journal article·2011-12

High temperature dissolution of oxides in complexing media

Valil S. Sathyaseelan, Appadurai L. Rufus, Hariharan Subramanian, Anupkumar Bhaskarapillai, Shiny Wilson, Sevilimedu V. Narasimhan, Sankaralingam Velmurugan

Journal of Nuclear Materials· Volume 419· Issue 1-3
Publisher page

Abstract

Abstract Dissolution of transition metal oxides such as magnetite (Fe 3 O 4 ), mixed ferrites (NiFe 2 O 4 , ZnFe 2 O 4 , MgFe 2 O 4 ), bonaccordite (Ni 2 FeBO 5 ) and chromium oxide (Cr 2 O 3 ) in organic complexing media was attempted at higher temperatures (80–180 °C). On increasing the temperature from 80 to 180 °C, the dissolution rate of magnetite in nitrilo triacetic acid (NTA) medium increased six folds. The trend obtained for the dissolution of other oxides was ZnFe 2 O 4 > NiFe 2 O 4 > MgFe 2 O 4 > Cr 2 O 3 , which followed the same trend as the lability of their metal–oxo bonds. Other complexing agents such as ethylene diamine tetra acetic acid (EDTA), pyridine dicarboxylic acid (PDCA), citric acid and reducing agents viz., oxalic acid and ascorbic acid were also evaluated for their oxide dissolution efficiency at 160 °C. EDTA showed maximum dissolution rate of 21.4 μm/h for magnetite. Addition of oxalic acid/ascorbic acid to complexing media (NTA/EDTA) showed identical effect on the dissolution of magnetite. Addition of hydrazine, another reducing agent, to NTA decreased the rate of dissolution of magnetite by 50%.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Minerals Flotation and Separation Techniques · Iron oxide chemistry and applications · Extraction and Separation Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Rufus · BNES · 2000 · 1 · 192
2. Lister · Nucl. Technol. · 2002 · 140 · 28810.13182/NT02-A3340 ↗
3. Rufus · Prog. Nucl. Energy · 2004 · 44 · 1310.1016/S0149-1970(04)90005-4 ↗
4. Ayers · 1970
5. H. Ocken, K. Fruzzetti, P. Frattini, C.J. Wood, in: Int. Conf. Water Chemistry in Nuclear Reactors Systems, Chimie 2002, Avignon, France, 2002, pp. 25–41.
6. Velmurugan · J. Nucl. Sci. Technol. · 1996 · 33 · 64110.1080/18811248.1996.9731971 ↗
7. Halden In-reactor Test to Exhibit PWR Axial Offset Anomaly, EPRI Report 1008106, 2004.
8. Rufus · Prog. Nucl. Energy · 2001 · 39 · 28510.1016/S0149-1970(01)00004-X ↗
9. Afonso · J. Colloid Interf. Sci. · 1990 · 138 · 7410.1016/0021-9797(90)90181-M ↗
10. Shailaja · J. Nucl. Sci. Technol. · 1991 · 28 · 110710.1080/18811248.1991.9731477 ↗
11. Sawicki · J. Nucl. Mater. · 2008 · 374 · 24810.1016/j.jnucmat.2007.08.014 ↗
12. T. Swan, M.G. Segal, W.J. Williams, M.E. Pick, EPRI Report No. NP-5522 M, 1987.
13. Hocsman · J. Colloid Interf. Sci. · 2006 · 297 · 69610.1016/j.jcis.2005.11.020 ↗
14. Tamura · Corros. Sci. · 2001 · 43 · 167510.1016/S0010-938X(00)00171-2 ↗
15. Torres · J. Colloid Interf. Sci. · 1990 · 134 · 47510.1016/0021-9797(90)90157-J ↗
16. Panias · Hydrometallurgy · 1996 · 42 · 25710.1016/0304-386X(95)00104-O ↗
17. Rodenas · J. Solid State Chem. · 2008 · 181 · 235010.1016/j.jssc.2008.05.032 ↗
18. Gouda · Corros. Sci. · 1975 · 15 · 19910.1016/S0010-938X(75)80009-6 ↗
19. NIST Critically Selected Stability Constants of Metal Complexes, Version 8.0.
20. Zhang · Int. J. Miner. Process. · 2002 · 65 · 19110.1016/S0301-7516(01)00077-1 ↗