Thermo-mechanical assessment of full SiC/SiC composite cladding for LWR applications with sensitivity analysis
Source abstract
Abstract
Abstract SiC/SiC composites are considered among leading candidates for accident tolerant fuel cladding in light water reactors. However, when SiC-based materials are exposed to neutron irradiation, they experience significant changes in dimensions and physical properties. Under a large heat flux application (i.e. fuel cladding), the non-uniform changes in the dimensions and physical properties will lead to build-up of stresses in the structure over the course of time. To ensure reliable and safe operation of such a structure it is important to assess its thermo-mechanical performance under in-reactor conditions of irradiation and elevated temperature. In this work, the foundation for 3D thermo-mechanical analysis of SiC/SiC cladding is put in place and a set of analyses with simplified boundary conditions has been performed. The analyses were carried out with two different codes that were benchmarked against one another and prior results in the literature. A constitutive model is constructed and solved numerically to predict the stress distribution and variation in the cladding under normal operating conditions. The dependence of dimensions and physical properties variation with irradiation and temperature has been incorporated. These robust models may now be modified to take into account the axial and circumferential variation in neutron and heat flux to fully account for 3D effects. The results from the simple analyses show the development of high tensile stresses especially in the circumferential and axial directions at the inner region of the cladding. Based on the results obtained, design guidelines are recommended. For lack of certainty in or tailor-ability for the physical and mechanical properties of SiC/SiC composite material a sensitivity analysis is conducted. The analysis results establish a precedence order of the properties based on the extent to which these properties influence the temperature and the stresses.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Advanced ceramic materials synthesis · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
2. Silicon carbide oxidation in steam up to 2 MPa10.1111/jace.13094 ↗
3. Oxidation at high temperatures in steam atmosphere and quench of silicon carbide composites for nuclear application10.1016/j.nucengdes.2015.10.002 ↗
4. Radiation effects in SiC for nuclear structural applications10.1016/j.cossms.2012.03.005 ↗
5. Bloore · 2013
6. Neutronic analysis of candidate accident-tolerant cladding concepts in pressurized water reactors10.1016/j.anucene.2014.09.005 ↗
7. Hydrothermal corrosion of SiC in LWR coolant environments in the absence of irradiation10.1016/j.jnucmat.2015.06.019 ↗
8. Effect of irradiation damage on hydrothermal corrosion of SiC10.1016/j.jnucmat.2015.04.034 ↗
9. Effect of dissolved hydrogen on the corrosion behavior of chemically vapor deposited SiC in a simulated pressurized water reactor environment10.1016/j.corsci.2015.05.031 ↗
10. High performance silicon carbide fiber Hi-Nicalon for ceramic matrix composites
11. Evaluation of neutron irradiated near-stoichiometric silicon carbide fiber composites10.1016/S0022-3115(00)00235-X ↗
12. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
13. Continuous SiC fiber, CVI SiC matrix composites for nuclear applications: properties and irradiation effects10.1016/j.jnucmat.2013.06.040 ↗
14. Carpenter · 2010
15. Falcon-Based Comparative Assessment of Prototype Zr-4 and SiC Fuel Rod, EPRI-1022907, Electric Power Research Institute, Palo Alto, CA2011.
16. Thermo-mechanical analysis of LWR SiC/SiC composite cladding10.1016/j.jnucmat.2014.01.006 ↗
17. A structural model for multi-layered ceramic cylinders and its application to silicon carbide cladding of light water reactor fuel10.1016/j.jnucmat.2014.12.013 ↗
18. Stress analysis and probabilistic assessment of multi-layer SiC-based accident tolerant nuclear fuel cladding10.1016/j.jnucmat.2015.08.001 ↗
19. Kinetics and mechanisms of high-temperature creep in silicon carbide: II, chemically vapor deposited10.1111/j.1151-2916.1984.tb19510.x ↗
20. Observation and possible mechanism of irradiation induced creep in ceramics10.1016/j.jnucmat.2012.11.035 ↗
21. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
22. Stability of SiC and its composites at high neutron fluence10.1016/j.jnucmat.2010.12.088 ↗
23. Barrett · 2012
24. Grain size dependence of the thermal conductivity of polycrystalline chemical vapor deposited β-SiC at low temperatures10.1063/1.346852 ↗
25. Chemically vapor deposited silicon carbide (SiC) for optical applications10.1016/0168-9002(90)90040-D ↗
26. Thermal properties of neutron-irradiated SiC; effects of boron doping10.1016/0022-3115(82)90540-2 ↗
27. Mechanical and thermal properties of SiC f/SiC composites irradiated with neutrons at high temperatures10.1016/j.fusengdes.2005.06.307 ↗
28. Katoh · 2010
29. Characterization of SiC–SiC composites for accident tolerant fuel cladding10.1016/j.jnucmat.2015.08.020 ↗
30. Investigations on ceramic materials for fusion technology10.1016/0022-3115(90)90427-O ↗
31. Mechanical, thermal, and microstructural properties of neutron-irradiated SiC10.1111/j.1151-2916.1983.tb10596.x ↗
32. Thermal conductivity of neutron-irradiated pyrolytic beta-silicon carbide10.1016/0022-3115(73)90041-X ↗
33. Dimensional stability and strength of neutron-irradiated SiC-based fibers10.13182/FST96-A11963061 ↗
34. Limits on irradiation-induced thermal conductivity and electrical resistivity in silicon carbide materials10.1016/j.jnucmat.2004.04.294 ↗
35. Thermal conductivity degradation of ceramic materials due to low temperature, low dose neutron irradiation10.1016/j.jnucmat.2004.11.009 ↗
36. Swelling of SiC at intermediate and high irradiation temperatures10.1016/j.jnucmat.2007.03.097 ↗
37. Thermophysical and mechanical properties of near-stoichiometric fiber CVI SiC/SiC composites after neutron irradiation at elevated temperatures10.1016/j.jnucmat.2010.06.002 ↗
38. Multidimensional multiphysics simulation of nuclear fuel behavior10.1016/j.jnucmat.2012.01.012 ↗
39. Interlaboratory round robin axial tensile properties of SiC-SiC tubular specimens
40. Singh · 2017
41. Re-defining failure envelopes for silicon carbide composites based on damage process analysis by acoustic emission10.1016/j.fusengdes.2013.05.054 ↗
42. Annealing behavior of neutron-irradiated silicon carbide temperature monitors10.13182/NT72-A31222 ↗
43. Effects of thermal annealing on the macroscopic dimension and lattice parameter of heavily neutron-irradiated silicon carbide10.1080/18811248.1992.9731578 ↗
44. Damage accumulation and annealing in 6H–SiC irradiated with Si+10.1016/S0168-583X(98)00381-4 ↗
45. Method for analyzing passive silicon carbide thermometry with a continuous dilatometer to determine irradiation temperature10.1016/j.nimb.2016.01.005 ↗
46. Finite rotation effects in numerical integration of rate constitutive equations arising in large-deformation analysis10.1002/nme.1620151210 ↗