Recovery in oxidation behavior of damaged SiC ZrB2/SiC coating of carbon/carbon composites
Source abstract
Abstract
Polysiloxane (PSO) was adopted as the matrix of the repair agents, and SiCZrB2 powder was used as the filler, to repair the prefabricated defects on the SiCZrB2/SiC (SZS) coating of carbon/carbon (C/C) composites. The repair agents were brushed on the defect areas and then underwent preoxidation (PR) or heat-treatment (HR) in a vacuum. The effects of different treatment processes on the chemical composition, microstructure of the repair agents, and the oxidation resistance behavior of the repaired coating were investigated. The repaired agents after both processes were pyrolyzed and generated SiOC ceramics, and they were well combined with the original coating. The thermal stability of PSO after preoxidation is poorer than that after heat-treatment, resulting in a weight loss rate of 5.88% after oxidation at 1 500 °C for 270 min, while that of the HR coating is only −0.87%, yet both have been great improvement compared with the unrepaired coating. This work provides an effective and simple approach to repairing damaged coatings for high-temperature applications.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Effect of in-situ grown SiC nanowires on the mechanical properties of HfC-ZrB2-SiC modified C/C composites10.1016/j.jallcom.2017.08.060 ↗
2. The improvement of the self-healing ability of MoSi2 coatings at 900 ∼ 1200 °C by introducing SiB610.1016/j.jeurceramsoc.2020.01.048 ↗
3. Radially one-dimensional hafnium carbide-carbon/carbon networks composites for ultra-high temperature ablation-resistance10.1016/j.corsci.2021.109443 ↗
4. A novel HfSiO wire drawing phenomenon after ablation of SiCnws/HfC-SiC coating on C/C composites10.1016/j.jmat.2020.03.001 ↗
5. Ablation resistance of HfC-TaC/HfC-SiC alternate coating for SiC-coated carbon/carbon composites under cyclic ablation10.1016/j.jeurceramsoc.2021.01.050 ↗
6. High temperature C/C-SiC composite by liquid silicon infiltration: a literature review10.1007/s12034-011-0247-5 ↗
7. SiOC modified carbon-bonded carbon fiber composite with SiC nanowires enhanced interfibrous junctions10.1111/jace.17025 ↗
8. Effects of LaB6 on composition, microstructure and ablation property of the HfC-TaC-SiC doped C/C composites prepared by precursor infiltration and pyrolysis
9. Micro/nano multiscale reinforcing strategies toward extreme high-temperature applications: take carbon/carbon composites and their coatings as the examples10.1016/j.jmst.2021.03.076 ↗
10. A SiC-ZrB2-ZrC coating toughened by electrophoretically-deposited SiC nanowires to protect C/C composites against thermal shock and oxidation10.1016/j.apsusc.2015.05.028 ↗
11. Grain growth limitation in the monolayer ZrB2-SiC coating above 1700 °C10.1016/j.ceramint.2022.02.014 ↗
12. A dense ZrB2-SiC-Si/SiC-Si coating to protect carbon/carbon composites against oxidation at 1773 K and 1973 K10.1016/j.corsci.2021.109331 ↗
13. Influence of chromium diboride on the oxidation resistance of ZrB2-MoSi2 and ZrB2-SiC ceramics10.1016/j.jeurceramsoc.2020.12.036 ↗
14. Nanoindentation and high temperature oxidation behavior of ZrB2-20SiC-(0-10 wt.%) Ta UHTCs10.1016/j.ceramint.2021.04.241 ↗
15. Liquid poly(silylacetylene)siloxane resin as a novel precursor of silicon carbide and silicon oxycarbide ceramics10.1016/j.ceramint.2011.11.012 ↗
16. Low/intermediate temperature pyrolyzed polysiloxane derived ceramics with increased carbon for electrical applications10.1016/j.jeurceramsoc.2021.04.007 ↗
17. Thermal conversion of carbon fibres/polysiloxane composites to carbon fibres/ceramic composites10.1016/j.ceramint.2012.10.219 ↗
18. Microwave-absorption properties of heterostructural SiC nanowires/SiOC ceramic derived from polysiloxane10.1016/j.ceramint.2018.09.306 ↗
19. Formation of carbon fiber-reinforced ceramic matrix composites with polysiloxane/silicon derived matrix10.1016/j.msea.2006.08.102 ↗
20. Preparation and characterization of oxidation-resistant black glass (SiCO) coatings obtained by hydrosilylation of polysiloxanes
21. Effect of the sintering temperature on the microstructure, properties and formation mechanism of ceramic materials obtained from polysiloxane elastomer-based ceramizable composites10.1016/j.jallcom.2016.04.030 ↗
22. Effect of PSO and TiB2 content on the high temperature adhesion strength of SiBCNO ceramic10.1016/j.ceramint.2018.09.229 ↗
23. Synthesis of a novel preceramic polymer (V-PMS) and its performance in heat-resistant organic adhesives for joining SiC ceramic10.1016/j.jeurceramsoc.2012.03.032 ↗
24. Synthesis and electrochemical performance of a polymer-derived silicon oxycarbide/boron nitride nanotube composite10.1039/C7RA01545C ↗
25. Silicon oxycarbide glass-graphene composite paper electrode for long-cycle lithium-ion batteries10.1038/ncomms10998 ↗
26. A simply prepared flexible SiBOC ultrafine fiber mat with enhanced high-temperature stability and chemical resistance10.1039/C5RA03100A ↗
27. A novel crosslinking agent of polymethyl(ketoxime)siloxane for room temperature vulcanized silicone rubbers: synthesis, properties and thermal stability10.1039/C7RA13375H ↗
28. Effect of incremental curing agent additions on thermal degradation of polydimethylsiloxane in air: a kinetic study10.14233/ajchem.2014.17132 ↗
29. Improvement of thermal resistance of polydimethylsiloxanes with polymethylmethoxysiloxane as crosslinker10.1016/j.polymdegradstab.2007.09.010 ↗