journal article·2026-08Open access

Structural, mechanical and tribocorrosion performances of Fe-based amorphous coating via cryogenic cycling treatment

Meng Wang, Xuqiang Li, Wensheng Li, Bo Cheng, Xinjian Zhang, Haimin Zhai

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · Tribology and Wear Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Development and crystallization kinetics of novel near-equiatomic high-entropy bulk metallic glasses10.1016/j.jallcom.2018.11.299 ↗
2. Room-temperature plasticity of metallic glass composites: a review10.1016/j.compositesb.2024.111453 ↗
3. Structural heterogeneities and mechanical behavior of amorphous alloys10.1016/j.pmatsci.2019.04.005 ↗
4. Influence of the substrate on the formation of metallic glass coatings by cold gas spraying10.1007/s11666-016-0419-3 ↗
5. Evaluation of the effects of the crystallinity of kinetically sprayed Ni–Ti–Zr–Si–Sn bulk metallic glass on the scratch response10.1016/j.msea.2006.02.434 ↗
6. Effects of substrate bias on structure and mechanical properties of (TiVCrZrHf)N coatings10.1016/j.surfcoat.2012.07.004 ↗
7. Effect of spray powder particle size on the bionic hydrophobic structures and corrosion performance of Fe-based amorphous metallic coatings10.1016/j.surfcoat.2022.128377 ↗
8. Influence of heat treatment on microstructure and mechanical properties of iron-based coating10.1016/j.matdes.2010.12.055 ↗
9. Effect of porosity defects on the long-term corrosion behaviour of Fe-based amorphous alloy coated mild steel10.1016/j.corsci.2016.04.021 ↗
10. Influence of the size of spraying powders on the microstructure and corrosion resistance of Fe-based amorphous coating10.1016/j.electacta.2011.05.020 ↗
11. Study of dry sliding wear behavior of a Fe-based amorphous coating synthesized by detonation spraying on an AZ31B magnesium alloy10.1007/s11665-020-05357-w ↗
12. Corrosion resistance mechanisms of detonation sprayed Fe-based amorphous coating on AZ31B magnesium alloy10.1016/j.jnoncrysol.2021.121276 ↗
13. Influence of the high-velocity oxygen-fuel spray parameters on the porosity and corrosion resistance of iron-based amorphous coatings10.1016/j.surfcoat.2019.03.046 ↗
14. Interfacial bonding mechanism and properties of HVOF-sprayed Fe-based amorphous coatings on LA141 magnesium alloy substrate10.1016/j.surfcoat.2021.127801 ↗
15. Two-stage rejuvenation and the correlation between rejuvenation behavior and the boson heat capacity peak of a bulk metallic glass10.1016/j.actamat.2019.08.040 ↗
16. Rejuvenation by enthalpy relaxation in metallic glasses10.1016/j.actamat.2022.118376 ↗
17. Intermediate structural state for maximizing the rejuvenation effect in metallic glass via thermo-cycling treatment10.1016/j.jallcom.2019.05.026 ↗
18. Improving plasticity of the Zr46Cu46Al8 bulk metallic glass via thermal rejuvenation10.1016/j.scib.2018.04.021 ↗
19. Nanoscale structural evolution and anomalous mechanical response of nanoglasses by cryogenic thermal cycling10.1021/acs.nanolett.8b01007 ↗
20. Effect of cyclic cryogenic treatment on tribological performance of Fe-based amorphous coatings in air and in 3.5% NaCl solution10.1016/j.jnoncrysol.2022.121471 ↗
21. Rejuvenation and malleability enhancement of Zr-based metallic glass by Sub- T G annealing and cryogenic thermal cycle treatment10.1007/s11665-022-07723-2 ↗
22. Novel corrosion behaviours of the annealing and cryogenic thermal cycling treated Ti-based metallic glasses10.1016/j.intermet.2019.04.010 ↗
23. Strategy for improving the wear-resistance properties of detonation sprayed Fe-based amorphous coatings by cryogenic cycling treatment10.1016/j.surfcoat.2021.126962 ↗
24. Relevance of shear transformations in the relaxation of supercooled liquids10.1103/PhysRevLett.129.195501 ↗
25. Various rejuvenation behaviors of Zr-based metallic glass by cryogenic cycling treatment with different casting temperatures10.1186/s11671-018-2816-7 ↗
26. Structural heterogeneity, β relaxation and magnetic properties of Fe-Zr-B amorphous alloys with Si and Cu additions10.1016/j.jallcom.2023.171059 ↗
