Mechanism of local stress release in armchair single-wall zinc oxide nanotube under tensile loading

Wen-Jay Lee, Jee-Gong Chang, Shin-Pon Ju, Chia-Hung Lee

Journal of Nanoparticle Research· Volume 13· Issue 10
Publisher page

Abstract

The deformation mechanism of zinc oxide (ZnO) nanotube has been first examined by molecular dynamics. The result demonstrated that ZnO nanotubes relax it excess strain via the phase transformation from an armchair structure to a fourfold-coordinated structure, then to a zigzag structure, which is started by a slip deformation. In contrast to carbon, silicon carbide, and boron nitride nanotubes, they relax it local stress via the transformation of the Stone–Wales transformation. After yielding, the 8-4 dislocation loops are found and the numbers of 8-4 dislocation loops grow up, which relax the tensile strain at the necking region and leads the work hardening. Finally, the nanotube is broken down by crack deformation at the interface between different phases.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: ZnO doping and properties · Boron and Carbon Nanomaterials Research · Carbon Nanotubes in Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. An W, Wu XJ, Zeng XC (2008) Adsorption of O-2, H-2, CO, NH3, and NO2 on ZnO nanotube: A density functional theory study. J Phys Chem C 112:5747–575510.1021/jp711105d ↗
2. Chandra N, Namilae S, Shet C (2004) Local elastic properties of carbon nanotubes in the presence of Stone–Wales defects. Phys Rev B 69:09410110.1103/PhysRevB.69.094101 ↗
3. Chou HC, Rohatgi A, Jokerst NM, Kamra S, Stock SR, Lowrie SL, Ahrenkiel RK, Levi DH (1996) Approach toward high efficiency CdTe/CdS heterojunction solar cells. Mater Chem Phys 43:178–18210.1016/0254-0584(95)01626-6 ↗
4. Chowdhury R, Adhikari S, Scarpa F (2010) Elasticity and piezoelectricity of zinc oxide nanostructure. Physica E 42:2036–204010.1016/j.physe.2010.03.018 ↗
5. Chu XF, Jiang DL, Djurisic AB, Yu HL (2005) Gas-sensing properties of thick film based on ZnO nano-tetrapods. Chem Phys Lett 401:426–42910.1016/j.cplett.2004.11.091 ↗
6. Chubachi N (1976) ZnO films for surface acoustooptic devices on nonpiezoelectric substrates. Proc IEEE 64:772–77410.1109/PROC.1976.10210 ↗
7. Das R, Ray S (2003) Zinc oxide—a transparent, conducting IR-reflector prepared by rf-magnetron sputtering. J Phys D 36:152–15510.1088/0022-3727/36/2/312 ↗
8. Dumitrică T, Yakobson BI (2005) Rate theory of yield in boron nitride nanotubes. Phys Rev B 72:03541810.1103/PhysRevB.72.035418 ↗
9. Erkoc S, Kokten H (2005) Structural and electronic properties of single-wall ZnO nanotubes. Physica E 28:162–17010.1016/j.physe.2005.03.004 ↗
10. Ferekides C, Britt J (1994) CdTe solar-cells with efficiencies over 15-percent. Sol Energy Mater Sol Cells 35:255–26210.1016/0927-0248(94)90148-1 ↗
11. Fulati A, Ali SMU, Riaz M, Amin G, Nur O, Willander M (2009) Miniaturized pH sensors based on zinc oxide nanotubes/nanorods. Sensors 9:8911–892310.3390/s91108911 ↗
12. Hoover WG (1985) Canonical dynamics: equilibrium phase-space distributions. Phys Rev A 31:1695–169710.1103/PhysRevA.31.1695 ↗
