New FeSiBPCCu amorphous/noncrystalline alloys with high saturation magnetic flux density and low coercivity

Kuang Lv, Yuluo Li, Ningning Shen, Gaofeng Li, Yanli Wang, Xidong Hui

Publisher page

Abstract

In this work, we present a new kind of FeSiBPCCu amorphous/nanocrystalline alloys with superb comprehensive soft magnetic properties by mediating the alloy composition and process technology. Fe 84.3- xSi 1B 9.2P 5C 0.5Cu x ( x = 0, 0.2, 0.4, 0.5, 0.6, 0.8) with full amorphous structure can be prepared by melt-spun technology. Among them, Fe 84.3Si 1B 9.2P 5C 0.5 amorphous alloy annealed at 370℃ exhibits high saturation magnetic flux density ( B s) of 1.7 T and low coercivity ( H c) of 3.5 A/m. The appropriate addition of Cu is beneficial to the nucleation of α-Fe grains and inhibition of the precipitation of other compound phases. When added 0.8 at.% Cu and annealed at 470 ℃, the B s of Fe 83.5Si 1B 9.2P 5C 0.5Cu 0.8 nanocrystalline alloy reaches to 1.82 T. The perfect combination of high B s and low H c of the FeSiBPCCu amorphous/nanocrystalline alloys shows prospect to be applied for the power and electronic devices energy.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Magnetic Properties of Alloys · Electromagnetic wave absorption materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Evolution of microstructure at hot band annealing of ferritic FeSi steels10.1016/j.jmmm.2016.10.035 ↗
2. Structure and magnetic anisotropy of rapidly quenched FeSiB ribbons10.1016/j.jnoncrysol.2011.05.015 ↗
3. Crystallization-nitriding process of FeSiB and FeSiBCuNb ribbons: influence of additive (Cu,Nb) pair and nitrogen on structure, magnetic and magnetostrictive parameters10.1016/S0022-3093(01)00737-2 ↗
4. Synthesis of FeSiBPNbCu nanocrystalline soft-magnetic alloys with high saturation magnetization10.1016/j.jallcom.2014.04.223 ↗
5. Structure and magnetic properties of Si-rich FeAlSiBNbCu alloys10.1016/j.jnoncrysol.2014.12.035 ↗
6. Low core losses and magnetic properties Fe85-86Si1-2B8P4Cu1 nanocrystalline alloys with high B for power application10.1063/1.3535169 ↗
7. The influence of Al content on glass forming ability and magnetic properties of high Ms nanocrystalline FeSiBPCuAl alloy10.1016/j.matlet.2010.01.006 ↗
8. Effect of Co content on structure and magnetic behaviors of high induction Fe-based amorphous alloys10.1016/j.jmmm.2016.02.055 ↗
9. Magnetic-field-induced anisotropies and exchange softening in Fe-rich nanocrystalline soft magnetic alloys10.1016/j.scriptamat.2012.03.006 ↗
10. Atomic scale study of Cu clustering and pseudo-homogeneous Fe-Si nanocrystallization in soft magnetic FeSiNbB(Cu) alloys10.1016/j.ultramic.2015.04.006 ↗
11. Compositional design and crystallization mechanism of High Bs nanocrystalline alloys10.1016/j.materresbull.2019.01.007 ↗
12. Crystallization behavior and magnetic properties in high Fe content FeBCSiCu alloy system10.1016/j.jmmm.2015.03.033 ↗
13. Magnetostriction of nanocrystalline (Fe,Co)-Si-B-P-Cu alloys10.1016/j.scriptamat.2016.11.004 ↗
14. Soft magnetic Fe-Co-based amorphous alloys with extremely high saturation magnetization exceeding 1.9 T and low coercivity of 2 A/m10.1016/j.jallcom.2017.06.192 ↗
15. Composition design of high Bs Fe-based amorphous alloys with good amorphous-forming ability10.1016/j.jallcom.2015.09.216 ↗
16. Effect of Nb, Si and Cu on the crystallization process and magnetic properties of FeNbBP alloys10.1016/j.jallcom.2017.11.256 ↗
17. Optimization of crystallization behavior and soft magnetic properties of the Si-free Fe-B-P-C-Cu nanocrystalline alloys by Cu content tuning10.1016/j.mseb.2020.114740 ↗
18. Effect of microalloying on crystallization behavior, magnetic properties and bending ductility of high Fe content FeSiBCuPC alloys10.1016/j.jallcom.2018.11.029 ↗
19. Improvement of soft magnetic properties in (Fe0.85B0.15)100-xCux melt-spun alloys10.2320/matertrans.MAW200730 ↗
20. Effect of the substitution of C for Si on microstructure, magnetic properties and bending ductility in high Fe content FeSiBCuPC alloy ribbons10.1016/j.jallcom.2017.08.181 ↗
21. Role of Si in high Bs and low core-loss Fe85.2B10-xP4Cu0.8Six nano-crystalline alloys10.1063/1.4765718 ↗
22. Stress relaxation in amorphous alloys10.1016/0025-5416(78)90127-1 ↗
23. Modern soft magnets: amorphous and nanocrystalline materials10.1016/j.actamat.2012.10.040 ↗
24. Grain size dependence of coercivity and permeability in nanocrystalline ferromagnets10.1109/20.104389 ↗
25. Nanocrystallization, good soft magnetic properties and ultrahigh mechanical strength for Fe82-85B13-16Si1Cu1 amorphous alloys10.1016/j.jallcom.2019.01.150 ↗
26. Cu addition effect on soft magnetic properties in Fe–Si–B alloy system10.1063/1.2829240 ↗
27. High Bs Fe84−xSi4B8P4Cux (x = 0 –1.5) nanocrystalline alloys with excellent magnetic softness10.1063/1.3535290 ↗
28. Role of Si in high Bs and low core-loss Fe85.2B10−xP4Cu0.8Six nano-crystalline alloys10.1063/1.4765718 ↗
29. Dependence of soft magnetic properties of Fe81-85.5Si2B10P1.5−6Cu1 Alloys on P Content
30. Atomic level structural modulation during the structural relaxation and its effect on magnetic properties of Fe81Si4B10P4Cu1 nanocrystalline alloy10.1016/j.jmmm.2018.02.043 ↗
31. Effect of P on crystallization behavior and soft-magnetic properties of Fe83.3Si4Cu0.7B12-xPx nanocrystalline soft-magnetic alloys10.1016/j.tsf.2011.03.110 ↗
32. Significant improvement of soft magnetic properties for Fe(Co)BPSiC amorphous alloys by magnetic field annealing10.1016/j.jallcom.2018.01.311 ↗
33. Thermal, magnetic, and magnetomechanical properties of Metglas 2605 S2 and S310.1063/1.330270 ↗
34. Magnetostriction and magnetic anisotropy of field annealed Metglas* 2605 alloys via dc M-H loop measurements under stress10.1063/1.330932 ↗