Tensile and Charpy impact properties of heat-treated high manganese steel at cryogenic temperatures
Source abstract
Abstract
The structural materials for the superconductor in next generation DEMO fusion reactor are in great demanded with excellent nonmagnetic and mechanical properties such as strength, toughness, and ductility at the cryogenic temperature. High-Mn steels, newly developed for application to cryogenic industry, including DEMO fusion reactor, can change its deformation mechanism by twinning, martensite transformation and dislocation slip according to the range of stacking fault energy (SFE). Therefore, it is very important to investigate the mechanism of deformation behavior at cryogenic temperatures. In this study, tensile tests and Charpy impact tests were performed to investigate the effects of heat treatment on mechanical properties of high-Mn steels at cryogenic temperatures. In addition, the deformation mechanism of high-Mn steels at room temperature and cryogenic temperature was investigated through various analysis such as microstructure, XRD, EBSD and TEM. As a result, phase transformation from austenite to ε and α`-martensite was generated in the tensile test with a slow loading rate at cryogenic temperatures, while ε and α`-martensite was not observed in the Charpy impact test with a high loading rate.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Cryogenics in fusion: Industrial approach of cryogenics applied to fusion Plants10.1007/s10894-018-0196-8 ↗
2. Progress of ITER superconducting magnet procurement10.1016/j.phpro.2013.05.008 ↗
3. Deformation behavior of austenitic stainless steel at deep cryogenic temperatures10.1016/j.jnucmat.2018.03.019 ↗
4. Tensile properties and deformation behavior of ferrite and austenite duplex stainless steel at cryogenic temperatures10.1016/j.msea.2020.140442 ↗
5. A modified stress-strain relation for austenitic stainless steels at cryogenic temperatures10.1016/j.cryogenics.2019.06.003 ↗
6. Effect of annealing temperature on microstructures and mechanical properties of a 5083 Al alloy deformed at cryogenic temperature10.1016/j.scriptamat.2004.02.037 ↗
7. The effect of heat treatment on microstructure and cryogenic fracture properties in 5Ni and 9Ni stee10.1007/BF02653488 ↗
8. Effect of cryogenic deformation on microstructure and mechanical properties of 304 austenitic stainless steel10.1016/j.matchar.2017.09.027 ↗
9. Choi JK, Lee S-G, Park Y-H, Han I-W, Morris Jr. JW. High Manganese Austenitic Steel For Cryogenic Applications, In: Proc. 22th. Int. Offshore and Polar Eng. Conf. OnePetro. (2012)
10. Low temperature mechanical properties of 316L type stainless steel after hydrostatic extrusion10.1016/j.fusengdes.2010.12.067 ↗
11. Driving force for g → « martensitic transformation and SFE of austenite in Fe-Mn binary system10.1007/s11661-000-0271-3 ↗
12. Thermodynamic modeling of the stacking fault energy of austenitic steels10.1016/j.actamat.2010.10.037 ↗
13. Deformation behavior and tensile properties of an austenitic Fe-24Mn-4Cr-0.5C high-manganese steel: Effect of grain size10.1016/j.msea.2018.10.107 ↗
14. Dependence of tensile deformation behavior of TWIP steels on stacking fault energy, temperature and strain rate10.1016/j.actamat.2010.05.049 ↗
15. Influence of addition elements on the stacking-fault energy and mechanical properties of an austenitic Fe-Mn-C steel10.1016/j.msea.2006.12.170 ↗
16. The effects of grain size on yielding, strain hardening, and mechanical twinning in Fe-18Mn-0.6C-1.5Al twinning-induced plasticity steel10.1016/j.msea.2015.11.096 ↗
17. Unusual relationship between impact toughness and grain size in a high-manganese steel10.1016/j.jmst.2021.01.089 ↗
18. Effect of grain and twin boundaries on the hardening mechanisms of twinning-induced plasticity steels10.1016/j.scriptamat.2007.10.050 ↗
19. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe-Mn-C alloys10.1016/j.msea.2004.01.059 ↗
20. Effect of stacking fault energy on work hardening behaviors in Fe-Mn-Si-C high manganese steels by varying silicon and carbon contents10.1016/j.matdes.2015.07.072 ↗
21. Characteristics of nucleation and transformation sequence in deformation-induced martensitic transformation10.1016/j.matchar.2020.110234 ↗
22. Effects of Mn and Al contents on cryogenic-temperature tensile and Charpy impact properties in four austenitic high-Mn steels10.1016/j.actamat.2015.08.027 ↗
23. Effects of Mn Addition on tensile and Charpy impact properties in austenitic Fe-Mn-C-Al-based steels for cryogenic applications10.1007/s11661-014-2513-9 ↗
24. Effects of Ni and Cu addition on cryogenic-temperature tensile and Charpy impact properties in austenitic 22Mn-0.45C–1Al steels10.1016/j.jallcom.2019.152407 ↗
25. Softening behavior by excessive twinning and adiabatic heating at high strain rate in a Fe-20Mn-0.6C TWIP steel10.1016/j.actamat.2015.09.061 ↗
26. Quasi-static and dynamic deformation mechanisms interpreted by microstructural evolution in TWinning Induced Plasticity (TWIP) steel10.1016/j.msea.2016.12.037 ↗
27. Effects of high strain rate and self-heating on plastic deformation of metal materials under fast compression loading10.1007/s40870-019-00214-x ↗
28. Effects of strain rate on the TRIP–TWIP transition of an austenitic Fe-18Mn-2Si-2Al Steel10.1007/s11661-019-05331-9 ↗
29. Effects of strain rate on room- and cryogenic-temperature compressive properties in metastable V10Cr10Fe45Co35 high-entropy alloy
30. Estimating dynamic ultimate tensile strength from instrumented Charpy data10.1016/j.matdes.2016.02.116 ↗
31. Comparasion of impact and tensile properties of high-strength steel10.3390/met8070511 ↗
32. Fang J., Group B. Fracture of nano and engineering materials and structures. Fract Nano Eng Mater Struct 2006.
33. Experimental assessment of the equivalent strain rate for an instrumented charpy test10.6028/jres.121.007 ↗
34. A general mechanism of martensitic nucleation: Part I. General concepts and the FCC → HCP transformation
35. Cryogenic toughness in a low-cost austenitic steel10.1038/s43246-021-00149-8 ↗
36. Effects of rolling temperature on the microstructure and mechanical properties of a high-Mn austenitic steel for cryogenic applications10.1002/srin.201900660 ↗
37. Dislocation-based serrated plastic flow of high entropy alloys at cryogenic temperatures10.1016/j.actamat.2020.09.052 ↗
38. Serration phenomena occurring during tensile tests of three high-manganese twinning-induced plasticity (TWIP) steels10.1007/s11661-013-2007-1 ↗
39. The effects of post weld heat treatment for welded high-Mn austenitic steels using the submerged arc welding method10.1016/j.jmrt.2022.04.103 ↗
40. The effects of recrystallization on strength and impact toughness of cold-worked high-Mn austenitic steels10.3390/met9090948 ↗
41. Tensile and microstructural characteristics of Fe-24Mn steel welds for cryogenic applications10.1007/s12540-019-00320-4 ↗
42. Grain refinement effect on cryogenic tensile ductility in a Fe-Mn-C twinning-induced plasticity steel10.1016/j.matdes.2013.01.061 ↗
43. Deformation mechanisms of a 20Mn TWIP steel investigated by in situ neutron diffraction and TEM10.1016/j.actamat.2013.06.051 ↗
44. Investigation on the nucleation mechanism of deformation-induced martensite in an austenitic stainless steel under severe plastic deformation10.1557/jmr.2007.0094 ↗
45. Microstructure and mechanical properties of gas tungsten arcwelded high manganese steel sheet10.3390/met9111167 ↗
46. Strain rate dependent mechanical properties of TWIP steel10.1007/s11837-018-3137-0 ↗