Abstract

Abstract Silicon carbide (SiC) fiber reinforced SiC matrix composites continue to undergo development for fusion applications worldwide because of inherent advantages of the material including low activation, high temperature capability, relatively low neutron absorption, and radiation resistance. This paper presents an international overview of recent achievements in SiC-based composites for fusion applications. Key subjects include applications in fusion reactors, high-dose radiation effects, transmutation effects, material lifetime assessment, and development of joining technology (processing, test method development, irradiation resistance, and modeling capability). This paper also discusses synergy among research for fusion materials and non-fusion materials (for fission and aerospace applications). Finally, future research directions and opportunities are proposed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Fusion materials and technologies · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Current status and recent research achievements in SiC/SiC composites10.1016/j.jnucmat.2014.06.003 ↗
2. Current status and prospects of SiCf/SiC for fusion structural applications10.1016/j.jeurceramsoc.2013.02.013 ↗
3. Continuous SiC fiber, CVI SiC matrix composites for nuclear applications: properties and irradiation effects10.1016/j.jnucmat.2013.06.040 ↗
4. Thermo-mechanical properties and microstructure of silicon carbide composites fabricated by nano-infiltrated transient eutectoid process10.1016/S0920-3796(02)00180-1 ↗
5. Effects of neutron irradiation on mechanical properties of silicon carbide composites fabricated by nano-infiltration and transient eutectic-phase process10.1016/j.jnucmat.2013.10.005 ↗
6. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
7. Development status of a sic-foam based flow channel insert for a U.S.-ITER DCLL tbm10.13182/FST09-7 ↗
8. ITER-Test blanket module functional materials10.1016/j.jnucmat.2007.03.241 ↗
9. Design and material issues for high performance SiCf/SiC-based fusion power cores10.1016/S0920-3796(01)00181-8 ↗
10. Tungsten monoblock concepts for the Fusion Nuclear Science Facility (FNSF) first wall and divertor
11. J. Lamon, Chemical vapor infiltrated sic/sic composites (CVI sic/sic), in: Handb. Ceram. Compos, Springer US, n.d.: pp. 55–76. doi:10.1007/0-387-23986-3_3.10.1007/0-387-23986-3_3 ↗
12. Characterization of SiC-SiC composites for accident tolerant fuel cladding10.1016/j.jnucmat.2015.08.020 ↗
13. Ceramic matrix composites: nuclear applications
14. Neutronic analysis of candidate accident-tolerant cladding concepts in pressurized water reactors10.1016/j.anucene.2014.09.005 ↗
15. Low activation structural materials for fusion10.1016/0920-3796(89)90021-5 ↗
16. Silicon carbide oxidation in steam up to 2 MPa10.1111/jace.13094 ↗
17. The ARIES-I tokamak reactor study10.13182/FST91-A29440 ↗
18. Design requirements for SiC/SiC composites structural material in fusion power reactor blankets10.1016/S0920-3796(97)00200-7 ↗
19. Improved tokamak concept focusing on easy maintenance10.1016/S0920-3796(98)00119-7 ↗
20. Magnetohydrodynamic and thermal issues of the SiC f/SiC flow channel insert10.13182/FST06-A1226 ↗
21. The EU advanced lead lithium blanket concept using SiCf/SiC flow channel inserts as electrical and thermal insulators10.1016/S0920-3796(01)00506-3 ↗
22. Blanket system selection for the ARIES-ST10.1016/S0920-3796(00)00146-0 ↗
23. Functional materials for breeding blankets - status and developments10.1088/1741-4326/aa7e4e ↗
24. Fabrication issues of sandwich-like flow inserts for circular pipes
25. Materials challenges for the fusion nuclear science facility
26. SiC-based sandwich material for Flow Channel Inserts in DCLL blankets: manufacturing, characterization, corrosion tests10.1016/j.fusengdes.2017.05.059 ↗
27. Numerical modeling of first experiments on PbLi MHD flows in a rectangular duct with foam-based SiC flow channel insert10.1016/j.fusengdes.2016.04.035 ↗
28. Interfacial reactions and mechanical properties of W-SiC in-situ joints for plasma facing components10.1016/j.jnucmat.2004.04.285 ↗
29. Microstructural and mechanical characterization of W/SiC bonding for structural material in fusion10.1016/j.jnucmat.2010.12.079 ↗
