journal article·2025-04

Effect of bias voltage and deposition temperature on the microstructure, mechanical properties and lead-bismuth corrosion resistance of FeCrAlY coating

Rongshuo Wang, Wei Zhang, Jijun Yang, Yilong Zhong, Jian Yang, Changda Zhu, Hao Liu, Sha Zhao, Jiuguo Deng

Vacuum· Volume 234
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metal and Thin Film Mechanics · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Evaluation of the optimal Y content for the FeCrAl coating with excellent LBE corrosion resistance10.1016/j.jnucmat.2024.155316 ↗
2. A comparative study on liquid metal embrittlement susceptibility of three FeCrAl ferritic alloys in contact with liquid lead-bismuth eutectic at 350°C10.1016/j.corsci.2021.109346 ↗
3. A study of early corrosion behaviors of FeCrAl alloys in liquid lead–bismuth eutectic environments10.1016/j.jnucmat.2010.10.018 ↗
4. Corrosion studies of a low alloyed Fe–10Cr–4Al steel exposed in liquid Pb at very high temperatures10.1016/j.jnucmat.2020.152022 ↗
5. Lead– B ismuth eutectic (LBE): a coolant candidate for gen. IV advanced nuclear reactor concepts10.1002/adem.201300296 ↗
6. Corrosion behavior of refractory TiNbZrMoV high-entropy alloy coating in static lead-bismuth eutectic alloy: a novel design strategy of LBE corrosion-resistant coating?10.1016/j.surfcoat.2022.128884 ↗
7. A novel AlCrFeMoTi high-entropy alloy coating with a high corrosion-resistance in lead-bismuth eutectic alloy10.1016/j.corsci.2021.109524 ↗
8. Improved LBE corrosion resistance of the FeCrAl coating by the addition of trace Si element10.1016/j.intermet.2024.108197 ↗
9. Challenges and coating solutions for wear and corrosion inside Lead Bismuth Eutectic: a review10.1016/j.surfcoat.2022.128542 ↗
10. Corrosion, Al containing corrosion barriers and mechanical properties of steels foreseen as structural materials in liquid lead alloy cooled nuclear systems10.1016/j.nucengdes.2010.08.005 ↗
11. T91 cladding tubes with and without modified FeCrAlY coatings exposed in LBE at different flow, stress and temperature conditions10.1016/j.jnucmat.2008.02.026 ↗
12. Corrosion behavior of Al-alloying high Cr-ODS steels in lead–bismuth eutectic
13. Corrosion behaviour of Al-added high Mn austenitic steels in molten lead bismuth eutectic with saturated and low oxygen concentrations at 450 °C10.1016/j.corsci.2020.108864 ↗
14. Corrosion experiments and materials developed for the Japanese HLM systems10.1016/j.jnucmat.2011.04.039 ↗
15. Effect of variation in oxygen concentration in static Pb–Bi eutectic on long-term corrosion performance of Al-alloyed austenitic steels at 500 °C10.1016/j.corsci.2021.109963 ↗
16. Corrosion behaviour of Al-added high Mn austenitic steels in molten lead bismuth eutectic with saturated and low oxygen concentrations at 450 °C10.1016/j.corsci.2020.108864 ↗
17. Pre- and post-deformation microstructures of oxide dispersion strengthened ferritic steels10.1016/j.jnucmat.2007.03.141 ↗
18. A novel FeCrAlW high entropy alloy coating for enhancing lead-bismuth eutectic corrosion resistance10.1016/j.jnucmat.2023.154844 ↗
19. Early stages of dissolution corrosion in 316L and DIN 1.4970 austenitic stainless steels with and without anticorrosion coatings in static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.matchar.2021.111234 ↗
20. Effect of LBE corrosion on microstructure of amorphous Al2O3 coating by magnetron sputtering10.1016/j.surfcoat.2022.128598 ↗
21. Oxidation mechanism of refractory Molybdenum exposed to oxygen-saturated lead-bismuth eutectic at 600 °C10.1016/j.corsci.2020.109132 ↗
