journal article·2022-11

Effects of room temperature rolling in different directions on magnetic properties, electrical properties and bending ductility of Fe85P11C2B2 amorphous alloy

Yimin Guo, Ding Ma, Xuan Li, Lingjie Lu, Yu Gao, Yan Shen, Tao Zhang

Publisher page

Abstract

The effects of room temperature rolling in different directions on magnetic properties, electrical properties and bending ductility of Fe 85P 11C 2B 2 amorphous alloy were evaluated. Room temperature rolling can improve the saturation magnetization ( M s) of samples, which is due to the formation of α-Fe nanocrystals in matrix. The increase in free volume and surface roughness can enhance the resistivity ( ρ). Through adjusting the rolling direction, the M s of the sample is enhanced from 1.54 T to 1.72 T and the resistivity is increased from 177.05 μΩ·cm to 211.03 μΩ·cm. The rolled ribbons maintain good bending ductility. The appropriate heat treatment can reduce the coercivity of rolled samples. Our results provide new insights into the improvement of rolling which is expected to be used in engineering fields.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Magnetic properties of thin films · Magnetic Properties of Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Rotor eddy current loss and multiphysics fields analysis for a high-speed permanent magnet machine10.1109/TIE.2020.2988192 ↗
2. Nanoscale structural heterogeneity perspective on the ameliorated magnetic properties of a Fe-based amorphous alloy with decreasing cooling rate10.1016/j.jnoncrysol.2022.121433 ↗
3. Mechanism of low thermal conductivity for Fe76Si13B8Nb2Cu1 amorphous and nanocrystalline alloys at room temperature10.1016/j.jnoncrysol.2021.121264 ↗
4. Effects of oxygen on thermal behavior and magnetic properties of FePC amorphous alloy10.1016/j.jnoncrysol.2022.121413 ↗
5. Selective laser melting of a Fe-Si-Cr-B-C-based complex-shaped amorphous soft-magnetic electric motor rotor with record dimensions10.1016/j.matdes.2022.110483 ↗
6. New FeSiBPCCu amorphous/noncrystalline alloys with high saturation magnetic flux density and low coercivity10.1016/j.jnoncrysol.2021.121355 ↗
7. Surface-oxidized amorphous alloy powder/epoxy-resin composite bulk magnetic core and its application to megahertz switching LLC resonant converter10.1109/TMAG.2017.2718042 ↗
8. Hysteresis and loss measurements on the plastically deformed Fe–(3 wt%)Si under sinusoidal and triangular external field
9. Composition dependence of the microstructure and soft magnetic properties of Fe-based amorphous/nanocrystalline alloys: a review study10.1016/j.jnoncrysol.2014.03.010 ↗
10. Excellent soft magnetic Fe-Co-B-based amorphous alloys with extremely high saturation magnetization above 1.85 T and low coercivity below 3 A/m10.1016/j.jallcom.2017.03.341 ↗
11. Fe-based amorphous soft magnetic alloys with high saturation magnetization and good bending ductility10.1016/j.jallcom.2014.06.093 ↗
12. Development of Fe-based bulk metallic glasses with high saturation magnetization10.1016/j.scriptamat.2014.02.018 ↗
13. Design of cost-effective Fe-based amorphous coating alloys having high amorphous forming ability by thermodynamic calculation10.1007/s12540-014-4001-6 ↗
14. High-frequency soft magnetic properties of Fe-Si-B-P-Mo-Cu amorphous and nanocrystalline alloys10.1016/j.jnoncrysol.2019.119702 ↗
15. R.D. Fe-B-Si-C-Cu amorphous and nanocrystalline alloys with ultrahigh hardness and enhanced soft magnetic properties10.1016/j.jnoncrysol.2020.120606 ↗
16. Thermal transport property correlated with microstructural evolution of Fe-based amorphous alloy10.1016/j.actamat.2020.09.072 ↗
17. A study of the crystallization behavior of an amorphous Fe77.5Si13.5B9 alloy10.1016/j.msea.2005.10.033 ↗
