Protection of graphite from salt and gas permeation in molten salt reactors

Jo Jo Lee, José D. Arregui-Mena, Cristian I. Contescu, Timothy D. Burchell, Yutai Katoh, Sudarshan K. Loyalka

Abstract

Abstract The reactor core, moderator and reflectors of a thermal spectrum advanced molten salt reactor will constitute multi-tons of graphite. Porous reactor-grade graphite, if unprotected, can be permeated by molten salt depending on the infiltrating pressure differential and entrance diameters of accessible graphite pores. Salt and gas permeation of graphite can affect microstructural properties and radiation behavior but also facilitate diffusion, deposition and retention of fission products and tritium. Because of the significant void volume of nuclear graphite, fission products and tritium retention due to salt permeation necessitates seal coatings or pore impregnation to reduce open porosity. Alternatively, very fine-grained graphite grades with low Xe permeability are being developed. Here, we survey the current technologies for mitigating salt and gas transport into graphite.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Graphite, nuclear technology, radiation studies · Nuclear and radioactivity studies · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. 1964
2. Atkinson · 2018
3. Rosenthal · 1968 · 191
4. Redox potential control in molten salt systems for corrosion mitigation10.1016/j.corsci.2018.08.035 ↗
5. Rosenthal · 1968
6. Graphite and xenon behavior and their influence on molten-salt reactor design
7. Molten-salt reactors—history, status, and potential
8. Grimes · 1962
9. Briggs · 1965
10. The molten salt reactor adventure10.13182/NSE90-374 ↗
11. Rosenthal · 1967
12. New developments in materials for molten-salt reactors
13. Thoma · 1971
14. Grimes · 1967
15. Rosenthal · 1969
16. McCoy · 1978
17. Graphite behavior and its effects on MSBR performance10.1016/0029-5493(69)90057-0 ↗
18. Kasten · 1969
19. Briggs · 1966
20. Briggs · 1965
21. Briggs · 1964
22. Briggs · 1962
23. ASTM · 2016
24. 10 - Thorium as a nuclear fuel
25. Design and licensing strategies for the fluoride-salt-cooled, high-temperature reactor (FHR) technology10.1016/j.pnucene.2014.07.002 ↗
26. The current status of fluoride salt cooled high temperature reactor (FHR) technology and its overlap with HIF target chamber concepts10.1016/j.nima.2013.05.094 ↗
27. Tritium control and capture in salt-cooled fission and fusion reactors: status, challenges, and path forward10.13182/NT16-101 ↗
28. Tritium control and capture in salt-cooled fission and fusion reactors10.1080/15361055.2017.1289450 ↗
29. 3.07 - TRISO-coated particle fuel performance
30. X-Energy · 2018
31. Comparison of two irradiation testing results of HTR-10 fuel spheres10.1016/j.nucengdes.2011.09.047 ↗
32. Coated particle fuel: historical perspectives and current progress10.1016/j.jnucmat.2018.09.044 ↗
33. Testing of HTR UO2 TRISO fuels in AVR and in material test reactors10.1016/j.jnucmat.2013.05.062 ↗
34. Criticality calculations of the HTR-10 pebble-bed reactor with SCALE6/CSAS6 and MCNP510.1016/j.anucene.2013.09.031 ↗
35. 2014
36. 2013 · 1
37. Fabrication methods and anisotropic properties of graphite matrix compacts for use in HTGR10.1016/j.jnucmat.2017.11.055 ↗
38. Preparation of spherical fuel elements for HTR-PM in INET10.1016/j.nucengdes.2013.07.001 ↗
39. Windes · 2010
40. ASTM D7219-08 · 2008
41. ASTM D8075 · 2016
42. Study on the comprehensive properties and microstructures of A3-3 matrix graphite related to the high temperature purification treatment10.1155/2018/6084747 ↗
43. Key results from irradiation and post-irradiation examination of AGR-1 UCO TRISO fuel10.1016/j.nucengdes.2017.09.005 ↗
44. The design features of the HTR-1010.1016/S0029-5493(02)00182-6 ↗
45. Overview of HTTR design features10.1016/j.nucengdes.2004.07.016 ↗
46. Pore structure development in oxidized IG-110 nuclear graphite10.1016/j.jnucmat.2012.07.015 ↗
47. Beyond the classical kinetic model for chronic graphite oxidation by moisture in high temperature gas-cooled reactors10.1016/j.carbon.2017.11.001 ↗
48. ASTM D7219-08 · 2008
49. IBIDEN, ETU-10 Property data. https://www.fgm.ibiden.co.jp/multilanguage/english/list.html.
50. G.Q. Zheng, Xu, P., Sridharan, K. and Allen, T.R., Pore structure analysis of nuclear graphites IG-110 and NBG-18, Advances in Materials Science for Environmental and Nuclear Technology II, pp. 251-260.10.1002/9781118144527.ch24 ↗
51. Microstructural characterization and pore structure analysis of nuclear graphite10.1016/j.jnucmat.2011.05.053 ↗
52. Preparation of binderless nanopore-isotropic graphite for inhibiting the liquid fluoride salt and Xe 135 penetration for molten salt nuclear reactor10.1016/j.carbon.2014.07.022 ↗
