Optimization of laser process method and HF-based chemical etchants for laser-induced deep etching of NXT glass
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Laser Material Processing Techniques · Advanced Surface Polishing Techniques · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Enhancing anti-reflective properties of electronic glass through two-step chemical etching10.1016/j.ceramint.2024.03.246 ↗
2. Flat panel display glass: Current status and future10.1016/j.jnoncrysol.2015.05.007 ↗
3. Mini-LED, micro-LED and OLED displays: present status and future perspectives10.1038/s41377-020-0341-9 ↗
4. Soft human–machine interface sensing displays: Materials and devices
5. Characterization of masking layers for deep wet etching of glass in an improved HF/HCl solution10.1016/j.surfcoat.2004.10.094 ↗
6. Eco-friendly glass wet etching for MEMS application: A review10.1111/jace.19961 ↗
7. Chemical etching of glasses in hydrofluoric acid: A brief review10.1016/j.matpr.2021.12.110 ↗
8. Evolution of HF etching rate of borosilicate glass by friction-induced damages10.1016/j.apsusc.2019.144789 ↗
9. 257 Nm deep UV femtosecond laser ablation with minimized crack and chipping on display ultra-thin glass10.1007/s12541-023-00929-x ↗
10. Nanocrystalline diamond-glass platform for the development of three-dimensional micro- and nanodevices10.1016/j.diamond.2019.107511 ↗
11. Display materials and processes
12. P.L. Bocko, G.R. Trott, Glass for the future: Displays and semiconductors, in: 2013 Symposium on VLSI Circuits, 2013, pp. C86–C89.
13. Laser-assisted etching of eaglexg glass by irradiation at low pulse-repetition rate10.3390/app12030948 ↗
14. Controlling the size and curvature radius of concave microlens array on fused silica by wet-etching-assisted with picosecond laser10.1007/s00339-023-07222-8 ↗
15. Processing of thin, curved borosilicate glass with selective laser-induced etching
16. Hollow channel formation inside sodium aluminoborate glass by femtosecond laser writing and distilled water etching10.3390/ma14195495 ↗
17. An investigation on effectiveness of temperature treatment for fluorine-based reactive plasma jet machining of N-BK7®10.1002/ppap.202000016 ↗
18. Deep multilevel wet etching of fused silica glass microstructures in BOE solution10.1038/s41598-023-32503-w ↗
19. Fabrication of ultra-fine vias in low CTE build-up films using a novel dry etching technology
20. Integrated multimode optical waveguides in glass using laser induced deep etching10.1364/AO.506670 ↗
21. Optimizing laser-induced deep etching technique for micromachining of NXT glass10.1364/OE.549850 ↗
22. Experimental investigation of material removal and surface roughness during optical glass polishing10.1080/10426914.2015.1103867 ↗
23. Roughness influence on the optical properties and scratch behavior of acrylic coating deposited on sandblasted glass10.1016/j.porgcoat.2016.09.014 ↗
24. Femtosecond filamentation in transparent media10.1016/j.physrep.2006.12.005 ↗
25. Chapter 7 - processes resulting from the intensity-dependent refractive index
26. Sub-picosecond ultraviolet laser filamentation-induced bulk modifications in fused silica10.1007/s00339-005-3271-8 ↗
27. Filament damage formation in fused silica glass as a result of 1–50 ps near-infrared laser pulses10.1364/AO.56.003666 ↗
28. Filamentation and damage in fused silica induced by tightly focused femtosecond laser pulses10.1103/PhysRevB.71.125435 ↗
29. Polarization-selective etching in femtosecond laser-assisted microfluidic channel fabrication in fused silica10.1364/OL.30.001867 ↗
30. 19 - Ultrasonic cleaning and washing of surfaces
31. Laser marking on soda-lime glass by laser-induced backside wet etching with two-beam interference10.1088/0960-1317/26/9/095015 ↗
32. Chemical etching of fused silica after modification with two-pulse bursts of femtosecond laser10.1364/OE.431306 ↗
33. Etching mechanism of vitreous silicon dioxide in HF-based solutions10.1021/ja993803z ↗
34. Defect-free wet etching through pyrex glass using Cr/Au mask10.1007/s00542-006-0116-0 ↗
35. Koyama · 2013
36. Water adsorption isotherm and surface conductivity of boroaluminosilicate glasses10.1021/acs.langmuir.3c02595 ↗
37. Optically transparent glass micro-actuator fabricated by femtosecond laser exposure and chemical etching10.1063/1.4750236 ↗
38. 157-Nm laser micromachining of N-BK7 glass and replication for microcontact printing10.1007/s00339-002-1936-0 ↗
39. Wet chemical and plasma etching of photosensitive glass10.3390/solids4030014 ↗
40. Silicon dioxide sacrificial layer etching in surface micromachining10.1088/0960-1317/7/1/001 ↗
41. Characterization of deep wet etching of fused silica glass for single cell and optical sensor deposition10.1088/0960-1317/19/6/065013 ↗
42. Pneumatically actuated thin glass microlens for on-chip multi-magnification observations10.3390/act9030073 ↗
43. Effective metrology and standard of the surface roughness of micro/nanoscale waveguides with confocal laser scanning microscopy10.1364/OL.44.000747 ↗
44. Glass etching with gaseous hydrogen fluoride: Rapid management of surface nano-roughness10.1111/ijag.16577 ↗
45. Fabrication of fePt/FePt-BN/FePt-SiOx granular film for HAMR media on corning lotus NXT glass substrate10.1109/TMAG.2021.3082920 ↗