30. Mechanical property degradation of high crystalline SiC fiber-reinforced SiC matrix composite neutron irradiated to ∼100 displacements per atom
31. High-dose neutron irradiation of Hi-Nicalon Type S silicon carbide composites. Part 2: mechanical and physical properties10.1016/j.jnucmat.2014.12.121 ↗
32. Evaluation of neutron irradiated silicon carbide and silicon carbide composites10.1016/j.jnucmat.2007.05.007 ↗
33. High dose neutron irradiation of Hi-Nicalon Type S silicon carbide composites, Part 1: microstructural evaluations10.1016/j.jnucmat.2014.06.038 ↗
34. Irradiation-induced shrinkage of highly crystalline SiC fibers10.1016/j.actamat.2014.07.057 ↗
35. Neutron-irradiation creep of silicon carbide materials beyond the initial transient10.1016/j.jnucmat.2016.06.006 ↗
36. Silicon carbide composites as fusion power reactor structural materials10.1016/j.jnucmat.2011.03.005 ↗
37. Magnesium behavior and structural defects in Mg+ ion implanted silicon carbide10.1016/j.jnucmat.2014.12.071 ↗
38. Precipitates and voids in cubic silicon carbide implanted with25Mg+ions10.1016/j.jnucmat.2017.10.046 ↗
39. Investigation of the damage behavior in CVD SiC irradiated with 70 keV He ions by NEXAFS, Raman and TEM10.1016/j.jeurceramsoc.2016.11.046 ↗
40. Dose dependence of helium bubble formation in nano-engineered SiC at 700 °C10.1016/j.jnucmat.2016.01.029 ↗
41. In situ observation of microstructure evolution in 4H-SiC under 3.5 keV He+irradiation10.1016/j.jnucmat.2016.01.017 ↗
42. Irradiation creep of 3C-SiC and microstructural understanding of the underlying mechanisms10.1016/j.jnucmat.2013.09.004 ↗
43. Nucleation and growth of self-interstitial atom clusters in β-SiC during irradiation: kinetic Monte-Carlo modeling10.1016/j.nimb.2011.01.132 ↗
44. Accelerated atomistic simulation study on the stability and mobility of carbon tri-interstitial cluster in cubic SiC10.1016/j.commatsci.2014.03.051 ↗
45. First principles defect energetics for simulations of silicon carbide under irradiation: kinetic mechanisms of silicon di-interstitials10.1016/j.nimb.2013.09.044 ↗
46. Evolution of small defect clusters in ion-irradiated 3C-SiC: combined cluster dynamics modeling and experimental study10.1016/j.actamat.2016.12.020 ↗
47. Neutron irradiation-induced voids in β-silicon carbide10.1016/0022-3115(73)90077-9 ↗
48. Microstructure and annealing behavior of heavily neutron-irradiated β-SiC10.1016/0022-3115(88)90261-9 ↗
49. Transmission electron microscopy and high-resolution electron microscopy studies of structural defects induced in 6H α-SiC single crystals irradiated by swift Xe ions10.1080/01418619408244341 ↗
50. Atomic structure of nano voids in irradiated 3C-SiC10.1016/j.jnucmat.2017.09.043 ↗
51. Equilibrium shapes and surface selection of nanostructures in 6H-SiC10.1063/1.4979550 ↗
52. Atomic configuration of point defect clusters in ion-irradiated silicon carbide
53. Atomic configuration of irradiation-induced planar defects in 3C-SiC10.1063/1.4869829 ↗
54. Irradiation-induced β to α SiC transformation at low temperature10.1038/s41598-017-01395-y ↗
55. Positron annihilation spectroscopy investigation of vacancy defects in neutron-irradiated 3C-SiC10.1103/PhysRevB.95.104103 ↗
56. Positron annihilation spectroscopy investigation of vacancy clusters in silicon carbide: combining experiments and electronic structure calculations10.1103/PhysRevB.89.155203 ↗
57. Calculation of positron annihilation characteristics of six main defects in 6H -SiC and the possibility to distinguish them experimentally10.1103/PhysRevB.94.014103 ↗
58. Quantification of irradiation defects in beta-silicon carbide using Raman spectroscopy10.1016/j.scriptamat.2016.08.004 ↗
59. Irradiation effects in 6H–SiC induced by neutron and heavy ions: Raman spectroscopy and high-resolution XRD analysis10.1016/j.jnucmat.2016.06.020 ↗
60. Raman spectroscopy study of heavy-ion-irradiated α-SiC10.1088/0953-8984/18/22/022 ↗
61. Microstructural evolution of neutron irradiated 3C-SiC10.1016/j.scriptamat.2017.02.030 ↗
62. Irradiation-induced microstructural evolution and swelling of 3C-SiC10.1016/j.jnucmat.2015.01.040 ↗
63. Standard Practice for Constant-amplitude, Axial, Tension-tension Cyclic Fatigue of Continuous Fiber-reinforced Advanced Ceramics at Ambient Temperatures, (n.d.). doi:10.1520/C1360-17.10.1520/C1360-17 ↗
64. Monotonic tension, fatigue and creep behavior of SiC-fiber-reinforced SiC-matrix composites: a review10.1016/S0266-3538(99)00014-7 ↗