53. Excluding molten fluoride salt from nuclear graphite by SiC/glassy carbon composite coating10.1016/j.net.2019.03.006 ↗
54. Burchell · 2007 · 15
55. MERSEN Specialty graphite grades. https://www.graphite-eng.com/uploads/.
56. Microstructure and molten salt impregnation characteristics of a micro-fine grain graphite for use in molten salt reactors10.1016/S1872-5805(16)60034-3 ↗
57. Evans · 1969
58. Infiltration of graphite by molten 2LiF–BeF2 salt10.1007/s10853-017-1310-4 ↗
59. Microcracks in nuclear graphite and highly oriented pyrolytic graphite (Hopg)10.1016/j.jnucmat.2008.07.012 ↗
60. On the nature of cracks and voids in nuclear graphite10.1016/j.carbon.2016.03.011 ↗
61. The dynamics of capillary flow10.1103/PhysRev.17.273 ↗
62. Chapter 1.5 - interfacial free energy and wettability
63. Wetting in infiltration of alumina particle preforms with molten copper10.1007/s10853-005-1980-1 ↗
64. Protection of nuclear graphite toward liquid fluoride salt by isotropic pyrolytic carbon coating10.1016/j.jnucmat.2013.09.015 ↗
65. Fluorination of nuclear graphite IG-110 in molten 2LiF-BeF2 (FLiBe) salt at 700 °C10.1016/j.jfluchem.2018.04.001 ↗
66. Molten FLiNaK salt infiltration into degassed nuclear graphite under inert gas pressure10.1016/j.carbon.2014.12.044 ↗
67. Preparation of pyrolytic carbon coating on graphite for inhibiting liquid fluoride salt and Xe135 penetration for molten salt breeder reactor10.1016/j.jnucmat.2014.09.006 ↗
68. SiC coating: an alternative for the protection of nuclear graphite from liquid fluoride salt10.1016/j.jnucmat.2014.01.034 ↗
69. Improving molten fluoride salt and Xe 135 barrier property of nuclear graphite by phenolic resin impregnation process10.1016/j.jnucmat.2017.11.019 ↗
70. Protecting nuclear graphite from liquid fluoride salt and oxidation by SiC coating derived from polycarbosilane10.1016/j.jeurceramsoc.2017.09.031 ↗
71. Carburization effects on the corrosion of Cr_Fe_Ni_W_ and Mo in Fluoride-scalt cooled high temperature reactor10.1016/j.anucene.2018.05.013 ↗
72. Materials corrosion in molten LiF–NaF–KF salt10.1016/j.jfluchem.2008.05.008 ↗
73. High-temperature corrosion of UNS N10003 in molten Li2BeF4 (FLiBe) salt10.5006/1657 ↗
74. An integrated model of tritium transport and corrosion in Fluoride Salt-Cooled High-Temperature Reactors (FHRs) – Part I: theory and benchmarking10.1016/j.nucengdes.2016.10.051 ↗
75. Adsorption and desorption of tritium in nuclear graphite at 700°C: a gas chromatographic study using hydrogen10.1080/00295450.2019.1590076 ↗
76. Study of tritium retention in graphite by simulating first wall circumstances10.13182/FST95-A30589 ↗
77. Hydrogen behavior in carbon and graphite before and after neutron irradiation – trapping, diffusion and the simulation of bulk retention10.1016/j.jnucmat.2010.12.100 ↗
78. Hydrogen trapping in neutron-irradiated graphite10.1016/j.jnucmat.2008.12.135 ↗
79. Hydrogen adsorption on and solubility in graphites10.1016/S0022-3115(96)00067-0 ↗
80. Adsorption of atomic hydrogen on defect sites of graphite: influence of surface reconstruction and irradiation damage10.1016/j.carbon.2017.09.095 ↗
81. Engel · 1971
82. Lane · 1958
83. Rosenthal · 1971
84. Corrosion of 316 stainless steel in high temperature molten Li 2 BeF 4 (FLiBe) salt10.1016/j.jnucmat.2015.03.004 ↗
85. MacPherson · 1960
86. Tarpinian · 1959
87. Absorption of molten fluoride salts in glassy carbon, pyrographite and Hastelloy B10.1016/S0022-3115(01)00419-6 ↗
88. Jenkins · 1976
89. Effect of neutron irradiation on properties of glassy carbon10.1023/A:1016232223288 ↗
90. Irradiation-induced length changes of glassy carbon10.1016/0008-6223(72)90048-6 ↗
91. Neutron irradiation induced changes in the structure and properties of glassy carbon10.1023/A:1019991326301 ↗
92. Neutron irradiation effect on the thermal conductivity and dimensional change of graphite materials10.1016/0022-3115(92)90362-O ↗
93. Neutron irradiation effects of electrical properties in glassy carbon10.1143/JPSJ.20.1288 ↗
94. Protection of nuclear graphite toward fluoride molten salt by glassy carbon deposit10.1016/j.jnucmat.2008.11.032 ↗
95. Surface coating of graphite pebbles for Korean HCCR TBM10.1016/j.fusengdes.2013.12.027 ↗
96. CVR-SiC coating of graphite pebbles for fusion blanket application10.1016/j.ceramint.2013.06.082 ↗
97. The corrosion behavior of CVI SiC matrix in SiCf/SiC composites under molten fluoride salt environment10.1016/j.jnucmat.2017.02.007 ↗
98. Corrosion of SiC induced by Hastelloy N alloy and its corrosion products in LiF–NaF–KF molten salt10.1016/j.corsci.2016.03.029 ↗
99. Assessment of SiC-CMC compatibility with components of actinide fuel systems10.1016/j.anucene.2018.12.030 ↗
100. Chemical compatibility between UO2 fuel and SiC cladding for LWRs. Application to ATF (Accident-Tolerant Fuels)10.1016/j.jnucmat.2017.02.031 ↗