Abstract
This study describes the surface modification of porous Vycor glass® (PVG®) with ionic species based on 1-methyl-imidazolium groups, and the posterior utilization of the functional porous substrate to synthesize supported gold nanoparticles (Au NPs). The functionalization degree (amount of imidazolium groups per gram of PVG®) was successfully controlled by the concentration of the imidazolium-based alkoxysilane in the reaction media. The ion-exchange properties of the functional groups allowed an effective and homogeneous upload of AuCl4 − throughout the monolithic PVG® structure, with subsequent conversion to Au NPs by thermal treatment at 823 K, which also eliminated the organic groups chemically bonded to the surface. The amount of adsorbed AuCl4 − ions was shown to have influence on loading of the Au NPs while no size variation is observed, indicating that the porous environment of PVG® acts as a nanoreactor where the particles are formed in the confined space.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Supercapacitor Materials and Fabrication · Transition Metal Oxide Nanomaterials · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Alfaya RVS, Fujiwara ST, Gushikem Y, Kholin YV (2004) Adsorption of metal halides from ethanol solutions by a 3-n-propylpyridiniumsilsesquioxane chloride-coated silica gel surface. J Colloid Interface Sci 269:32–36. doi: 10.1016/S0021-9797(03)00611-810.1016/S0021-9797(03)00611-8 ↗
2. Berg RW (2007) Raman spectroscopy and ab initio model calculations on ionic liquids. Mon Chem 138:1045–1075. doi: 10.1007/s00706-007-0760-910.1007/s00706-007-0760-9 ↗
3. Caiut JMA, Nakagaki S, Friedermann GR, Drechsel SM, Zarbin AJG (2004) Nickel(II) and manganese(III) tetraazaannulenes complexes encapsulated in porous Vycor glass (PVG): investigation of catalytic activity. J Mol Catal A 222:213–222. doi: 10.1016/j.molcata.2004.08.01110.1016/j.molcata.2004.08.011 ↗
4. Cangussu D, Nunes WC, Pereira CLM, Pedroso EF, Mazali IO, Knobel M, Alves OL, Stumpf HO (2008) Slow magnetic relaxation in (CoCuII)-Cu-II coordination oligomer built into mesoporous material. Eur J Inorg Chem 24:3802–3808. doi: 10.1002/ejic.20080033010.1002/ejic.200800330 ↗
5. Cangussu D, Nunes WC, Corrêa HLS, Macedo WAA, Knobel M, Alves OL, Filho AGS, Mazali IO (2009) γ-Fe2O3 nanoparticles dispersed in porous Vycor glass: a magnetically diluted integrated system. J Appl Phys 105:013901. doi: 10.1063/1.305417310.1063/1.3054173 ↗
6. Carneiro NM, Nunes WC, Borges RP, Godinho M, Fernandez-Outon LE, Macedo WAA, Mazali IO (2010) NiO nanoparticles dispersed in mesoporous silica glass. J Phys Chem C 114:18773–18778. doi: 10.1021/jp104688610.1021/jp1046886 ↗
7. Chen H, Kou X, Yang Z, Ni W, Wang J (2008) Shape- and size-dependent refractive index sensitivity of gold nanoparticles. Langmuir 24:5233–5237. doi: 10.1021/la800305j10.1021/la800305j ↗
8. Correa DN, Silva JMDE, Santos EB, Sigoli FA, Souza Filho AG, Mazali IO (2011) TiO2- and CeO2-based biphasic core-shell nanoparticles with tunable core sizes and shell thicknesses. J Phys Chem C 115:10380–10387. doi: 10.1021/jp200540g10.1021/jp200540g ↗
9. Corning Glass datasheet (2012) VYCOR® Brand Porous Glass 7930 datasheet. Corning Inc. http://www.corning.com/docs/specialtymaterials/pisheets/Vycor%207930.pdf . Accessed 11 Sep 2012
10. Daniel MC, Astruc D (2004) Gold nanoparticles: assembly, supramolecular chemistry, quantum-size-related properties, and applications toward biology, catalysis, and nanotechnology. Chem Rev 104:293–346. doi: 10.1021/cr030698+10.1021/cr030698+ ↗
