An in situ (W,Ti)C–Ni composite fabricated by SHS method
Source abstract
Abstract
Abstract The combustion synthesis reaction was combined with liquid phase sintering to fabricate net-shape TiC–Ni and TiC–WC–Ni composites in a single processing operation. When Ti and C powders used for in situ production of TiC–Ni cermet, the final product was porous and had low strength. By the addition of fine W powder with W/Ti = 1 molar ratio, the product contained (Ti,W)C, W 2 C and mix compounds of type Ni 2 W 4 C. Using W with W/Ti = 2 molar ratio results in a dense high strength product containing (Ti,W)C and WC.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Kinetics of combustion synthesis in the Ti–C and Ti–C–Ni systems10.1111/j.1151-2916.1989.tb06083.x ↗
2. Characteristics of the combustion synthesis of TiC and Fe–TiC composites10.1007/BF01151089 ↗
3. Ignition phenomena and reaction mechanism of the self-propagating high-temperature synthesis reaction in the titanium–carbon–aluminum system10.1111/j.1151-2916.1997.tb02790.x ↗
4. In situ combustion synthesis and densification of TiC−xNi cermets10.1016/S0921-5093(99)00606-1 ↗
5. An in situ WC–Ni composite fabricated by the SHS method10.1016/S0924-0136(03)00621-6 ↗
6. Synthesis of tungsten carbide–nickel composites by the field-activated combustion method10.1016/S0921-5093(03)00038-8 ↗
7. Dunmead · J. Mater. Sci. · 1991 · 26 · 241010.1007/BF01130188 ↗
8. Preparation of some new tungsten carbide hardmetals
9. Indentation fracture toughness of WC–Co cermets10.1007/BF00555296 ↗
10. Kubaschewski · 1993
11. Upadhyaya · 1998
12. Production of (W,Ti)C reinforced Ni–Ti matrix composites10.1016/S0924-0136(02)00130-9 ↗
13. Self-propagating exothermic reactions: the synthesis of high-temperature materials by combustion10.1016/S0920-2307(89)80002-7 ↗
14. A model for the hardness of cemented carbides10.1016/S0043-1648(01)00866-3 ↗
15. Hardness to toughness relationship of fine-grained WC–Co hardmetals10.1016/S0263-4368(98)00028-6 ↗
16. On the fatigue crack growth behavior of WC–Co cemented carbides: kinetics description, microstructural effects and fatigue sensitivity10.1016/S1359-6454(02)00071-X ↗