetics in Zircaloy-4 studied using synchrotron X-ray diffraction10.1016/j.jnucmat.2015.02.035 ↗
15. O'Donnell · 2001
16. The H_Zr (Hydrogen_Zirconium) system10.1007/BF02843318 ↗
17. The terminal solid solubility of hydrogen in zirconium alloys
18. The terminal solid solubility of hydrogen in irradiated Zircaloy-2 and microscopic modeling of hydride behavior10.1016/j.jnucmat.2009.01.017 ↗
19. Hydrogen pickup and redistribution in alpha-annealed Zircaloy-4
20. Sawatzky · 1961
21. Harkness · 1965
22. Thermotransport of hydrogen in Zircaloy-4 and modified Zircaloy-410.1016/S0022-3115(98)00430-9 ↗
23. Application of the BEPU methodology to assess fuel performance in dry storage10.1016/j.anucene.2016.08.029 ↗
24. Sahle · 2010