11. Fattori N, Maroneze CM, Da Costa LP, Strauss M, Sigoli FA, Mazali IO, Gushikem Y (2012) Ion-exchange properties of imidazolium-grafted SBA-15 toward AuCl4 − anions and their conversion into supported gold nanoparticles. Langmuir 28:10281–10288. doi: 10.1021/la301374z10.1021/la301374z ↗
12. Fujiwara ST, Gushikem Y, Alfaya RVS (2001) Adsorption of FeCl3, CuCl2 and ZnCl2 on silsesquioxane 3-n-propylpyridiniumchloride polymer film adsorbed on Al2O3 coated silica gel. Colloids Surf A 178:135–141. doi: 10.1016/S0927-7757(00)00685-310.1016/S0927-7757(00)00685-3 ↗
13. Iamamoto MS, Gushikem Y (1989) Adsorption and pre-concentration of some metal ions from ethanol on silica gel modified with pyridinium ion. Analyst 114:983–985. doi: 10.1039/AN989140098310.1039/an9891400983 ↗
14. Jeon Y, Sung J, Seo C, Lim H, Cheong H, Kang M, Moon B, Ouchi Y, Kim D (2008) Structures of ionic liquids with different anions studied by infrared vibration spectroscopy. J Phys Chem B 112:4735–4740. doi: 10.1021/jp712075210.1021/jp7120752 ↗
15. Kelly KL, Coronado E, Zhao LL, Schatz GC (2003) The optical properties of metal nanoparticles: the influence of size, shape, and dielectric environment. J Phys Chem B 107:668–677. doi: 10.1021/jp026731y10.1021/jp026731y ↗
16. Lowell S, Shields JE, Thomas MA, Thommes M (2006) Characterization of porous solids and powders: surface area. Pore size and density. Springer, Dordrecht
17. Maroneze CM, Magosso HA, Panteleimonov AV, Kholin YV, Gushikem Y (2011) Surface functionalization of SBA-15 and a nonordered mesoporous silica with a 1,4-diazabicyclo[2.2.2]octane derivative: study of CuCl2 adsorption from ethanol solution. J Colloid Interface Sci 356:248–256. doi: 10.1016/j.jcis.2010.12.03010.1016/j.jcis.2010.12.030 ↗
18. Mazali IO, Souza Filho AG, Viana BC, Mendes Filho J, Alves OL (2006) Size-controllable synthesis of nanosized-TiO2 anatase using porous Vycor glass as template. J Nanopart Res 8:141–148. doi: 10.1007/s11051-005-9003-310.1007/s11051-005-9003-3 ↗
19. Mie GVG (1907) Die optischen Eigenschaften kolloider Goldlösungen. Ann Phys 25:129–133
20. Rouquerol F, Rouquerol J, Sing KSW (1999) Adsorption by powders and porous solids. Academic Press, San Diego
21. Santos EB, Sigoli FA, Mazali IO (2012) Structural evolution in crystalline MoO3 nanoparticles with tunable size. J Solid State Chem 190:80–84. doi: 10.1016/j.jssc.2012.02.01210.1016/j.jssc.2012.02.012 ↗
22. Sing KSW, Everett DH, Haul RAW, Moscou L, Pierotti RA, Rouquerol J, Siemieniewska T (1985) Reporting physisorption data for gas/solid systems with special reference to the determination of surface area and porosity. Pure Appl Chem 57:603–619. doi: 10.1351/pac19855704060310.1351/pac198557040603 ↗
23. Stammreich H, Forneris R (1960) Raman spectra and force constants of planar square molecules of the type AB4. Spectrochim Acta 16(3):363–367. doi: 10.1016/0371-1951(60)80097-510.1016/0371-1951(60)80097-5 ↗
24. Strauss M, Destefani TA, Sigoli FA, Mazali IO (2011) Crystalline SnO2 nanoparticles size probed by Eu3+ luminescence. Cryst Growth Des 11:4511–4516. doi: 10.1021/cg200729210.1021/cg2007292 ↗
25. Usher A, McPhail DC, Brugger J (2009) A spectrophotometric study of aqueous Au(III) halide–hydroxide complexes at 25–80 °C. Geochim Cosmochim Acta 73:3359–3380. doi: 10.1016/j.gca.2009.01.03610.1016/j.gca.2009.01.036 ↗
26. Wada Y, Kaneko M, Niinobe D, Tsukahara Y (2005) In situ synthesis of Ag2S nanosized particles in porous materials using single-source precursor. Chem Lett 34(12):1618–1619. doi: 10.1246/cl.2005.161810.1246/cl.2005.1618 ↗
27. Wada Y, Niinobe D, Kaneko M, Tsukahara Y (2006) Synthesis of Cd x Zn1−x S nanoparticles in porous Vycor glass by reaction of single-source precursors. Chem Lett 35(1):62–63. doi: 10.1246/cl.2006.6210.1246/cl.2006.62 ↗