journal article·2018-10

The effects of cold working on the corrosion behavior of an austenitic stainless steel in liquid lead-bismuth eutectic under vacuum at 873 K

Lu Bian, Shuang Xia, Qin Bai, Hui Li, Bangxin Zhou

Publisher page

Abstract

Abstract The effects of cold working (CW) on the corrosion of CN1515 austenitic stainless steel in a static liquid lead-bismuth eutectic (LBE) under vacuum at 873 K for 1000–3000 h were investigated. The inward penetration of LBE into the sample and the associated outward dissolution of Ni and Cr resulted in the formation of a ferrite layer in the surface of samples. The thickness of the ferrite layer of the CW samples is larger than that of the solution annealed (SA) samples. The ferrite grains maintains a {011} α//{111} γ, α// γ relationship with the original austenitic grains. Slip bands in FCC grains act as preferential penetration paths of LBE and result in the larger thickness of the ferrite layer of CW samples over SA samples.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear reactor physics and engineering · Nuclear Materials and Properties · Thermodynamic and Structural Properties of Metals and Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Role of ADS in the back-end of the fuel cycle strategies and associated design activities: the case of Japan10.1016/j.jnucmat.2011.04.032 ↗
2. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
3. Corrosion issue in lead-cooled fast reactor (LFR) and accelerator driven systems (ADS)
4. Analysis on liquid metal corrosion-oxidation interactions10.1016/j.corsci.2007.05.012 ↗
5. A review of steel corrosion by liquid lead and lead-bismuth10.1016/j.corsci.2009.03.013 ↗
6. Results of steel corrosion tests in flowing liquid Pb/Bi at 420-600 °C after 2000 h10.1016/S0022-3115(01)00725-5 ↗
7. Compatibility tests on steels in molten lead and lead-bismuth10.1016/S0022-3115(01)00538-4 ↗
8. Compatibility tests of steels in flowing liquid lead-bismuth10.1016/S0022-3115(01)00570-0 ↗
9. Koury · J. Nucl. Mater. · 2012 · 429 · 21010.1016/j.jnucmat.2012.05.041 ↗
10. Effect of flowing Lead-Bismuth Eutectic on the mechanical and structural properties of stainless steel 304L10.1007/s12666-013-0332-0 ↗
11. Corrosion behaviors of US steels in flowing lead-bismuth eutectic (LBE)10.1016/j.jnucmat.2004.08.002 ↗
12. Corrosion behavior of steels in liquid lead-bismuth with low oxygen concentrations10.1016/j.jnucmat.2007.05.051 ↗
13. Dissolution and oxidation behaviour of various austenitic steels and Ni rich alloys in lead-bismuth eutectic at 520 °C10.1016/j.jnucmat.2015.11.005 ↗
14. Investigation on oxygen controlled liquid lead corrosion of surface treated steels10.1016/S0022-3115(99)00211-1 ↗
15. Temperature effect on the corrosion mechanism of austenitic and martensitic steels in lead-bismuth10.1016/S0022-3115(01)00723-1 ↗
16. Oxide layer stability in lead-bismuth at high temperature10.1016/j.jnucmat.2004.07.017 ↗
17. Corrosion of stainless steels in lead-bismuth eutectic up to 600 °C10.1016/j.jnucmat.2004.07.012 ↗
18. Corrosion behaviour of steels in lead-bismuth at 823 K10.1016/j.jnucmat.2004.07.013 ↗
19. Liquid metal corrosion of T91 and A316L materials in Pb-Bi eutectic at temperatures 400-600 °C10.1016/j.corsci.2005.04.001 ↗
20. Comparison of the corrosion behavior of austenitic and ferritic/martensitic steels exposed to static liquid Pb-Bi at 450 and 550 °C10.1016/j.jnucmat.2004.07.064 ↗
21. Grain boundary engineering of austenitic steel PNC316 for use in nuclear reactors10.1016/j.jnucmat.2011.03.049 ↗
22. Spectroscopic and microscopic investigation of the corrosion of 316/316L stainless steel by lead-bismuth eutectic (LBE) at elevated temperatures: importance of surface preparation10.1016/j.jnucmat.2004.03.006 ↗
23. Twin boundary-accelerated ferritization of austenitic stainless steels in liquid lead-bismuth eutectic10.1016/j.scriptamat.2016.02.029 ↗
24. Corrosion behavior of cold-worked austenitic stainless steels in liquid lead-bismuth eutectic10.1016/j.jnucmat.2014.02.006 ↗
25. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500°C10.1016/j.jnucmat.2017.04.004 ↗
26. Effect of cold working on the corrosion resistance of JPCA stainless steel in flowing Pb-Bi at 450 °C10.1016/j.jnucmat.2011.11.022 ↗
27. Nickel solubility limit in liquid lead-bismuth eutectic10.1016/j.jnucmat.2010.03.008 ↗
28. Thermodynamic assessment of solubility and activity of iron, chromium and nickel in lead bismuth eutectic10.1016/j.jnucmat.2014.03.011 ↗
29. Dissolution mechanism of 316L in lead-bismuth eutectic at 500°C10.1016/j.corsci.2011.05.031 ↗
30. Continuous atomic displacements and lattice distortion during fcc-bcc martensitic transformation10.1016/j.actamat.2015.06.010 ↗