18. Cold-rolled Zr50Cu30Ni10Al10 bulk amorphous alloys with tensile plastic elongation at room temperature10.2320/matertrans.43.3199 ↗
19. On nanovoids formation in shear bands of an amorphous Al-based alloy10.1016/j.mechmat.2017.07.007 ↗
20. Mapping of residual strains around a shear band in bulk metallic glass by nanobeam X-ray diffraction10.1016/j.actamat.2016.03.035 ↗
21. Effect of treatment conditions on parameters of nanocrystalline structure in Al-based alloys10.1016/j.matlet.2016.07.053 ↗
22. Composition dependences and optimization of the magnetic properties of Fe-based metallic glasses10.1088/2053-1591/1/4/046110 ↗
23. Stabilization of metallic supercooled liquid and bulk amorphous alloys10.1016/S1359-6454(99)00300-6 ↗
24. Nonlocal nature of the viscous transport in supercooled liquids: complex fluid approach to supercooled liquids10.1103/PhysRevLett.103.135703 ↗
25. Rejuvenation of metallic glasses by non-affine thermal strain10.1038/nature14674 ↗
26. Alloy design strategies for sustained ductility in Mg-based amorphous alloys – tackling structural relaxation10.1016/j.actamat.2015.08.077 ↗
27. Novel Fe(97−x−y)PxByNb2Cr1 glassy alloys with high magnetization and low loss characteristics for inductor core materials10.1109/TMAG.2009.2033708 ↗
28. Recent progress in Fe-based amorphous and nanocrystalline soft magnetic materials10.1016/j.jmmm.2019.166373 ↗
29. Microstructure and magnetic properties of amorphous/nanocrystalline Co40Fe22Ta8B30 alloy produced by mechanical alloying10.1016/j.matchemphys.2012.04.031 ↗
30. Revealing the effects of cooling rate on soft magnetic properties of (Fe0·9Co0·1)86Ni1B13 amorphous alloy10.1016/j.intermet.2022.107583 ↗
31. Microstructural origin of the ultra-low coercivity in bulk Fe65.5Cr4Mo4Ga4P12B5.5C5 metallic glasses10.1016/j.jmmm.2018.06.083 ↗
32. Surface roughness and electrical resistivity of high-purity zinc irradiated with nanosecond visible laser pulses10.1016/j.apsusc.2014.03.114 ↗
33. Electrical resistivity and wave character of free electrons in amorphous and nanoglass Sc75Fe2510.1088/1361-648X/aa9adf ↗
34. Microstructure and residual stress improvement in wire and arc additively manufactured parts through high-pressure rolling10.1016/j.jmatprotec.2013.04.012 ↗
35. Modern soft magnets: amorphous and nanocrystalline materials10.1016/j.actamat.2012.10.040 ↗
36. The influence of the casting parameters and of the surface quality on magnetic and magnetoelastic properties of the amorphous Co21Fe64B15 alloy10.1016/S0921-5093(97)80047-0 ↗
37. Origin of low coercivity of Fe-(Al, Ga)-(P, C, B, Si, Ge) bulk glassy alloys10.2320/matertrans.44.2020 ↗
38. Effect of primary α-Fe on soft magnetic properties of FeCuNbSiB amorphous/nanocrystalline alloy10.1016/j.jnoncrysol.2021.121079 ↗
39. Mechanism of the deformation-induced nanocrystallization in a Cu-based bulk amorphous alloy under uniaxial compression10.1016/j.scriptamat.2006.01.002 ↗
40. Crystallization-induced plasticity of Cu–Zr containing bulk amorphous alloys10.1016/j.actamat.2005.09.007 ↗
41. Thermal stability and magnetic properties of partially Co-substituted (Fe71.2B24Y4.8)96Nb4 bulk metallic glasses
42. Frequency and magnetic field dependences of coercivity and core loss in Fe–Mo–Si–P–C–B amorphous alloys10.1016/j.jallcom.2010.03.116 ↗
43. Effects of nanocrystal formation on the soft magnetic properties of Fe-based bulk metallic glasses10.1063/1.3621832 ↗
44. Magnetic properties of very high permeability, low coercivity, and high electrical resistivity in Fe87Zr7B5Ag1 amorphous alloy10.1063/1.359284 ↗
45. Fe content dependence of magnetic properties and bending ductility of FeSiBPC amorphous alloy ribbons10.1016/j.jallcom.2016.10.107 ↗