journal article·2017-09

Enhanced mechanical properties of Ni62Nb38 bulk metallic glasses by Ta substitution

M.K. He, S.H. Chen, P. Yu, L. Xia

Publisher page

Abstract

Abstract By substituting Ta for Nb in a binary Ni62Nb38 bulk metallic glass (BMG), ternary Ni62Nb38 − xTax (x = 5–35) BMGs were fabricated by copper mold suction casting. The present NiNbTa BMGs not only have good glass forming ability (GFA), but also have combinations of both high strength and relatively-large plastic strains, which are superior to the binary Ni62Ni38 BMG and some other Ni-Nb-based BMGs. The Ni62Nb18Ta20 BMG has fracture strength of about 3.2 GPa and a plastic strain of about 1.36%. The enhancement of the mechanical properties of the NiNbTa BMGs is related to the change of the liquid behavior and glass forming ability by Ta-substitution.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Glass properties and applications · Phase-change materials and chalcogenides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Is metallic glass poised to come of age?10.1038/nmat4297 ↗
2. Achieving high energy absorption capacity in cellular bulk metallic glasses10.1038/srep10302 ↗
3. Fe-based bulk metallic glasses with diameter thickness larger than one centimeter10.1557/JMR.2004.0176 ↗
4. Formation of Ti-Zr-Cu-Ni bulk metallic glasses10.1063/1.360537 ↗
5. Mechanical properties of bulk metallic glasses10.1016/j.pmatsci.2010.04.002 ↗
6. Glass forming ability and thermal stability of ternary Ca-Mg-Zn bulk metallic glasses10.1016/j.jnoncrysol.2005.07.022 ↗
7. Ni-based bulk metallic glass formation in the Ni-Nb-Sn and Ni-Nb-Sn-X (X=B,Fe,Cu) alloy systems10.1063/1.1544434 ↗
8. Glass formability, thermal stability and mechanical properties of La-based bulk metallic glasses10.1016/j.jallcom.2006.07.109 ↗
9. Highly corrosion-resistant Ni-based bulk amorphous alloys10.1016/S0921-5093(00)01587-2 ↗
10. Formation and mechanical properties of Ni-based Ni-Nb-Ti-Hf bulk glassy alloys10.1016/S1359-6462(02)00469-4 ↗
11. Effect of annealing on the microstructure, microhardness, and corrosion resistance of Ni62Nb33Zr5 metallic glass and its composites10.1016/j.jnoncrysol.2015.05.027 ↗
12. Thermal stability and mechanical properties of glassy and amorphous Ni-Nb-Zr alloys produced by rapid solidification10.2320/matertrans.44.1167 ↗
13. Thermal stability and mechanical strength of bulk glassy Ni-Nb-Ti-Zr alloys10.2320/matertrans.43.1952 ↗
14. Bulk glassy Ni(Co-)Nb-Ti-Zr alloys with high corrosion resistance and high strength10.1016/j.msea.2003.10.152 ↗
15. Binary Ni-Nb bulk metallic glasses10.1063/1.2158130 ↗
16. Binary bulk metallic glass Ni62Nb38 with high compressive strength of 3100MPa10.1016/j.intermet.2006.12.008 ↗
17. In situ visualization of Ni-Nb bulk metallic glasses phase transition10.1016/j.actamat.2013.05.014 ↗
18. Nanoindentation study of size effect on shear transformation zone size in a Ni-Nb metallic glass10.1016/j.msea.2015.01.001 ↗
19. Ni-Ta binary bulk metallic glasses10.1016/j.scriptamat.2010.03.044 ↗
20. Ni-Nb-Ta bulk metallic glasses designed by a cluster-plus-glue atom model10.1007/s12666-011-0059-8 ↗
21. Under what conditions can a glass be formed?10.1080/00107516908204405 ↗
22. Glass formation criterion for various glass-forming systems10.1103/PhysRevLett.91.115505 ↗
23. Poisson's ratio and the fragility of glass-forming liquids10.1038/nature02947 ↗
24. Catching the Ni-based ternary metallic glasses with critical diameter up to 3 mm in Ni-Nb-Zr system10.1016/j.jallcom.2007.02.114 ↗
25. Difference in compressive and tensile fracture mechanisms of Zr59Cu20Al10Ni8Ti3 bulk metallic glass10.1016/S1359-6454(02)00521-9 ↗
26. Hierarchical amorphous structures in a Zr50Cu42Al8 bulk metallic glass10.1016/j.msea.2015.04.045 ↗
27. Mechanical properties of bulk metallic glasses10.1557/mrs2007.125 ↗
28. Flow serration in a Zr-based bulk metallic glass in compression at low strain rates10.1016/j.intermet.2008.03.007 ↗
29. Loading-rate-independent delay of catastrophic avalanches in a bulk metallic glass10.1038/srep21967 ↗
30. Unified equation for the strength of bulk metallic glasses10.1063/1.2206099 ↗
31. The elastic properties, elastic models and elastic perspectives of metallic glasses10.1016/j.pmatsci.2011.07.001 ↗
32. Elastic moduli and behaviors of metallic glasses10.1016/j.jnoncrysol.2005.03.024 ↗
33. New bulk glassy Ni-based alloys with high strength of 3000MPa10.2320/matertrans.43.708 ↗