journal article·2003-09

Thermal annealing of sputtered Al–Si–Cu–N films

H. Zeman, J. Musil, J. Vlček, P.H. Mayrhofer, C. Mitterer

Vacuum· Volume 72· Issue 1
Publisher page

Abstract

Abstract This article reports on stress, structure and thermal stability of Al–Si–Cu–N films prepared by DC reactive magnetron sputtering. The films were deposited under the following conditions: discharge current I d =1 A, substrate bias U s =−100 V, substrate ion current density i s =0.6 and 0.9 mA/cm 2 , substrate temperature T s =300°C and 500°C, substrate-to-target distance d s−t =60 mm, partial pressure of nitrogen p N 2 ranging from 0.06 to 0.14 Pa and constant total pressure p T =p Ar +p N 2 =0.5 Pa . It was found that [1] the macrostress σ increases with increasing p N 2 and [2] the films sputtered at very low values of p N 2 (i) are polycrystalline films consisting of Al and small amounts of Al 2 Cu, (ii) are in tension and (iii) have a mat appearance due to a rough surface. According to the changes in structure during annealing up to 700°C, the Al–Si–Cu–N films can be divided into two groups: (a) metastable films which are characterized by a crystalline structure and (b) stable films which exhibit an X-ray amorphous structure. The metastable films change their structure upon thermal annealing. On the contrary, the stable films remain amorphous even after annealing at T a =700°C for 30 min. The stable films contain a high (approx. 8 at%) amount of copper and exhibit the lowest thermal expansion coefficient α c ≈4.2×10 −6 K −1 compared to the metastable films with α c ≈10–12×10 −6 K −1 . The experiments described in this paper show that the thermal expansion coefficient of the films strongly depends on their structure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Copper Interconnects and Reliability · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Hoffmann · Surf Interface Anal · 1981 · 3 · 6210.1002/sia.740030113 ↗
2. Thornton · Thin Solid Films · 1989 · 171 · 510.1016/0040-6090(89)90030-8 ↗
3. d’Heurle · Thin Solid Films · 1989 · 171 · 8110.1016/0040-6090(89)90035-7 ↗
4. Bromark · Surf Eng · 1994 · 10 · 20510.1179/sur.1994.10.3.205 ↗
5. Kleer · Surf Coat Technol · 1992 · 54–55 · 16710.1016/0257-8972(92)90157-6 ↗
6. Broitman · Appl Phys Lett · 1998 · 72 · 253210.1063/1.121410 ↗
7. Teixeira · Surf Coat Technol · 1999 · 120–121 · 10310.1016/S0257-8972(99)00341-2 ↗
8. Michler · Thin Solid Films · 1999 · 357 · 18910.1016/S0040-6090(99)00528-3 ↗
9. Karlsson · Thin Solid Films · 2000 · 371 · 16710.1016/S0040-6090(00)00996-2 ↗
10. Kendig · Surf Coat Technol · 2000 · 132 · 12410.1016/S0257-8972(00)00908-7 ↗
11. Shen · Surf Coat Technol · 2000 · 127 · 23910.1016/S0257-8972(00)00664-2 ↗
12. Göbel Th, Menzel S, Hecker M, Brückner W, Weitzig K, Genzel Ch. Surf Coat Technol 2001;142–144:861.10.1016/S0257-8972(01)01102-1 ↗
13. Vaz · Thin Solid Films · 2002 · 402 · 19510.1016/S0040-6090(01)01672-8 ↗
14. Niederhofer · Surf Coat Technol · 1999 · 120–121 · 17310.1016/S0257-8972(99)00451-X ↗
15. Männling · Surf Coat Technol · 2001 · 146–147 · 26310.1016/S0257-8972(01)01474-8 ↗
16. Karvánková · Surf Coat Technol · 2001 · 146–146 · 28010.1016/S0257-8972(01)01477-3 ↗
17. Mayrhofer · Surf Coat Technol · 2000 · 133–134 · 13110.1016/S0257-8972(00)00887-2 ↗
18. Mayrhofer · Surf Coat Technol · 2001 · 142–144 · 7810.1016/S0257-8972(01)01090-8 ↗
19. Mayrhofer · Thin Solid Films · 2001 · 415 · 15110.1016/S0040-6090(02)00511-4 ↗
20. Mitterer · Thermal stability of PVD hard coatings, Vacuum · 2003 · 71 · 279
21. Shiraishi M, Ischizama W, Oshino T, Murakami K. Jpn J Appl Phys. Pt. 1, No 12B, 2000;39:6810.10.1143/JJAP.39.6810 ↗
22. Berger · Thin Solid Films · 2001 · 401 · 17910.1016/S0040-6090(01)01481-X ↗
23. Sheeja · Surf Coat Technol · 2002 · 154 · 28910.1016/S0257-8972(02)00005-1 ↗
24. Kunc F, Musil J, Mayrhofer MH, Mitterer C. Low-stress Ti–B films prepared by magnetron sputtering, Paper No. WePNS1 at the 8th International Conference on Plasma Surface Engineering, September 9–13, 2002, Garmisch-Partenkirchen, Germany.
25. Musil · J Kasl Thin Solid Films · 2002 · 413 · 12110.1016/S0040-6090(02)00357-7 ↗
26. Wilcock · Thin Solid Films · 1969 · 3 · 310.1016/0040-6090(69)90107-2 ↗
27. Ebert · 1971 · 402