27. Rejuvenation and plasticization of metallic glass by deep cryogenic cycling treatment10.1016/j.intermet.2017.11.015 ↗
28. Rejuvenation of metallic glasses by non-affine thermal strain10.1038/nature14674 ↗
29. Microstructure and tribological behavior of multilayered CrN coating by arc ion plating10.1016/j.surfcoat.2015.04.045 ↗
30. Corrosion and tribo-corrosion behaviors of detonation sprayed Fe-based amorphous coating10.1016/j.surfcoat.2024.130717 ↗
31. Effects of crystallization on the corrosion resistance of Fe-based amorphous coatings10.1016/j.corsci.2012.02.003 ↗
32. Electrochemical and tribocorrosion performances of CrMoSiCN coating on Ti-6Al-4V titanium alloy in artificial seawater10.1016/j.corsci.2019.108385 ↗
33. Influence of Ag target current on the structure and tribological properties of CrMoSiCN/Ag coatings in air and water10.1016/j.triboint.2021.107059 ↗
34. The study of mechanical properties and corrosion behavior of the Fe-based amorphous alloy coatings using high velocity oxygen fuel spraying10.1016/j.jallcom.2021.159132 ↗
35. Long term semiconducting and passive film properties of a novel dense FeCrMoCBY amorphous coating by atmospheric plasma spraying10.1016/j.apsusc.2019.143600 ↗
36. Corrosive wear behaviors and mechanisms of a biocompatible Fe-based bulk metallic glass10.1016/j.jnoncrysol.2020.120088 ↗
37. Structure and tribocorrosion behavior of CrMoSiCN nanocomposite coating with low C content in artificial seawater10.1007/s40544-020-0445-5 ↗
38. Influence of carbon contents on the structure and tribocorrosion properties of TiSiCN coatings on Ti6Al4V10.1016/j.triboint.2017.01.002 ↗
39. Structural, mechanical and tribocorrosion performances of CrMoSiN coatings with various Mo contents in artificial seawater10.1016/j.apsusc.2020.146629 ↗
40. Corrosive wear behavior of HVOF-sprayed micro-nano-structured Cr3C2–NiCr cermet coatings under aqueous media10.1016/j.ceramint.2022.02.044 ↗
41. Tribocorrosion behavior of Al-based amorphous coatings prepared by different spraying methods
42. The tribocorrosion behavior of the Cu-based glassy composite coating produced via high velocity air-fuel thermal spraying10.1016/j.intermet.2025.108747 ↗
43. Tribocorrosion behavior of low friction TiSiCN nanocomposite coatings deposited on titanium alloy for biomedical applications10.1016/j.surfcoat.2018.04.049 ↗
44. Methods of measuring wear-corrosion synergism10.1016/0043-1648(94)07108-X ↗
45. Advancing electrochemical impedance analysis through innovations in the distribution of relaxation times method10.1016/j.joule.2024.05.008 ↗
46. Erosion-corrosion mapping of Fe in aqueous slurries: some views on a new rationale for defining the erosion-corrosion interaction10.1016/S0043-1648(03)00566-0 ↗
47. Mapping erosion–corrosion of WC/Co–Cr based composite coatings: particle velocity and applied potential effects10.1016/j.surfcoat.2006.01.069 ↗
48. Tribocorrosion performance of 316L stainless steel enhanced by laser clad 2-layer coating using Fe-based amorphous powder10.1016/j.jmrt.2022.01.046 ↗
49. Impact angle effects on the erosion–corrosion of superlattice CrN/NbN PVD coatings10.1016/j.surfcoat.2004.07.075 ↗
50. Abnormal fretting wear behavior of Fe-based amorphous coating10.1016/j.wear.2024.205419 ↗
51. Outstanding anti-oxidation performance of boride coating under high-temperature friction10.1016/j.corsci.2020.109133 ↗
52. The influence of corrosion on diamond-like carbon topography and friction at the nanoscale10.1016/j.carbon.2021.04.068 ↗
53. A model on the coupling between cyclic fatigue and microstructure evolution in a metallic glass10.1016/j.ijfatigue.2024.108446 ↗
54. Atomic-scale origin of shear band multiplication in heterogeneous metallic glasses10.1016/j.scriptamat.2019.11.006 ↗
55. Elucidating how correlated operation of shear transformation zones leads to shear localization and fracture in metallic glasses: tensile tests on CuZr based metallic-glass microwires, molecular dynamics simulations, and modelling10.1016/j.ijplas.2019.02.011 ↗