Hot corrosion behavior of Ba2DyAlO5 exposed to calcium-magnesium-alumina-silicate at 1300 °C and 1350 °C
Source abstract
Abstract
Abstract Calcium-magnesium-alumina-silicate (CMAS) attack has been considered as one of the significant failure mechanisms for thermal barrier coatings (TBCs). In this study, CMAS corrosion behavior of Ba2DyAlO5 is investigated at 1300 °C and 1350 °C for 0.5 h, 4 h, 12 h and 24 h. The results indicated that Ba2DyAlO5 had high resistance to CMAS infiltration for prolonged durations (24 h), ascribed to the rapid formation of crystallization phases by chemical reaction between Ba2DyAlO5 and CMAS. The corrosion products with a main constitution of Ca2Dy8(SiO4)6O2, Ba1.31Ca0.69SiO4, BaAl2O4 and Dy2O3 phases formed a sealing layer on the sample surfaces, which can effectively suppress further penetration of the molten CMAS. The associated mechanism was discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Calcia-magnesia-alumino-silicate (CMAS)-induced degradation and failure of air plasma sprayed yttria-stabilized zirconia thermal barrier coatings10.1016/j.actamat.2015.12.044 ↗
2. A study on the thermal cyclic behavior of thermal barrier coatings with different MCrAlY roughness10.1016/j.vacuum.2016.12.033 ↗
3. Microstructures and deposition mechanisms of quasi-columnar structured yttria-stabilized zirconia coatings by plasma spray physical vapor deposition10.1016/j.ceramint.2017.06.190 ↗
4. Stage growth of columnar 7YSZ coating prepared by plasma spray-physical vapor deposition10.1016/j.vacuum.2017.08.025 ↗
5. Tailoring the EB-PVD columnar microstructure to mitigate the infiltration of CMAS in 7YSZ thermal barrier coatings10.1016/j.jeurceramsoc.2016.07.027 ↗
6. Adsorbability and spreadability of calcium-magnesium-alumino-silicate (CMAS) on Al-modified 7YSZ thermal barrier coating10.1016/j.ceramint.2016.09.106 ↗
7. Wetting, infiltration and interaction behavior of CMAS towards columnar YSZ coatings deposited by plasma spray physical vapor10.1016/j.jeurceramsoc.2018.04.013 ↗
8. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts10.1111/j.1551-2916.2007.02175.x ↗
9. Hot corrosion behavior of LaMgAl11O19 ceramic coated with molten CMAS deposits at temperature of 1250° C in air10.1016/j.jallcom.2016.05.272 ↗
10. Plasma-sprayed La2Ce2O7 thermal barrier coatings against calcium-magnesium-alumina-silicate penetration10.1016/j.jeurceramsoc.2014.02.031 ↗
11. Hot corrosion behavior of solution precursor and atmospheric plasma sprayed thermal barrier coatings10.1016/j.corsci.2015.05.034 ↗
12. Microstructure, thermal conductivity and thermal cycling behavior of thermal barrier coatings prepared by plasma spray physical vapor deposition10.1016/j.surfcoat.2015.06.033 ↗
13. Effects of the combined vacuum pre-oxidation on the microcracks initiation and propagation of thermal barrier coatings deposited by means of plasma spraying10.1016/j.vacuum.2015.11.008 ↗
14. Microstructure and mechanical properties of plasma sprayed Al2O3-YSZ composite coatings10.1016/j.vacuum.2018.01.038 ↗
15. Calcia-magnesia-alumino-silicate (CMAS)-induced degradation and failure of air plasma sprayed yttria-stabilized zirconia thermal barrier coatings10.1016/j.actamat.2015.12.044 ↗
16. Hot corrosion behavior of BaLa2Ti3O10 exposed to calcium-magnesium-alumina-silicate at elevated temperatures10.1016/j.ceramint.2018.03.021 ↗
17. Composition effects of thermal barrier coating ceramics on their interaction with molten Ca-Mg-Al-silicate (CMAS) glass10.1016/j.actamat.2012.06.053 ↗
18. Preparation of plasma sprayed nanostructured GdPO4 thermal barrier coating and its hot corrosion behavior in molten salts10.1016/j.ceramint.2017.03.092 ↗
19. Step-by-step investigation of degradation mechanisms induced by CMAS attack on YSZ materials for TBC applications10.1016/j.surfcoat.2013.08.055 ↗
20. W.C. Hasz, M.P. Borom, C.A. Johnson, Protected thermal barrier coating composite with multiple coatings, U.S. Patent 5,914,189, 1999, 6–22.
21. R. Darolia, B.A. Nagaraj, Method of forming a coating resistant to deposits and coating formed thereby, U.S. Patent 6,720,038, 2004, 4–13.
22. CMAS (CaO-MgO-Al2O3-SiO2) resistance of Y2O3-stabilized ZrO2 thermal barrier coatings with Pt layers10.1016/j.ceramint.2017.09.197 ↗
23. CMAS-resistant plasma sprayed thermal barrier coatings based on Y2O3-stabilized ZrO2 with Al3+ and Ti4+ solute additions10.1007/s11666-014-0077-2 ↗
24. Calcium-magnesium-alumino-silicate induced degradation and failure of La2(Zr0.7Ce0.3)2O7/YSZ double-ceramic-layer thermal barrier coatings prepared by electron beam-physical vapor deposition10.1016/j.jeurceramsoc.2017.10.057 ↗
25. Calcium-magnesium-alumina-silicate (CMAS) resistance characteristics of LnPO4 (Ln= Nd, Sm, Gd) thermal barrier oxides10.1016/j.jeurceramsoc.2016.08.013 ↗
26. Defect engineering in development of low thermal conductivity materials: a review10.1016/j.jeurceramsoc.2016.07.036 ↗
27. Ultralow thermal conductivity in highly anion-defective aluminates10.1103/PhysRevLett.101.085901 ↗
28. Preparation and thermophysical properties of Yb-doped Ba2DyAlO5 ceramics10.1016/j.matlet.2015.01.003 ↗
29. Chemical compatibility and oxygen-ion conductivity of Ba2DyAlO5 ceramic for thermal barrier coatings10.1179/1432891715Z.0000000001509 ↗
30. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
31. High-temperature corrosion of EB-PVD yttria partially ptabilized pirconia phermal barrier voatings with an artificial volcanic ash overlay
32. Can TBC porosity be estimated by non-destructive infrared techniques? A theoretical and experimental analysis10.1016/j.surfcoat.2015.03.036 ↗
33. La2(Zr0.7Ce0.3)2O7 thermal barrier coatings prepared by electron beam-physical vapor deposition that are resistant to high temperature attack by molten silicate10.1016/j.corsci.2016.11.015 ↗
34. Environmental degradation of thermal-barrier coatings by molten deposits10.1557/mrs.2012.230 ↗
35. Interaction between ceramic powder and molten calcia-magnesia-alumino-silicate (CMAS) glass, and its implication on CMAS-resistant thermal barrier coatings10.1016/j.scriptamat.2015.09.027 ↗
36. 2ZrO2· Y2O3 thermal barrier coatings resistant to degradation by molten CMAS: part I, optical basicity considerations and processing10.1111/jace.13210 ↗
37. High temperature viscosity of calcium-magnesium-aluminosilicate glass from synthetic sand10.1016/j.scriptamat.2016.07.020 ↗
38. Glass viscosity calculation based on a global statistical modelling approach, Glass Technol