Diamond deposition on Mo with thermal stress buffer layer coated mild steel substrate by combustion flame CVD
Source abstract
Abstract
In order to develop wear resistance diamond/molybdenum (Mo) hybrid coating process can be conducted in open air. Diamond deposition on the molybdenum with thermal stress buffer layer coated mild steel substrate by the combustion flame chemical vapor deposition (CFCVD) was carried out. As the thermal stress buffer layer, atmospheric plasma sprayed Mo/Fe mixture coating was deposited between Mo top coat and mild steel substrate. Consequently, crack generation and peeling off of the coating occurred due to thermal influences on the condition of Mo coated mild steel substrate in our previous study, diamond particles could be created on the Mo coating without fracture and peeling off. Besides, an additional Mo coating after diamond deposition increases the adhesion force between the diamond coating and the initial Mo coating. This encapsulation of the diamond particles between two Mo layers dramatically improves the resistance of the global coating making it strong enough to resist to the wearing test. These results demonstrate the high potential of thermal sprayed coating for the wear resistance improvement.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Application of diamond-like carbon to a rotary engine
2. DLC coating technology applied to sliding parts of automotive engine
3. Press release. Business development in the 1st half of 2007 and outlook for the MAHLE group; September 3, 2007. p. 1–16.
4. PVD CrxN coatings for tribological application on piston rings10.1016/S0257-8972(97)00335-6 ↗
5. Friction behavior of sintered and sprayed FeMoS alloy powders10.4262/denkiseiko.72.83 ↗
6. Aumuller B, Lang A, Bergmann HW. Thermal spraying of freestanding parts for the automobile industry. In: Proceedings of the international conference on spray deposition and melt atomization; 2000. p. 367–78.
7. Marple BR, Voyer J. Improved wear performance by the incorporation of solid lubricants during thermal spraying. In: Proceedings of international thermal spray conference; 2000. p. 909–18.10.31399/asm.cp.itsc2000p0909 ↗
8. Gawne DT, Qiu Z, Zhang T, Bao Y, Zhang K. Abrasive wear resistance of plasma-sprayed glass-composite coatings. In: Proceedings of international thermal spray conference; 2000. p. 977–81.10.31399/asm.cp.itsc2000p0977 ↗
9. Ando Y, Fukuda K, Tobe S. Improvement of wear resistance of thermal sprayed molybdenum coating by diamond deposition using combustion flame CVD. In: Proceedings of thermal spray conference; 2001. p. 1093–98.10.31399/asm.cp.itsc2001p1093 ↗
10. Heteroepitaxial growth of smooth and continuous diamond thin films on silicon substrates via high quality silicon carbide buffer layers10.1063/1.114020 ↗