Argon ion beam voltage in a dual ion beam sputtering system influence on the aluminum nitride films microstructure
Source abstract
Abstract
Abstract The aluminum nitride (AlN) film has been successfully prepared at argon ion beam voltages ranging from 600 to 1200 V in the dual ion beam sputtering system. The AlN film had the (0 0 2) preferred orientation at 800 V and then changed to AlN (1 0 0) above 1000 V. Moreover, the nano-grain size presented in AlN film was observed using TEM. The Al-2p 3/2 and N-1s spectra were, respectively, centered at 74.2±0.2 eV and 397.4±0.2 eV at all voltages, which indicated the formation of Al–N bond. Furthermore, the Al concentration decreased monotonically with argon ion beam voltages. The stoichiometric AlN films can be synthesized around 960 V in the present study. The microstructure changes associated with argon ion beam voltages are also discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: GaN-based semiconductor devices and materials · Metal and Thin Film Mechanics · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Powder Diffraction File. Philadelphia, PA: Joint Committee on Powder Diffraction Standards. ASTM; 1996 Card 25–1133.
2. Ishihara · Thin Solid Films · 1998 · 316 · 15210.1016/S0040-6090(98)00406-4 ↗
3. Wang · Diamond Relat Mater · 1999 · 8 · 134210.1016/S0925-9635(99)00134-X ↗
4. Reier · Electrochim Acta · 1998 · 43 · 14910.1016/S0013-4686(97)00243-0 ↗
5. Strite · J Vac Sci Technol B · 1992 · 10 · 123710.1116/1.585897 ↗
6. Wang · Surf Coat Technol · 1998 · 103/104 · 33410.1016/S0257-8972(98)00410-1 ↗
7. Engelmark · J Vac Sci Technol A · 2000 · 18 · 160910.1116/1.582394 ↗
8. Wauk · Appl Phys Lett · 1968 · 13 · 28610.1063/1.1652613 ↗
9. García López · Diamond Relat Mater · 2003 · 12 · 115710.1016/S0925-9635(02)00306-0 ↗
10. Akiyama · Thin Solid Films · 1998 · 315 · 6210.1016/S0040-6090(97)00697-4 ↗
11. Yim · J Appl Phys · 1973 · 44 · 29210.1063/1.1661876 ↗
12. Someno · Thin Solid Films · 1991 · 202 · 33310.1016/0040-6090(91)90104-6 ↗
13. Ohchi · J Vac Sci Technol A · 1987 · 5 · 163010.1116/1.574579 ↗
14. Gadenne · Thin Solid Films · 1998 · 333 · 25110.1016/S0040-6090(98)00816-5 ↗
15. Chu · Thin Solid Films · 2003 · 429 · 110.1016/S0040-6090(02)01286-5 ↗
16. Rowland · J Mater Res · 1993 · 8 · 231010.1557/JMR.1993.2310 ↗
17. Norton · J Appl Phys · 1991 · 70 · 287110.1063/1.349352 ↗
18. Fuentes · Surf Coat Technol · 2002 · 151/152 · 36510.1016/S0257-8972(01)01558-4 ↗
19. Ensinger · Nucl Instrum Methods B · 1995 · 106 · 14210.1016/0168-583X(95)00693-1 ↗
20. Ensinger · Surf Coat Technol · 1998 · 99 · 110.1016/S0257-8972(97)00410-6 ↗
21. Manova · Vacuum · 1999 · 52 · 30110.1016/S0042-207X(98)00303-0 ↗
22. Laidani · Surf Coat Technol · 1999 · 122 · 24210.1016/S0257-8972(99)00377-1 ↗
23. Sánchez-Lòpez · Nanostructured Mater · 1999 · 11 · 24910.1016/S0965-9773(99)00038-0 ↗
24. Laio · J Vac Sci Technol A · 1993 · 11 · 268110.1116/1.578626 ↗
25. Gredelj · Appl Surf Sci · 2001 · 174 · 24010.1016/S0169-4332(01)00169-6 ↗
26. Cho · J Appl Phys · 1999 · 85 · 790910.1063/1.370606 ↗
27. Briggs · 1996 · vol. 1