Formation of MoSi2 by rapid thermal annealing in vacuum of CVD – Mo films on silicon substrate
Source abstract
Abstract
Abstract Silicide formation due to thermal treatment of thin (200–1000 A) molybdenum films on single-crystal silicon substrates in the temperature range of 800–1000°C was studied. Rapid thermal annealing (RTA) in vacuum was performed on Mo/Si system to form silicides. Molybdenum films were deposited on Si (1 0 0) by chemical vapor deposition (CVD), using Mo(CO)6 (molybdenum hexacarbonyl) as precursor. The as-deposited films with thicknesses of 200 and 1000 A were heated in vacuum at RTA temperatures of 800 and 1000°C for time durations of 15 and 30 s, 1 and 3 min. The results from the X-ray diffraction analysis and the Reflection Infrared Spectroscopy measurements show that Mo films after annealing transform into Mo silicides, preferably tetragonal MoSi2 crystal phase. The presence of Mo5Si3 formation is also found. There is a change in the electrical resistance of the films before and after annealing. For the molybdenum silicides obtained the resistivity is in the range 0.9–9.8 mΩ cm.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and interfaces · Metallurgical and Alloy Processes · Force Microscopy Techniques and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Nicolet MA, Lau SS. VLSI electronics microstructure science. New York: Academic Press, 1983. p. 328.
2. d'Heurle FM, VLSI science and technology. In: Dell'Oca C, Bullis WM, editors. Penington, NJ: Electrochemical Society, 1982. p. 194.
3. Murarka · J Vac Sci Technol · 1980 · 1 · 693
4. Doland · J Mater Res · 1990 · 5 · 1210.1557/JMR.1990.2854 ↗
5. Nava · Thin Solid Films · 1982 · 94 · 5910.1016/0040-6090(82)90030-X ↗
6. Taubenblatt · J Appl Phys · 1982 · 53 · 630810.1063/1.331551 ↗
7. Karlin · Appl Surf Sci · 1993 · 73 · 28010.1016/0169-4332(93)90180-J ↗
8. Gao · Appl Phys A · 1999 · 68 · 33310.1007/s003390050898 ↗
9. Backhous · Thin Solid Films · 1997 · 311 · 29910.1016/S0040-6090(97)00700-1 ↗
10. Gesheva · Vacuum · 1998 · 51 · 18110.1016/S0042-207X(98)00155-9 ↗
11. Gesheva KA, Abrosimova V, Beshkov GD. J Phys IV 1991;1:(Suppl. Phys II)C2-865–71.10.1051/jp4:19912103 ↗
12. Gesheva · Appl Surf Sci · 1993 · 73 · 8610.1016/0169-4332(93)90150-A ↗
13. Gesheva · J Phys IV · 1999 · 9 · 453
14. Gogova · J Cryst Growth · 1999 · 198/199 · 123010.1016/S0022-0248(98)01051-3 ↗