13. Huang MH, Mao S, Feick H, Yan HQ, Wu YY, Kind H, Weber E, Russo R, Yang PD (2001) Room-temperature ultraviolet nanowire nanolasers. Science 292:1897–189910.1126/science.1060367 ↗
14. Jing LQ, Wang BQ, Xin BF, Li SD, Shi KY, Cai WM, Fu HG (2004) Investigations on the surface modification of ZnO nanoparticle photocatalyst by depositing Pd. J Solid State Chem 177:4221–422710.1016/j.jssc.2004.08.016 ↗
15. Keis K, Magnusson E, Lindstrom H, Lindquist SE, Hagfeldt A (2002) A 5% efficient photo electrochemical solar cell based on nanostructured ZnO electrodes. Sol Energy Mater Sol Cells 73:51–5810.1016/S0927-0248(01)00110-6 ↗
16. Kong XH, Sun XM, Li XL, Li YD (2003) Catalytic growth of ZnO nanotubes. Mater Chem Phys 82:997–100110.1016/j.matchemphys.2003.09.004 ↗
17. Kong T, Chen Y, Ye YP, Zhang K, Wang ZX, Wang XP (2009) An amperometric glucose biosensor based on the immobilization of glucose oxidase on the ZnO nanotubes. Sens Actuators B: Chem 138:344–35010.1016/j.snb.2009.01.002 ↗
18. Kulkarni AJ, Zhou M, Ke FJ (2005) Orientation and size dependence of the elastic properties of zinc oxide nanobelts. Nanotechnology 16:2749–275610.1088/0957-4484/16/12/001 ↗
19. Liao L, Lu HB, Li JC, He H, Wang DF, Fu DJ, Liu C, Zhang WF (2007) Size dependence of gas sensitivity of ZnO nanorods. J Phys Chem C 111:1900–190310.1021/jp065963k ↗
20. Liu P, She GW, Liao ZL, Wang Y, Wang ZZ, Shi WS, Zhang XH, Lee ST, Chen DM (2009) Observation of persistent photoconductance in single ZnO nanotube. Appl Phys Lett 94:06312010.1063/1.3082173 ↗
21. Mao Y, Zhong J, Chen Y (2008) First principles study of the band structure and dielectric function of (6,6) single-walled zinc oxide nanotube. Physica E 40:499–50210.1016/j.physe.2007.07.008 ↗
22. Moon W, Hwang H (2008) Atomistic study of structures and elastic properties of single crystalline ZnO nanotubes. Nanotechnology 19:22570310.1088/0957-4484/19/22/225703 ↗
23. Nardelli MB, Yakobson BI, Bernholc J (1998a) Brittle and ductile behavior in carbon nanotubes. Phys Rev Lett 81:465610.1103/PhysRevLett.81.4656 ↗
24. Nardelli MB, Yakobson BI, Bernholc J (1998b) Mechanism of strain release in carbon nanotubes. Phys Rev B 57:R427710.1103/PhysRevB.57.R4277 ↗
25. Niemegeers A, Burgelman M (1997) Effects of the Au/CdTe back contact on IV and CV characteristics of Au/CdTe/CdS/TCO solar cells. J Appl Phys 81:2881–288610.1063/1.363946 ↗
26. Nosé S (1984) A unified formulation of the constant temperature molecular dynamics methods. J Chem Phys 81:51110.1063/1.447334 ↗
27. Qin Y, Wang XD, Wang ZL (2008) Microfibre-nanowire hybrid structure for energy scavenging. Nature 451:809–81310.1038/nature06601 ↗
28. Rao BB (2000) Zinc oxide ceramic semi-conductor gas sensor for ethanol vapour. Mater Chem Phys 64:62–6510.1016/S0254-0584(99)00267-9 ↗
29. Raymand D, Duin ACTv, Baudin M, Hermannson K (2008) A reactive force field (ReaxFF) for zinc oxide. Surf Sci 602:1020–103110.1016/j.susc.2007.12.023 ↗
30. Rodriguez JA, Jirsak T, Dvorak J, Sambasivan S, Fischer D (2000) Reaction of NO2 with Zn and ZnO: photoemission, XANES, and density functional studies on the formation of NO3. J Phys Chem B 104:319–32810.1021/jp993224g ↗