22. Compatibility of surface-coated steels, refractory metals and ceramics to high temperature lead–bismuth eutectic10.1016/j.pnucene.2007.11.081 ↗
23. T91 cladding tubes with and without modified FeCrAlY coatings exposed in LBE at different flow, stress and temperature conditions10.1016/j.jnucmat.2008.02.026 ↗
24. Corrosion of steels with surface treatment and Al-alloying by GESA exposed in lead–bismuth10.1016/j.jnucmat.2006.01.014 ↗
25. Oxide scale formation of modified FeCrAl coatings exposed to liquid lead10.1016/j.corsci.2011.10.019 ↗
26. Screening of the FeCrAl LBE corrosion-resistant coatings: the effect of Cr and Al contents10.1016/j.surfcoat.2023.129477 ↗
27. Synergistic effect of simultaneous proton irradiation and LBE corrosion on the microstructure of the FeCrAl(Y) coatings10.1016/j.corsci.2024.111874 ↗
28. Surface modification/alloying using intense pulsed electron beam as a tool for improving the corrosion resistance of steels exposed to heavy liquid metals10.1016/j.jnucmat.2011.04.030 ↗
29. Microstructure, oxidation and corrosion properties of FeCrAl coatings with low Al content prepared by magnetron sputtering for accident tolerant fuel cladding10.1016/j.jnucmat.2021.152966 ↗
30. Segregation at the Al2O3-FeCrAl interface during high-temperature oxidation10.1023/A:1018818906559 ↗
31. Continuous hot corrosion behaviour of an FeCrAlSi coating prepared by laser cladding10.1016/j.surfcoat.2021.127424 ↗
32. Oxide scale formation of modified FeCrAl coatings exposed to liquid lead10.1016/j.corsci.2011.10.019 ↗
33. T91 cladding tubes with and without modified FeCrAlY coatings exposed in LBE at different flow, stress and temperature conditions10.1016/j.jnucmat.2008.02.026 ↗
34. Microstructure, oxidation and corrosion properties of FeCrAl coatings with low Al content prepared by magnetron sputtering for accident tolerant fuel cladding10.1016/j.jnucmat.2021.152966 ↗
35. Effect of sputtering bias voltage on the microstructure and lead-bismuth eutectic corrosion resistance of the FeCrAlY coating10.5006/4509 ↗
36. Dependence of Arc Ion plating process on properties of CrAl coating for ATF cladding: effect of bias voltage and targets10.1016/j.jnucmat.2023.154593 ↗
37. A high-entropy alloy nitride protective coating for fuel cladding in high temperature lead-bismuth eutectic alloy10.1016/j.jnucmat.2022.153888 ↗
38. Microstructure and high-temperature steam oxidation properties of thick Cr coatings prepared by magnetron sputtering for accident tolerant fuel claddings: the role of bias in the deposition process10.1016/j.corsci.2019.108378 ↗
39. Chemical ordering and texture in Ni–25 at% Al thin films10.1016/S1359-6454(01)00373-1 ↗
40. Effects of substrate temperature on the structure, residual stress and nanohardness of Ti6Al4V films prepared by magnetron sputtering10.1016/j.apsusc.2016.02.021 ↗
41. Effect of the substrate temperature in ZrN coatings grown by the pulsed arc technique studied by XRD10.1016/j.surfcoat.2006.02.030 ↗
42. Screening of the FeCrAl LBE corrosion-resistant coatings: the effect of Cr and Al contents10.1016/j.surfcoat.2023.129477 ↗
43. Characterization of corrosion phenomena and kinetics on T91 ferritic/martensitic steel exposed at 450 and 550 °C to flowing Pb-Bi eutectic with 10−7 mass% dissolved oxygen10.1016/j.jnucmat.2017.07.031 ↗
44. Corrosion behavior of 410 stainless steel in flowing lead-bismuth eutectic alloy at 550 °C10.1016/j.jnucmat.2019.05.029 ↗
45. Physical chemistry of corrosion and oxygen control in liquid lead and lead-bismuth eutectic
46. X-ray photoelectron spectroscopy: towards reliable binding energy referencing10.1016/j.pmatsci.2019.100591 ↗
