Surface damage of refractory high entropy alloys subject to He irradiation
Source abstract
Abstract
Tungsten is a leading material considered for nuclear fusion applications. However, W usually suffers from severe surface modification under exposure to He ions generated from fusion reactions. The development of high entropy alloys provides a feasible way to overcome such vulnerabilities. Herein, we explore the response of refractory multi-principal element alloys (MPEAs), WTaTi, WTaCrV, and WTaCrVTi under He implantation and compare the results with pure W. To this end, we have parameterized the interatomic interactions between the constitutive metals and He. With the developed empirical potential, we show that the formation and binding energies of He bubbles in MPEAs are lower than those in W, suggesting a reduced thermodynamical driving force to form large He bubbles in MPEAs. Simulations of He implantation further reveal that the distribution of injected He only weakly depends on the surface orientations in MPEAs. In addition, He bubbles in MPEAs are much smaller and discretely positioned. Our results suggest superior resistance of MPEAs to surface modifications under the impact of energetic He ions, rendering them promising candidate materials for nuclear reactors.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Entropy Alloys Studies · Nuclear Materials and Properties · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Tungsten as material for plasma-facing components in fusion devices10.1016/j.jnucmat.2011.01.110 ↗
2. Materials needs for fusion, Generation IV fission reactors and spallation neutron sources – similarities and differences10.1016/j.jnucmat.2004.04.016 ↗
3. Challenges and opportunities of modeling plasma–surface interactions in tungsten using high-performance computing10.1016/j.jnucmat.2014.11.072 ↗
4. Materials challenges in nuclear energy10.1016/j.actamat.2012.11.004 ↗
5. Recent progress in research on tungsten materials for nuclear fusion applications in Europe10.1016/j.jnucmat.2012.08.018 ↗
6. Development of next generation tempered and ODS reduced activation ferritic/martensitic steels for fusion energy applications10.1088/1741-4326/57/9/092005 ↗
7. Formation mechanism of bubbles and holes on tungsten surface with low-energy and high-flux helium plasma irradiation in NAGDIS-II10.1016/j.jnucmat.2004.04.129 ↗
8. Surface morphology and helium retention on tungsten exposed to low energy and high flux helium plasma10.1016/S0022-3115(02)01362-4 ↗
9. Comparison of tungsten nano-tendrils grown in Alcator C-Mod and linear plasma devices10.1016/j.jnucmat.2013.01.013 ↗
10. Tungsten surface evolution by helium bubble nucleation, growth and rupture10.1088/0029-5515/53/7/073015 ↗
11. Helium, hydrogen, and fuzz in plasma-facing materials10.1088/2053-1591/aa8c22 ↗
12. Effect of tungsten crystallographic orientation on He-ion-induced surface morphology changes10.1016/j.actamat.2013.09.045 ↗
13. Grain orientations and grain boundaries in tungsten nonotendril fuzz grown under divertor-like conditions10.1016/j.scriptamat.2016.09.018 ↗
14. Noble gas bubbles in bcc metals: ab initio-based theory and kinetic Monte Carlo modeling10.1016/j.actamat.2021.116961 ↗
15. Ab initio theory of noble gas atoms in bcc transition metals10.1039/C8CP01817K ↗
16. Helium accumulation in metals during irradiation – where do we stand?10.1016/j.jnucmat.2003.09.001 ↗
17. Behavior of tungsten under irradiation and plasma interaction10.1016/j.jnucmat.2019.03.035 ↗
18. Diffusion controlled helium bubble formation resistance of FeCoNiCr high-entropy alloy in the half-melting temperature regime10.1016/j.jnucmat.2019.151747 ↗
19. Effects of minor alloying addition on He bubble formation in the irradiated FeCoNiCr-based high-entropy alloys10.1016/j.jnucmat.2020.152458 ↗
20. Loop and void damage during heavy ion irradiation on nanocrystalline and coarse grained tungsten: microstructure, effect of dpa rate, temperature, and grain size10.1016/j.actamat.2018.02.035 ↗
21. A comparative study on the in situ helium irradiation behavior of tungsten: coarse grain vs. nanocrystalline grain10.1016/j.actamat.2018.01.015 ↗