31. Sberveglieri G, Groppelli S, Nelli P, Tintinelli A, Giunta G (1995) A novel method for the preparation of NH3 sensors based on ZnO-In thin-films. Sens Actuators B: Chem 25:588–59010.1016/0925-4005(95)85128-3 ↗
32. Sebastian PJ, Ocampo M (1996) A photodetector based on ZnCdS nanoparticles in a CdS matrix formed by screen printing and sintering of CdS and ZnCl2. Sol Energy Mater Sol Cells 44:1–1010.1016/0927-0248(95)00168-9 ↗
33. Sun XW, Chu YD, Song T, Liu ZJ, Zhang L, Wang XG, Liu YX, Chen QF (2007) Application of a shell model in molecular dynamics simulation to ZnO with zinc-blende cubic structure. Solid State Commun 142:15–1910.1016/j.ssc.2007.01.035 ↗
34. Tien LC, Sadik PW, Norton DP, Voss LF, Pearton SJ, Wang HT, Kang BS, Ren F, Jun J, Lin J (2005) Hydrogen sensing at room temperature with Pt-coated ZnO thin films and nanorods. Appl Phys Lett 87:3
35. Touskova J, Kindl D, Tousek J (1997) Preparation and characterization of CdS/CdTe thin film solar cells. Thin Solid Films 293:272–27610.1016/S0040-6090(96)09113-4 ↗
36. Wang ZL, Song JH (2006) Piezoelectric nanogenerators based on zinc oxide nanowire arrays. Science 312:242–24610.1126/science.1124005 ↗
37. Wang RM, Xing YJ, Xu J, Yu DP (2003) Fabrication and microstructure analysis on zinc oxide nanotubes. New J Phys 5:11510.1088/1367-2630/5/1/115 ↗
38. Wang B, Nagase S, Zhao J, Wang G (2007) The stability and electronic structure of single-walled ZnO nanotubes by density functional theory. Nanotechnology 18:6
39. Weng MH, Ju SP, Wu WS (2009) The collective motion of carbon atoms in a (10,10) single wall carbon nanotube under axial tensile strain. J Appl Phys 106:06350410.1063/1.3181056 ↗
40. Xu JQ, Pan QY, Shun YA, Tian ZZ (2000) Grain size control and gas sensing properties of ZnO gas sensor. Sens Actuators B Chem 66:277–27910.1016/S0925-4005(00)00381-6 ↗
41. Xu H, Zhang RQ, Zhang XH, Rosa AL, Frauenheim T (2007) Structural and electronic properties of ZnO nanotubes from density functional calculations. Nanotechnology 18:6
42. Yakobson BI (1998) Mechanical relaxation and “intramolecular plasticity” in carbon nanotubes. Appl Phys Lett 72:91810.1063/1.120873 ↗
43. Yuan PF, Ding ZJ, Ju X (2008) Theoretical study on structural and elastic properties of ZnO nanotubes. Chin Phys Lett 25:1030–103310.1088/0256-307X/25/3/061 ↗
44. Zhang Y, Huang H (2008) Stability of single-wall silicon carbide nanotubes—molecular dynamics simulations. Comput Mater Sci 43:66410.1016/j.commatsci.2008.01.038 ↗
45. Zhou Z, Li Y, Liu L, Chen Y, Zhang SB, Chen Z (2008) Size- and surface-dependent stability, electronic properties, and potential as chemical sensors: computational studies on one-dimensional ZnO nanostructures. J Phys Chem C 112:13926–1393110.1021/jp803273r ↗
46. Zhu ZG, Chutia A, Sahnoun R, Koyama M, Tsuboi H, Hatakeyama N, Endou A, Takaba H, Kubo M, Del Carpio CA, Miyamoto A (2008) Theoretical study on electronic and electrical properties of nanostructural ZnO. Jpn J Appl Phys 47:2999–300610.1143/JJAP.47.2999 ↗