47. C 1s peak of adventitious carbon aligns to the vacuum level: dire consequences for material's bonding assignment by photoelectron spectroscopy10.1002/cphc.201700126 ↗
48. Reliable determination of chemical state in x-ray photoelectron spectroscopy based on sample-work-function referencing to adventitious carbon: resolving the myth of apparent constant binding energy of the C 1s peak10.1016/j.apsusc.2018.04.226 ↗
49. Influence of ion irradiation on the nanomechanical properties of thin alumina coatings deposited on 316L SS by PLD10.1016/j.surfcoat.2020.125491 ↗
50. An in-situ study on surface coloring mechanism of a 12Cr ferrite/martensite stainless steel during vacuum heat treatment10.1016/j.vacuum.2023.112270 ↗
51. Analysis of XPS spectra of Fe2+ and Fe3+ ions in oxide materials10.1016/j.apsusc.2007.09.063 ↗
52. Improvement in wear resistance of laser-clad Fe–Cr–Mo–B–C-(TiC) amorphous-nanocrystalline coating10.1016/j.vacuum.2022.111676 ↗
53. Microstructure evolution and oxidation resistance properties of oxide dispersion strengthened FeCrAl alloys at 1100 °C10.1016/j.vacuum.2024.113371 ↗
54. Structural and XPS characterization of ALD Al2O3 coated porous silicon10.1016/j.vacuum.2014.12.015 ↗
55. Microstructure, mechanical properties and lead-bismuth eutectic corrosion behavior of (AlCrFeTiMo)NO and (AlCrFeTiNb)NO high entropy metal sublattice ceramic coatings10.1016/j.vacuum.2022.111774 ↗
56. The scherrer formula for X-ray particle size determination10.1103/PhysRev.56.978 ↗
57. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
58. Effect of Au-ion irradiation on the surface morphology, microstructure and mechanical properties of amorphous AlCrFeMoTi HEA coating10.1016/j.surfcoat.2021.127252 ↗
59. Study on LBE corrosion failure of FeAl/Al2O3 coatings after ion irradiation10.1016/j.matdes.2024.113019 ↗
60. Commentary on using H/E and H/E as proxies for fracture toughness of hard coatings10.1016/j.tsf.2019.04.040 ↗
61. Corrosion behavior and failure mechanism of amorphous Al2O3 coating at high-temperature LBE10.1016/j.vacuum.2023.112251 ↗
62. Elastic and plastic work of indentation as a characteristic of wear behavior for cutting tools with nitride PVD coatings
63. Exploring the application potential of FexAl/Al2O3 coatings for lead-cooled fast reactors10.1016/j.jnucmat.2023.154807 ↗
64. Microstructure response and LBE corrosion behavior of the FeCrAlY coating after Au-ions irradiation10.1016/j.corsci.2024.112521 ↗
65. Dose rate dependence of Cr precipitation in an ion-irradiated Fe 18Cr alloy10.1016/j.scriptamat.2017.11.040 ↗
66. A combined APT and SANS investigation of α′ phase precipitation in neutron-irradiated model FeCrAl alloys10.1016/j.actamat.2017.02.077 ↗
67. Kinetics of α′ precipitation in an electron-irradiated Fe15Cr alloy10.1016/j.scriptamat.2016.05.021 ↗
68. Corrosion behavior of the FeCrAl coating with different Cr and Al contents before and after Au-ions irradiation in stagnant LBE10.1016/j.corsci.2023.111590 ↗
69. Effect of Si content on the microstructure and properties of CrSi coatings for ATF cladding10.1016/j.vacuum.2023.112627 ↗
70. Impact of sample storage type on adventitious carbon and native oxide growth: X-ray photoelectron spectroscopy study10.1016/j.vacuum.2022.111463 ↗
71. Effect of bias voltage on the structure and properties of CuNiTiNbCr dual-phase high entropy alloy films10.1016/j.jallcom.2022.167371 ↗
72. Structural morphology and characterization of (AlCrMoTaTi)N coating deposited via magnetron sputtering10.1016/j.apsusc.2013.06.057 ↗
73. Influence of deposition temperature on WTiN coatings tribological performance10.1016/j.apsusc.2017.07.215 ↗
