journal article·2010-10

Refractive index changes in photochromic SbPO4–WO3 glass by exposure to band-gap radiation

Meenu Ahlawat, Gloria V. Vázquez, Marcelo Nalin, Younes Messaddeq, Sidney Ribeiro, Raman Kashyap

Journal of Non-Crystalline Solids· Volume 356· Issue 44-49
Publisher page

Abstract

Abstract We report photoinduced photo-darkening in SbPO 4 –WO 3 glass by exposure to 532 nm light with a power density of 143 mW/cm 2 . The time of exposure was varied between 0 and 256 min following which visible photo-darkening, peaking at 850 nm was observed. Spectrophotometer measurement of absorption was performed for both treated and untreated regions of the sample. Time exposure to below band-gap light results in a single exponent Gaussian absorption function over an exceptionally wide range of wavelengths (500 nm–1600 nm), with a 1/ e width of 647.5 nm. Kramers–Kronig transform of the change in the absorption indicates a negative local change in the refractive index. The dispersed refractive index change at 1550 nm, ∆ n , is calculated to be ∼−5 × 10 − 8 . The peak absorption increases with time of exposure and the photo-darkening remains irreversible at room temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Transition Metal Oxide Nanomaterials · Glass properties and applications · Photorefractive and Nonlinear Optics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Zachariasen · J. Chem. Soc. · 1932 · 54 · 384110.1021/ja01349a006 ↗
2. Dubois · J. Non-Cryst. Solids · 1986 · 88 · 35510.1016/S0022-3093(86)80037-0 ↗
3. De Vicente · J. Non-Cryst. Solids · 2003 · 330 · 16810.1016/j.jnoncrysol.2003.08.047 ↗
4. Falcao · J. Appl. Phys. · 2005 · 97 · 0135035
5. Falcao · Appl. Phys. Lett. · 2003 · 83 · 129210.1063/1.1601679 ↗
6. Nalin · J. Optoelectron. Adv. Mater. · 2001 · 3 · 553
7. Poirier · J. Non-Cryst. Solids · 2005 · 351 · 29310.1016/j.jnoncrysol.2004.11.017 ↗
8. Nalin · J. Non-Cryst. Solids · 2006 · 352 · 353510.1016/j.jnoncrysol.2006.03.087 ↗
9. Nalin · J. Non-Cryst. Solids · 2007 · 353 · 159210.1016/j.jnoncrysol.2007.01.031 ↗
10. Nalin · J. Mater. Chem. · 2004 · 14 · 339810.1039/B406075J ↗
11. Temmink · Thin Solid Films · 1990 · 192 · 21110.1016/0040-6090(90)90066-M ↗
12. Gazzinelli · J. Phys. C · 1977 · 10 · L14510.1088/0022-3719/10/6/007 ↗
13. Tritthart · Electrochim. Acta · 1999 · 44 · 303910.1016/S0013-4686(99)00018-3 ↗
14. He · Res. Chem. Intermd. · 2004 · 30 · 45910.1163/1568567041280890 ↗