65. S. Nogami, T. Nozawa, D. Kawai, W. Guan, A. Hasegawa, Fatigue Properties of SiC/SiC Composites under Various Loading Modes, (n.d.). doi:10.1080/15361055.2017.1333822.10.1080/15361055.2017.1333822 ↗
66. Failure prediction in structural ceramics using acoustic emission10.1111/j.1151-2916.1973.tb12419.x ↗
67. Fatigue lifetime of ceramic matrix composites at intermediate temperature by acoustic emission10.3390/ma10060658 ↗
68. Mechanical properties of SiC/SiC braided tubes for fuel cladding10.1016/j.jnucmat.2014.06.035 ↗
69. A finite fracture model for the analysis of multi-cracking in woven ceramic matrix composites10.1016/j.compositesb.2017.11.050 ↗
70. Role of irradiation-induced defects on SiC dissolution in hot water10.1016/j.corsci.2016.08.007 ↗
71. Effect of irradiation damage on corrosion of 4H-SiC in FLiNaK molten salt10.1016/j.corsci.2017.05.028 ↗
72. Radiation-tolerant joining technologies for silicon carbide ceramics and composites10.1016/j.jnucmat.2013.10.002 ↗
73. Pressure-less joining of C/SiC and sic/sic by a MoSi2/Si composite10.1111/ijac.12631 ↗
74. Effect of heat treatment on the tensile strength and creep resistance of advanced SiC fibers10.1016/j.jnucmat.2004.04.123 ↗
75. Joining of β-SiC by spark plasma sintering10.1016/j.jeurceramsoc.2013.12.023 ↗
76. Flash joining of CVD-SiC coated Cf/SiC composites with a Ti interlayer10.1016/j.jeurceramsoc.2017.05.016 ↗
77. Thickness-dependent phase evolution and bonding strength of SiC ceramics joints with active Ti interlayer10.1016/j.jeurceramsoc.2016.12.009 ↗
78. Microstructure characteristic and its influence on the strength of SiC ceramic joints diffusion bonded by spark plasma sintering10.1016/j.ceramint.2017.11.185 ↗
79. Comparison of shear strength tests on AV119 epoxy-joined carbon/carbon composites10.1016/j.compositesb.2009.10.008 ↗
80. Torsional shear strength tests for glass-ceramic joined silicon carbide10.1111/ijac.12248 ↗
81. Bonding of ceramics: an analysis of the torsion hourglass specimen10.1016/j.ijadhadh.2016.05.006 ↗
82. Irradiation resistance of silicon carbide joint at light water reactor–relevant temperature10.1016/j.jnucmat.2017.03.017 ↗
83. Radiation stable, hybrid, chemical vapor infiltration/preceramic polymer joining of silicon carbide components10.1016/j.jnucmat.2017.02.012 ↗
84. He-irradiation effects on glass-ceramics for joining of SiC-based materials10.1016/j.jnucmat.2016.01.024 ↗
85. CaO-Al2O3 glass-ceramic as a joining material for SiC based components: a microstructural study of the effect of Si-ion irradiation10.1016/j.jnucmat.2018.01.033 ↗
86. Modeling and testing miniature torsion specimens for SiC joining development studies for fusion10.1016/j.jnucmat.2015.07.044 ↗
87. Modeling thermal and irradiation-induced swelling effects on the integrity of Ti3SiC2/SiC joints10.1016/j.jnucmat.2017.09.011 ↗
88. A dual-phase microstructural approach to damage and fracture of Ti3SiC2/SiC joints10.1016/j.jnucmat.2017.11.054 ↗
89. Accident tolerant fuel cladding development: promise, status, and challenges10.1016/j.jnucmat.2017.12.043 ↗
90. Review of SiCf/SiCmcorrosion, erosion and erosion-corrosion in high temperature helium relevant to GFR conditions10.1016/j.jnucmat.2017.09.010 ↗
91. High-temperature tests of silicon carbide composite cladding under GFR conditions10.1016/j.egypro.2017.08.116 ↗
92. In situ observation of mechanical damage within a SiC-SiC ceramic matrix composite10.1016/j.jnucmat.2016.09.007 ↗
93. Thermo-mechanical analysis of LWR SiC/SiC composite cladding10.1016/j.jnucmat.2014.01.006 ↗
94. Dimensional stability and anisotropy of SiC and SiC-based composites in transition swelling regime10.1016/j.jnucmat.2017.12.009 ↗
95. Experimental design and analysis for irradiation of SiC/SiC composite tubes under a prototypic high heat flux10.1016/j.jnucmat.2017.04.058 ↗
96. Neall · 2017 · 37
97. A structural model for multi-layered ceramic cylinders and its application to silicon carbide cladding of light water reactor fuel10.1016/j.jnucmat.2014.12.013 ↗
98. Ceramic-matrix composites enable revolutionary gains in turbine engine efficiency
99. The critical issues of SiC materials for future nuclear systems10.1016/j.scriptamat.2017.03.001 ↗
100. Re-evaluation of SiC permeation coefficients at high temperatures