Abstract

Abstract Surface modification with high-power glow discharges is a promising physical vapor deposition (PVD) technology for industrial usage. A metal ion density higher than 1018 m−3 can be obtained due to a high-power input in the plasma. In the present paper, titanium films were deposited on Si (100) substrates using high-power impulse magnetron sputtering (HIPIMS). The pulse duration was varied to investigate the deposition rate and the titanium film structure. The plasma source was an unbalanced magnetron sputtering (UBMS) discharge generation system. The deposition rate was correlated to the electrical characteristics. There was an instantaneous power threshold of approximately 36 kW to significantly increase the deposition rate by 4–5 times. The deposition rate increased linearly with respect to the average power until the average power reached 5.6 kW (about 30 W/cm2 for a total area of the target), and an 83% increase of the deposition rate from the linear relationship was observed. The increase of the deposition rate was possibly closely related to the so-called thermal spike, where the target temperature increases due to a high power input to the target. The surface morphology and the crystalline structure of the films were studied for a variety of pulse durations, and the results were compared to the case of the direct-current magnetron sputtering (dcMS) process. The titanium films at an average power of 1.2 kW and a pulse duration of 50 μs have a smaller crystalline size and a smoother surface than those at an average power of 825 W by dcMS. The crystal orientation (101) was dominated when the pulse duration was lengthened to 180 μs, although the (002) orientation was dominant in dcMS. The crystal size and the surface roughness increased significantly when the pulse duration was increased from 50 μs to 180 μs in HIPIMS. The consumed power in the plasma by HIPIMS can be an important parameter for the crystal size and the structure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Plasma Diagnostics and Applications · ZnO doping and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Helmerssen · Thin Solid Films · 2006 · 513 · 110.1016/j.tsf.2006.03.033 ↗
2. Wei · Surf Coat Tech · 2010 · 204 · 286910.1016/j.surfcoat.2010.01.046 ↗
3. Mändl · Nucl Instr Meth B · 2003 · 206 · 51710.1016/S0168-583X(03)00813-9 ↗
4. Huang · Surf Coat Technol · 2004 · 186 · 21810.1016/j.surfcoat.2004.04.041 ↗
5. Sarakinos · Surf Coat Tech · 2010 · 204 · 166110.1016/j.surfcoat.2009.11.013 ↗
6. Gudmundsson · J Vac Sci Technol · 2012 · A 30 · 03080110.1116/1.3691832 ↗
7. Bohlmark · Thin Solid Films · 2006 · 515 · 152210.1016/j.tsf.2006.04.051 ↗
8. Gudmundsson · Surf Coat Tech · 2002 · 161 · 24910.1016/S0257-8972(02)00518-2 ↗
9. Ehiasarian · Vacuum · 2002 · 65 · 12110.1016/S0042-207X(01)00475-4 ↗
10. Kouznetsov · Surf Coat Tech · 1999 · 122 · 29010.1016/S0257-8972(99)00292-3 ↗
11. Bohlmark · IEEE Transac Plasma Sci · 2005 · 33 · 34610.1109/TPS.2005.845022 ↗
12. Gudmundsson · J Phys: Conference Series · 2008 · volume 100
13. Ehiasarian · Surf Coat Tech · 2003 · 163–164 · 26710.1016/S0257-8972(02)00479-6 ↗
14. Ehiasarian · J Appl Phys · 2007 · 10110.1063/1.2697052 ↗
15. Bohlmark · J Vac Sci Technol · 2005 · A 23 · 1810.1116/1.1818135 ↗
16. Konstantinidis · J Vac Sci Technol · 2007 · B 25 · L19
17. Jing · Surf Coat Tech · 2011 · 206 · 96710.1016/j.surfcoat.2011.04.046 ↗
18. Samuelsson · Surf Coat Tech · 2010 · 205 · 59110.1016/j.surfcoat.2010.07.041 ↗
19. Anders · J.Phys.D Appl Phys · 2012 · 4510.1088/0022-3727/45/1/012003 ↗
20. Musil · J Vac Sci Technol · 2007 · A 25 · 66610.1116/1.2736680 ↗
21. Anders · J Appl Phys · 2007 · 102 · 11330310.1063/1.2817812 ↗
22. Chau · Thin Solid Films · 1996 · 287 · 5710.1016/S0040-6090(96)08559-8 ↗
23. Bräuer · Vacuum · 2010 · 84 · 135410.1016/j.vacuum.2009.12.014 ↗
24. Mercs · Surf Coat Tech · 2006 · 201 · 227610.1016/j.surfcoat.2006.03.035 ↗
25. Behrisch · Nucl Inst Methods Phys Research B · 1993 · 82 · 25510.1016/0168-583X(93)96027-A ↗
26. Bilek · Surf Coat Tech · 2004 · 186 · 2110.1016/j.surfcoat.2004.04.051 ↗
27. Gan · J Phys Condens Matter · 2004 · 16 · 175110.1088/0953-8984/16/10/007 ↗
28. Bilek · Thin Solid Films · 2005 · 482 · 6910.1016/j.tsf.2004.11.159 ↗
29. Jeyachandran · Mater Sci Eng · 2006 · A 431 · 27710.1016/j.msea.2006.06.020 ↗
30. Swalin · 1972
31. Chadwick · Philos Mag · 1969 · 20 · 40510.1080/14786436908228711 ↗
32. Checchetto · Thin Solid Films · 1997 · 299 · 510.1016/S0040-6090(97)00031-X ↗
33. Lundin · Plasma Sources Sci Technol · 2008 · 17
34. Chawla · Mater Chem Phys · 2008 · 111 · 41410.1016/j.matchemphys.2008.04.048 ↗
35. Cullity · 1978
36. Koto · Mater Chem Phys · 1998 · 54 · 12710.1016/S0254-0584(98)00021-2 ↗
37. Machunze · Thin Solid Films · 2009 · 518 · 156110.1016/j.tsf.2009.09.069 ↗
38. Alami · J Phys D Appl Phys · 2009 · 42