A quantitative explanation of the difference between nuclear spin relaxation and ionic conductivity relaxation in superionic glasses
Source abstract
Abstract
Electrical conductivity relaxation (ECR) experimental data represented by either the complex conductivity or the complex electric modulus are macroscopic in nature. In contrast to ECR, nuclear spin relaxation is a more direct probe of ionic movement and from its result we can infer the microscopic dynamics of the ions. Combined studies of ionic motion using ECR and nuclear spin-lattice relaxation (SLR) in several glassy ionic conductors have shown a large difference between the ECR and SLR times. Any theory that attempts to explain quantitatively the difference faces the dilemma of how to compare the SLR time with the ECR time. In this work we use a recent result [Phys. Rev. B 60 (1999) 9396] to find the ion hopping correlation time from the experimental ECR time. Next, we use the coupling model to calculate the SLR time from the ion hopping correlation time. Good agreements are obtained in three glassy ionic conductors and a crystalline ionic conductor.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · Material Dynamics and Properties · Solid-state spectroscopy and crystallography
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Tatsumisago · J. Chem. Phys. · 1992 · 97 · 686810.1063/1.463658 ↗
2. S. Estalji, R. Küchler, O. Kanert, R. Bölter, H. Jain, K.L. Ngai, J. Physique IV, Suppl. JP III, Colloq C2 (1992) 159
3. Kanert · Phys. Rev. B · 1994 · 49 · 7610.1103/PhysRevB.49.76 ↗
4. Trunnel · J. Non-Cryst. Solids · 1992 · 139 · 25710.1016/S0022-3093(05)80833-6 ↗
5. Borsa · Phys. Rev. B · 1992 · 46 · 79510.1103/PhysRevB.46.795 ↗
6. Kim · Solid State Ionics · 1996 · 91 · 710.1016/S0167-2738(96)00431-6 ↗
7. Kim · Solid State Ionics · 1995 · 90 · 2910.1016/S0167-2738(96)00401-8 ↗
8. Ngai · J. Non-Cryst. Solids · 1993 · 162 · 26810.1016/0022-3093(93)91246-Y ↗
9. Ngai · Solid State Ionics · 1993 · 61 · 34510.1016/0167-2738(93)90402-O ↗
10. Maass · Phys. Rev. Lett. · 1996 · 77 · 152810.1103/PhysRevLett.77.1528 ↗
11. Ngai · J. Chem. Phys. · 1993 · 98 · 642410.1063/1.464806 ↗
12. Ngai · Phys. Rev. B · 1993 · 48 · 1348110.1103/PhysRevB.48.13481 ↗
13. Ngai · Solid State Ionics · 1998 · 105 · 22510.1016/S0167-2738(97)00468-2 ↗
14. Svare · Phys. Rev. B · 1993 · 48 · 933610.1103/PhysRevB.48.9336 ↗
15. Svare · J. Non-Cryst. Solids · 1994 · 172–174 · 130010.1016/0022-3093(94)90656-4 ↗
16. Ngai · Comments Solid State Phys. · 1979 · 9 · 127
17. Tsang · Phys. Rev. E · 1996 · 54 · R306710.1103/PhysRevE.54.R3067 ↗
18. Tsang · Phys. Rev. E · 1997 · 56 · R1710.1103/PhysRevE.56.R17 ↗
19. Ngai · Phys. Rev. E · 1999 · 60 · 451110.1103/PhysRevE.60.4511 ↗
20. For a review, see K.L. Ngai, R.W. Rendell, in: J.T. Fourkas et al. (Eds.), Supercooled Liquids, Advances and Novel Applications, ACS Symposium Series 676, Am. Chem. Soc., Washington, DC, 1997, p. 4510.1021/bk-1997-0676.ch004 ↗
21. Ngai · IEEE Trans. Dielect. Elect. Insulat. · 2001 · 8 · 32910.1109/94.933340 ↗
22. Ngai · Phys. Rev. B · 1988 · 38 · 1035010.1103/PhysRevB.38.10350 ↗
23. Ngai · 1996 · 3
24. Cramer · Philos. Mag. B · 1995 · 71 · 70110.1080/01418639508238560 ↗
25. Cramer · Solid State Ionics · 1998 · 105 · 10910.1016/S0167-2738(97)00456-6 ↗
26. Ngai · J. Non-Cryst. Solids · 1999 · 248 · 19410.1016/S0022-3093(99)00145-3 ↗
27. Ngai · Phys. Rev. Lett. · 1998 · 80 · 101810.1103/PhysRevLett.80.1018 ↗
28. Ngai · Philos. Mag. B · 1998 · 77 · 18710.1080/014186398259941 ↗
29. Ngai · Phys. Rev. Lett. · 1996 · 76 · 129610.1103/PhysRevLett.76.1296 ↗
30. Ngai · Phys. Rev. B · 1999 · 60 · 939610.1103/PhysRevB.60.9396 ↗
31. Abragam · 1962
32. Moynihan · J. Non-Cryst. Solids · 1994 · 172–174 · 139510.1016/0022-3093(94)90668-8 ↗
33. Moynihan · J. Non-Cryst. Solids · 1996 · 203 · 35910.1016/0022-3093(96)00501-7 ↗
34. Moynihan · Solid State Ionics · 1998 · 105 · 7510.1016/S0167-2738(97)00462-1 ↗
35. Moynihan · J. Non-Cryst. Solids · 1975 · 17 · 4410.1016/0022-3093(75)90127-1 ↗
36. Howell · J. Phys. Chem. · 1974 · 78 · 63910.1021/j100599a016 ↗
37. Ngai · MRS Bull. · 1998 · 23 · 5110.1557/S0883769400031006 ↗
38. Wong · 1976
39. Angell · Chem. Rev. · 1990 · 90 · 52310.1021/cr00101a006 ↗
40. Ngai · J. Chem. Phys. · 1999 · 110 · 1057610.1063/1.478989 ↗
41. Ngai · Phys. Chem. Glasses · 1992 · 33 · 109
42. Burns · Phys. Chem. Glasses · 1989 · 30 · 264
43. Sidebottom · Phys. Rev. Lett. · 1995 · 74 · 506810.1103/PhysRevLett.74.5068 ↗
44. Lee · Phys. Rev. Lett. · 1991 · 67 · 155910.1103/PhysRevLett.67.1559 ↗
45. Nowick · Solid State Ionics · 1998 · 105 · 12110.1016/S0167-2738(97)00457-8 ↗
46. Nowick · J. Non-Cryst. Solids · 1994 · 172–174 · 124310.1016/0022-3093(94)90649-1 ↗
47. Lu · J. Phys. Chem. Solids · 1994 · 55 · 143310.1016/0022-3697(94)90569-X ↗
48. León · Phys. Rev. Lett. · 2001 · 86 · 127910.1103/PhysRevLett.86.1279 ↗
49. Rivera · Appl. Phys. Lett. · 2001 · 78 · 61010.1063/1.1343852 ↗
50. León · Phys. Rev. B · 1997 · 56 · 530210.1103/PhysRevB.56.5302 ↗
51. León · J. Non-Cryst. Solids · 1998 · 235–237 · 75310.1016/S0022-3093(98)00626-7 ↗
52. Svare · Phys. Rev. B · 2000 · 61 · 22810.1103/PhysRevB.61.228 ↗
53. Inaguma · Solid State Commun. · 1993 · 86 · 68910.1016/0038-1098(93)90841-A ↗