Diffusion brazing of monocrystal silicon by using germanium as filler material
Source abstract
Abstract
Abstract In this research, diffusion brazing of monocrystal silicon was performed using germanium powders as interlayer. The effects of brazing temperature (950–1050 °C) and time (1–3 h) were studied on the joint microstructure and its mechanical properties. The results indicated that, with the rise in brazing time and temperature, the morphology near the sample edge turned from sintered structures to bridge connections. While those in the center evolved from straight Ge layers to symmetric layer structures with the sequence of “Si base/Isothermal solidification zone/Athermal solidification zone/Ge laye r ”. Withal, the crushing and interlocking morphologies appeared. Bond strength was evaluated and maximum tensile strength over 15.8 MPa was obtained for the joint processed at 1000 °C for 3 h. Results showed that, thickness of diffusion layer (i.e., the isothermal solidification zone and athermal solidification zone) was proved to be the controlling factor for the tensile strength of diffusion brazed monocrystal silicon.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: 3D IC and TSV technologies · Advanced ceramic materials synthesis · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Influence of silicon crystal orientation on piezoelectric textured aluminium nitride deposited on metal electrodes10.1016/j.vacuum.2016.07.019 ↗
2. Adhesive wafer bonding10.1063/1.2168512 ↗
3. Strong high-yield and low-temperature thermocompression silicon wafer-level bonding with gold10.1088/0960-1317/14/7/007 ↗
4. Wafer bonding-a powerful tool for MEMS
5. Micropackaging technologies for integrated microsystems: applications to MEMS and MOEMS
6. Study of microstructure and property of monocrystal silicon by Au-Si eutectic diffusion bonding (in Chinese)
7. Study of die bond voids on memory semiconductor devices in 24-L cerquad packages10.1007/BF02657478 ↗
8. Amorphous Si/Au wafer bonding10.1063/1.2719025 ↗
9. Determination of hydrogen concentration in a-Si and a-Ge layers by elastic recoil detection analysis10.1016/j.vacuum.2011.07.050 ↗
10. Hydrogenated amorphous silicon germanium alloy with enhanced photosensitivity prepared by plasma enhanced chemical vapor deposition at high temperature10.1016/j.vacuum.2012.09.004 ↗
11. Synthesis of SiGe layered structure in single crystalline Ge substrate by low energy Si ion implantation10.1016/j.vacuum.2013.10.016 ↗
12. Low temperature germanium to silicon direct wafer bonding using free radical exposure10.1063/1.3360201 ↗
13. Comprehensive investigation of Ge-Si bonded interfaces using oxygen radical activation
14. Crystallographic properties of Ge/Si heterojunctions fabricated by wet wafer bonding10.1007/s11664-010-1228-y ↗
15. Thermal and electrical properties of Czochralski grown GeSi single crystals10.1016/S0022-3697(01)00026-9 ↗
16. Yu · 2001 · 203
17. Fabrication of vertical sidewalls by anisotropic etching of silicon (100)10.1149/1.2059299 ↗
18. Anisotropic etching of silicon in TMAH solutions10.1016/0924-4247(92)80139-T ↗
19. Formation mechanism of cellular structures during unidirectional growth of binary semiconductor Si-rich SiGe materials10.1063/1.3675860 ↗
20. The critical growth velocity for planar-to-faceted interfaces transformation in SiGe crystals10.1063/1.3698336 ↗
21. Hu · 2000 · 59
22. A study of the transient liquid phase bonding process applied to an Ag/Cu/Ag sandwich joint10.1007/BF02649282 ↗
23. Transient liquid phase bonding10.1146/annurev.ms.22.080192.000323 ↗
24. Microstructures and mechanical properties of magnesium alloy and stainless steel weld-joint made by friction stir lap welding10.1016/j.matdes.2011.07.016 ↗