Crevice corrosion behaviors of Alloy 690 and 405 stainless steel in chloride solutions with different concentrations of thiosulfate
Source abstract
Abstract
The crevice corrosion behaviors of Alloy 690 and 405 stainless steel (SS) in chloride (Cl −) solutions with different concentrations of thiosulfate (S 2O 3 2−) were investigated using a self-designed electrochemical testing device for crevice corrosion. The increase of concentration ratio of Cl −/S 2O 3 2− promotes crevice corrosion of Alloy 690. When crevice corrosion occurs between Alloy 690 and 405 SS, Alloy 690 outside the crevice is used as the cathode for reduction reaction of O 2, and Alloy 690 inside the crevice is also used as the cathode for hydrogen evolution reaction, both of which jointly promote the anodic dissolution of 405 SS inside the crevice. The crevice corrosion mechanisms of Alloy 690 and 405 SS are also discussed.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Materials challenges in nuclear energy10.1016/j.actamat.2012.11.004 ↗
2. Nodular corrosion inside the crevice of Alloy 690 in deaerated high-temperature chloride solution
3. The oxidation of alloy 690 in simulated pressurized water reactor primary water
4. Crevice corrosion behavior of Alloy 690 in high-temperature water10.1016/j.jnucmat.2018.12.050 ↗
5. Quantitative assessment of submodes of stress corrosion cracking on the secondary side of steam generator tubing in pressurized water reactors: part Ⅰ10.5006/1.3277522 ↗
6. A mechanistic study on thiosulfate-enhanced passivity degradation of Alloy 800 in chloride solutions10.1016/j.electacta.2013.08.030 ↗
7. Passivation degradation of Alloy 800 in boiling solution containing thiosulphate10.1016/j.electacta.2017.03.037 ↗
8. Transport processes in steam generator crevices III. Experimental results10.1016/S0010-938X(01)00029-4 ↗
9. A mechanistic study of sulfur-induced passivity degradation of Alloy 800 in a simulated alkaline crevice environment at 300 °C10.1007/s10008-015-2822-y ↗
10. Effects of 405 stainless steel on crevice corrosion behavior of Alloy 690 in high-temperature pure water10.1016/j.jmst.2020.02.004 ↗
11. Fretting wear between Alloy 690 and 405 stainless steel in high temperature pressurized water with different normal force and displacement10.1016/j.jnucmat.2019.151930 ↗
12. Effect of the frequency on fretting corrosion behavior between Alloy 690TT tube and 405 stainless steel plate in high temperature pressurized water10.1016/j.triboint.2021.107229 ↗
13. Review—Factors influencing sulfur induced corrosion on the secondary side in pressurized water reactors (PWRs)10.1149/2.0531902jes ↗
14. Effects of thiosulfate and dissolved oxygen on crevice corrosion of Alloy 690 in high-temperature chloride solution10.1016/j.jmst.2020.05.074 ↗
15. Correlation between film rupture ductility and PbSCC of Alloy 80010.1016/j.electacta.2007.12.070 ↗
16. Crevice corrosion of nickel-based alloys in neutral chloride and thiosulfate solutions10.5006/1.3584962 ↗
17. Effect of thiosulfate on pitting corrosion of Ni-Cr-Fe alloys in chloride solutions10.5006/2923 ↗
18. Pitting of steam-generator tubing alloys in solutions containing thiosulfate and sulfate or chloride10.1039/C5FD00008D ↗
19. Pitting corrosion mechanism of Alloy 800 in simulated crevice chemistries containing thiosulfate10.5796/electrochemistry.84.585 ↗
20. Effect of sulphate and chloride ions on the crevice chemistry and stress corrosion cracking of alloy 600 in high temperature aqueous solutions10.1016/0010-938X(92)90016-V ↗
21. Effect of thiosulfate on metastable pitting of 304 L and S32101 in chloride- and thiosulfate-containing environment10.5006/1955 ↗
22. Effect of thiosulfate on pitting corrosion of 316 SS10.1149/2.0041504jes ↗
23. Effects of sulfur compounds on the pitting behavior of type 304 stainless steel in near-neutral chloride solutions10.5006/1.3577348 ↗
24. The role of thiosulfates in the pitting corrosion of Fe-17Cr alloys in neutral chloride solution: electrochemical and XPS study10.1016/S0010-938X(97)81158-4 ↗
25. Occluded solution chemistry contral and the role of alloy sulfur on the initiation of crevice corrosion in type 304 SS10.1016/S0010-938X(98)00084-5 ↗
26. The role of inclusions on initiation of crevice corrosion of stainless steel: Ⅰ. experimental studies10.1149/1.2096896 ↗
27. Accelerated Corrosion in Dissimilar Metal Crevices
28. Mechanism of dissimilar metal crevice corrosion of superferritic stainless steels10.5006/1.3293560 ↗
29. Corrosion behavior of Alloy 690 in aerated supercritical water10.1016/j.corsci.2012.10.001 ↗
30. Crevice corrosion of N80 carbon steel in CO2-saturated environment containing acetic acid10.1016/j.corsci.2016.08.002 ↗
31. The role of acetic acid or H+ in initiating crevice corrosion of N80 carbon steel in CO2-saturated NaCl solution10.1016/j.corsci.2017.08.028 ↗
32. Inhibition effect of imidazoline inhibitor on the crevice corrosion of N80 carbon steel in the CO2-saturated NaCl solution containing acetic acid10.1016/j.corsci.2017.06.021 ↗
33. Effect of thiosulfate on crevice of stainless steel10.5006/1.3593899 ↗
34. A clearer view of how crevice corrosion occurs10.1007/BF03221250 ↗
35. A review of the theoretical modelling of crevice and pitting corrosion10.1016/0010-938X(87)90024-2 ↗
36. Crevice Corrosion of Stainless Steels Ⅰ: a Mathematical Model10.1179/000705978798358671 ↗
37. Simultaneous visualization of pH and Cl− distributions inside the crevice of stainless steel10.1016/j.corsci.2016.01.028 ↗
38. Crevice corrosion of stainless steels Ⅱ: experimental studies10.1179/000705978798276258 ↗
39. A critical crevice solution and IR drop crevice corrosion model10.1016/j.corsci.2008.02.020 ↗
40. Simple algorithms for 1D oxygen concentration profile in an occluded region10.1016/j.corsci.2008.08.039 ↗
41. High temperature potential/pH diagrams for the sulphur-water system10.1016/0013-4686(69)87003-9 ↗
42. Pitting corrosion of Alloy 690 in thiosulfate-containing chloride solutions10.1016/S0022-3115(99)00209-3 ↗
43. Thermodynamics of thiosulfate reduction on surfaces of iron, nickel and chromium in water at 25 and 300 °C10.1016/S0010-938X(97)00079-6 ↗
44. Thiosulfate Corrosion in Paper Machine White Water10.5006/1.3582988 ↗
45. Calculating chemical concentrations during the initiation of crevice corrosion10.1016/S0010-938X(99)00097-9 ↗
46. The crevice corrosion behaviour of stainless steel in sodium chloride solution10.1016/j.corsci.2011.08.012 ↗