Abstract
Abstract Cr–C deposits were electroplated on a pure Cu substrate in a Cr +3 -based plating bath. After electroplating, the Cr–C deposits with and without a Cu substrate were flame-heated for 2 s to increase their hardness. Experimental results show that the hardness and crack density of a flame-heated Cr–C deposit were strongly affected by the Cu-substrate thickness. The hardness of as-plated Cr–C deposit with a Cu substrate increased from 750 to 1600 Hv after flame heating, while a low hardness value of 970 Hv was detected from the flame-heated Cr–C deposit without a Cu substrate. Increase in hardness values of flame-heated Cr–C deposits is attributed to precipitation of crystalline diamond membranes. Fully crystalline diamond-like membranes were found in the flame-heated Cr–C deposit with a Cu substrate; while semi-crystalline diamond-like membranes were detected in the flame-heated deposit without a Cu substrate. The constraint effect of the Cu substrate induced a high internal tension stress in the Cr–C deposit during and after flame heating, leading to widening through-deposit cracks and increasing the deposit hardness.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Advanced materials and composites · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. PVD coatings as an environmentally clean alternative to electroplating and electroless processes10.1016/S0257-8972(99)00145-0 ↗
2. Alternative to chromium: characteristics and wear behavior of HVOF coatings for gas turbine shafts repair (heavy-duty)10.1016/j.jmatprotec.2004.02.061 ↗
3. Corrosion resistance and lubricated sliding wear behaviour of novel Ni–P graded alloys as an alternative to hard Cr deposits10.1016/j.apsusc.2005.08.040 ↗
4. Current efficiency and polarization behavior of trivalent chromium electrodeposition process10.1016/S0013-4686(02)00678-3 ↗
5. Characterization of intermediate Cr-C layer fabricated by electrodeposition in hexavalent and trivalent chromium baths10.1016/j.surfcoat.2003.09.069 ↗
6. Electrochemical corrosion behavior of chromium–phosphorus coatings electrodeposited from trivalent chromium baths10.1016/j.electacta.2008.03.081 ↗
7. Improved electrochemical performance of trivalent-chrome coating on Al 6063 alloy via urea and thiourea addition10.1016/j.electacta.2008.06.069 ↗
8. Nanocrystalline hard chromium electrodeposition from trivalent chromium bath containing carbamide and formic acid: structure, composition, electrochemical corrosion behavior, hardness and wear characteristics of deposits10.1016/j.apsusc.2011.04.095 ↗
9. The electrochemical reduction mechanism of trivalent chromium in the presence of formic acid10.1016/j.elecom.2008.11.055 ↗
10. Role of carbon in the chromium deposit electroplated from a trivalent chromium-based bath10.1016/j.surfcoat.2010.12.010 ↗
11. The hardening mechanism of a chromium–carbon deposit electroplated from a trivalent chromium-based bath10.1016/j.tsf.2009.03.188 ↗
12. Role of nickel undercoat and reduction-flame heating on the mechanical properties of Cr–C deposit electroplated from a trivalent chromium based bath10.1016/j.surfcoat.2009.03.010 ↗
13. Tribological and electrochemical behavior of thick Cr–C alloy coatings electrodeposited in trivalent chromium bath as an alternative to conventional Cr coatings10.1016/j.electacta.2006.07.038 ↗
14. Properties and preparation of amorphous chromium carbide electroplates10.1016/S0013-4686(02)00163-9 ↗
15. Electrodeposition and tribological behavior of amorphous chromium-alumina composite coatings10.1016/j.surfcoat.2007.10.008 ↗
16. Improving the corrosion performance of Cr–C amorphous coatings on steel substrate by modifying the steel surface preparation10.1016/j.surfcoat.2010.08.123 ↗
17. Microstructure study of the hardening mechanism of Cr–Ni alloy deposits after flame heating for a few seconds10.1016/j.surfcoat.2011.07.024 ↗