74. Influence of substrate bias, deposition temperature and post-deposition annealing on the structure and properties of multi-principal-component (AlCrMoSiTi)N coatings10.1016/j.surfcoat.2007.12.014 ↗
75. Effects of substrate bias on structure and mechanical properties of (AlCrNbSiTiV)N coatings10.1088/0022-3727/42/11/115401 ↗
76. Effects of substrate bias voltage on the phase structure, mechanical and wear resistance properties of tungsten boride films10.1016/j.ceramint.2022.01.009 ↗
77. A simple model for the formation of compressive stress in thin films by ion bombardment10.1016/0040-6090(93)90201-Y ↗
78. An intrinsic stress scaling law for polycrystalline thin films prepared by ion beam sputtering10.1063/1.339560 ↗
79. Residual stress in ion-assisted coatings10.1016/0257-8972(92)90158-7 ↗
80. Residual stresses in PVD hard coatings10.1016/0257-8972(95)02581-2 ↗
81. Thermal stability of PVD hard coatings10.1016/S0042-207X(02)00751-0 ↗
82. Effects of bias voltage on the microstructure and properties of Al-doped hydrogenated amorphous carbon films synthesized by a hybrid deposition technique10.1016/j.vacuum.2018.05.008 ↗
83. Tribological contact analysis of a rigid ball sliding on a hard coated surface10.1016/j.surfcoat.2005.03.040 ↗
84. Fabrication of AlTiN coatings deposited on the ultrasonic rolling textured substrates for improving coatings adhesion strength10.1016/j.apsusc.2021.149394 ↗
85. Damage mechanisms and cracking behavior of thermal sprayed WC–CoCr coating under scratch testing10.1016/j.wear.2014.02.017 ↗
86. Influence of surface morphology on corrosion and electronic behavior10.1016/j.actamat.2005.09.017 ↗
87. Corrosion behaviors of FeCrAl alloys exposed to oxygen-saturated static lead bismuth eutectic at 550 °C10.1016/j.corsci.2022.110767 ↗
88. Corrosion behaviors of ODS-FeCrAl in oxygen-saturated lead-bismuth eutectic at 550°C: effects of grain boundaries and minor elements10.1016/j.jnucmat.2023.154710 ↗
89. Oxide scales formed on Fe–Cr–Al-based model alloys exposed to oxygen containing molten lead10.1016/j.jnucmat.2013.02.044 ↗
90. Surface morphology of scale on FeCrAl (Pd, Pt, Y) alloys10.1016/j.jallcom.2007.01.170 ↗
91. Point defects and cation tracer diffusion in (CrxFe1-x,) 3-δO4 spinels10.1016/0167-2738(95)00190-H ↗
92. Influence of composition and microstructure on the corrosion behavior of different Fe–Cr–Al alloys in molten LBE10.1016/j.jnucmat.2011.11.049 ↗
93. TEM investigation of the microstructure of the scale formed on a FeCrAlRE alloy at 900 °C: the effect of Y-rich RE particles10.1007/s11085-010-9195-5 ↗
94. High temperature corrosion behavior of FeCrAlSi model alloys in the presence of water vapor and KCl at 600 °C – the influence of Cr content10.1016/j.corsci.2022.110114 ↗
95. Growth mechanism of reactively sputtered aluminum nitride thin films10.1016/S0921-5093(01)01477-0 ↗
96. Growth phenomena in room temperature pulsed laser deposited chromium and chromium nitride coatings10.1016/j.surfcoat.2005.02.016 ↗
97. Deposition of phase-pure Cr 2 AlC coating by DC magnetron sputtering and post annealing using Cr-Al-C targets with controlled elemental composition but different phase compositions10.1016/j.jmst.2017.01.029 ↗
98. The effect of oxygen incorporation in sputtered scandium nitride films10.1016/j.tsf.2008.05.050 ↗
99. Improved LBE corrosion resistance of the FeCrAl coating by the addition of trace Si element10.1016/j.intermet.2024.108197 ↗
100. Impact of cathode loss on plasma characteristics, microstructures and properties of 7YSZ coatings in PS-PVD10.1016/j.ceramint.2020.02.109 ↗