Plasma CVD of alumina—Unsolved problems
Source abstract
Abstract
Abstract In the present investigation, a commercial plasma CVD system suited for the deposition of titanium nitride (TiN) was adapted for alumina deposition up to substrate temperatures of 800 °C. The investigations clearly demonstrated that activating the process gas by plasma lowers the temperature needed for the formation of hard alumina coatings. The properties of the alumina coatings depend strongly on process parameters like temperature, plasma power and process gas composition. Higher plasma power as well as certain additives to the process gas favour the formation of hard alumina (α-phase) at lower temperatures and suppress the formation of softer alumina modifications. At the present stage, the process is still not sufficiently uniform. Furthermore, certain types of damage in the coatings were observed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Semiconductor materials and devices · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Täschner · Surf Coat Technol · 1998 · 108–109 · 25710.1016/S0257-8972(98)00561-1 ↗
2. Täschner · Surf Coat Technol · 1999 · 116–119 · 89110.1016/S0257-8972(99)00148-6 ↗
3. Kyrylov · Surf Coat Technol · 2003 · 163–164 · 20310.1016/S0257-8972(02)00482-6 ↗
4. Kyrylov · Appl Phys A · 2005 · 80 · 165710.1007/s00339-004-2998-y ↗
5. Fink · Surf Coat Technol · 2004 · 188–189 · 28110.1016/j.surfcoat.2004.08.044 ↗
6. Fink M, Laimer J, Mitterer C, Störi H. Surf Coat Technol, in press.
7. Rübig GmbH, Wels, Austria, http://www.rubig.com.
8. Beer · J Vac Sci Technol A · 2000 · 18 · 42310.1116/1.582204 ↗
9. Kugler · Vacuum · 2001 · 61 · 37910.1016/S0042-207X(01)00148-8 ↗
10. Fink · Vacuum · 2003 · 71 · 21910.1016/S0042-207X(02)00740-6 ↗