22. Suppressing irradiation induced grain growth and defect accumulation in nanocrystalline tungsten through grain boundary doping10.1016/j.actamat.2021.116629 ↗
23. Recent progress of radiation response in nanostructured tungsten for nuclear application10.1007/s42864-021-00075-9 ↗
24. Limitations of W and W–1%La2O3 for use as structural materials10.1016/j.jnucmat.2005.03.013 ↗
25. High-entropy alloys: a critical review10.1080/21663831.2014.912690 ↗
26. A critical review of high entropy alloys and related concepts10.1016/j.actamat.2016.08.081 ↗
27. Influence of chemical disorder on energy dissipation and defect evolution in concentrated solid solution alloys10.1038/ncomms9736 ↗
28. Mechanism of Radiation Damage Reduction in Equiatomic Multicomponent Single Phase Alloys10.1103/PhysRevLett.116.135504 ↗
29. Atomic-level heterogeneity and defect dynamics in concentrated solid-solution alloys, Current Opinion in Solid State and
30. Helium irradiated cavity formation and defect energetics in Ni-based binary single-phase concentrated solid solution alloys10.1016/j.actamat.2018.10.040 ↗
31. Copepods drive large-scale trait-mediated effects in marine plankton10.1126/sciadv.aat5096 ↗
32. Radiation damage tolerance of a novel metastable refractory high entropy alloy V2.5Cr1.2WMoCo0.0410.1016/j.jnucmat.2020.152005 ↗
33. Effects of 3d electron configurations on helium bubble formation and void swelling in concentrated solid-solution alloys10.1016/j.actamat.2019.10.013 ↗
34. Chemical effects on He bubble superlattice formation in high entropy alloys, Current Opinion in Solid State and
35. Effects of temperature on helium cavity evolution in single-phase concentrated solid-solution alloys10.1016/j.jnucmat.2021.153261 ↗
36. Helium implantation damage resistance in nanocrystalline W-Ta-V-Cr high entropy alloys
37. Large-scale atomistic simulations of low-energy helium implantation into tungsten single crystals10.1016/j.actamat.2017.09.061 ↗
38. Loop punching and bubble rupture causing surface roughening —A model for W fuzz growth10.1209/0295-5075/105/25002 ↗
39. Helium bubble bursting in tungsten10.1063/1.4860315 ↗
40. Molecular dynamics and Monte Carlo hybrid simulation for fuzzy tungsten nanostructure formation10.1088/0029-5515/55/7/073013 ↗
41. Crystal orientation effects on helium ion depth distributions and adatom formation processes in plasma-facing tungsten10.1063/1.4897419 ↗
42. Pair potential for Fe–He10.1016/j.jnucmat.2008.08.029 ↗
43. Fast three dimensional migration of He clusters in bcc Fe and Fe–Cr alloys10.1063/1.3126709 ↗
44. Interatomic potentials for simulation of He bubble formation in W10.1016/j.jnucmat.2012.07.023 ↗
45. Development of a pair potential for Ta-He system10.1016/j.commatsci.2018.09.057 ↗
46. SRIM – The stopping and range of ions in matter (2010)
47. Ab initio molecular dynamics for liquid metals10.1103/PhysRevB.47.558 ↗
48. Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set10.1016/0927-0256(96)00008-0 ↗
49. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
50. Fast parallel algorithms for short-range molecular dynamics10.1006/jcph.1995.1039 ↗
51. A new interatomic potential function for helium10.1080/00268976800100381 ↗
52. Thermal stability of helium–vacancy clusters in iron10.1016/S0168-583X(02)01832-3 ↗
53. Visualization and analysis of atomistic simulation data with OVITO–the Open Visualization Tool10.1088/0965-0393/18/1/015012 ↗
54. First-principles study of He behavior in a NiCoFeCr concentrated solid–solution alloy10.1080/21663831.2019.1574926 ↗
55. Defect energetics of concentrated solid-solution alloys from ab initio calculations: ni0.5Co0.5, Ni0.5Fe0.5, Ni0.8Fe0.2 and Ni0.8Cr0.210.1039/C6CP05161H ↗
56. Defect accumulation and evolution in refractory multi-principal element alloys10.1016/j.actamat.2021.117233 ↗
57. Behavior of high-entropy W-rich alloys Wx(TaVCrTi)y under He+ irradiation10.1016/j.fusengdes.2021.112904 ↗
58. Defect properties in a VTaCrW equiatomic high entropy alloy (HEA) with the body centered cubic (bcc) structure10.1016/j.jmst.2019.10.025 ↗
59. Influence of crystal orientation on damages of tungsten exposed to helium plasma10.1016/j.jnucmat.2013.01.190 ↗
60. Tungsten ‘fuzz’ growth re-examined: the dependence on ion fluence in non-erosive and erosive helium plasma10.1088/0029-5515/55/9/093033 ↗